daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Synthesis and Characterization of Organo-Soluble Polyimides Derived from Alicyclic Dianhydrides and a Dihydroxyl-Functionalized Spirobisindane Diamine AITranslate

King Abdullah University of Science and Technology (KAUST); King Abdullah University of Science and Technology (KAUST); King Abdullah University of Science and Technology (KAUST); King Abdullah University of Science and Technology (KAUST)
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Two organo-soluble polyimides were synthesized by reaction of alicyclic bicyclo[2.2.2]oct-7-ene-2,3,5,6-tetracarboxylic dianhydride (BC) or 1,4,7,8-tetrabromobicyclo[2.2.2]oct-7-ene-2,3,5,6-tetracarboxylic anhydride (BCBr4) with 3,3,3′,3′-tetramethyl-1,1′-spirobisindane-5,5′-diamino-6,6′-diol (SBIDA). BC–SBIDA and BCBr4–SBIDA showed thermal stability of up to ∼420 and 352 °C and displayed microporosity as indicated by Brunauer–Emmett–Teller surface areas of 191 and 243 m2 g–1, respectively. The polyimides were solution-processable in polar organic solvents and exhibited strong mechanical properties with tensile modulus of 1.15–1.4 GPa, tensile strength of 27–28 MPa, and elongation at break of 2–4%. Introducing alicyclic moieties disturbs the delocalization of π-electrons across the polyimide backbone that reduces formation of charge transfer complexes (CTCs) leading to formation of colorless and transparent polyimide films. A fresh film sample of the bromine substituted BCBr4–SBIDA showed oxygen permeability of 31 barrer and oxygen/nitrogen selectivity of 5.9. Long-term physical aging of BCBr4–SBIDA over 365 days resulted in decrease of O2 permeability to 17 barrer with a simultaneous boost in O2/N2 selectivity to 6.6, which demonstrated highly competitive performance compared to commercially available polymers for air separation.

KeyWords AITranslate

alicyclic dianhydrides polyimides intrinsic microporosity optical properties membrane gas separation
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.8b00036

Chinese Library Classification Number:

Citation Information:

Two organo-soluble polyimides were synthesized by reaction of alicyclic bicyclo[2.2.2]oct-7-ene-2,3,5,6-tetracarboxylic dianhydride (BC) or 1,4,7,8-tetrabromobicyclo[2.2.2]oct-7-ene-2,3,5,6-tetracarboxylic anhydride (BCBr4) with 3,3,3′,3′-tetramethyl-1,1′-spirobisindane-5,5′-diamino-6,6′-diol (SBIDA). BC–SBIDA and BCBr4–SBIDA showed thermal stability of up to ∼420 and 352 °C and displayed microporosity as indicated by Brunauer–Emmett–Teller surface areas of 191 and 243 m2 g–1, respectively. The polyimides were solution-processable in polar organic solvents and exhibited strong mechanical properties with tensile modulus of 1.15–1.4 GPa, tensile strength of 27–28 MPa, and elongation at break of 2–4%. Introducing alicyclic moieties disturbs the delocalization of π-electrons across the polyimide backbone that reduces formation of charge transfer complexes (CTCs) leading to formation of colorless and transparent polyimide films. A fresh film sample of the bromine substituted BCBr4–SBIDA showed oxygen permeability of 31 barrer and oxygen/nitrogen selectivity of 5.9. Long-term physical aging of BCBr4–SBIDA over 365 days resulted in decrease of O2 permeability to 17 barrer with a simultaneous boost in O2/N2 selectivity to 6.6, which demonstrated highly competitive performance compared to commercially available polymers for air separation.

quote

GB/T 7714-2015 [1] Mahmoud A. Abdulhamid, Xiaohua Ma, Bader S. Ghanem, et al. ACS Applied Polymer Materials, 2019(1). DOI:10.1021/acsapm.8b00036.
MLA [1] Mahmoud A. Abdulhamid, et al., ACS Applied Polymer Materials, no. 1, 2019, https://doi.org/10.1021/acsapm.8b00036.
APA [1] Mahmoud A. Abdulhamid, Xiaohua Ma, Bader S. Ghanem, & Ingo Pinnau. (2019). ACS Applied Polymer Materials(1). https://doi.org/10.1021/acsapm.8b00036
IEEE [1] Mahmoud A. Abdulhamid, Xiaohua Ma, Bader S. Ghanem, and Ingo Pinnau, ACS Applied Polymer Materials, no. 1, 2019, doi: 10.1021/acsapm.8b00036. keywords: {alicyclic dianhydrides;polyimides;intrinsic microporosity;optical properties;membrane;gas separation}