Hybrid electrolytes based on ionic liquids and amorphous porous silicon nanoparticles: Organization and electrochemical properties AITranslate
Abstract AITranslate
Ionic liquids (ILs) and ionic liquid-nanoparticle (IL-NP) hybrid electrolytes have garnered a lot of interest due to their unique properties that stimulate their use in various applications. Herein, we investigate the electrochemical and photo-physical properties of organic-inorganic hybrid electrolytes based on three imidazolium-based ionic liquids, i.e., 1-buthyl-3-methylimidazolium thiocyanate ([bmim] [SCN]), 1-ethyl-3-methylimidazolium tetrafluoroborate ([emim] [BF4]) and 1-buthyl-3-methylimidazolium acetate ([bmim] [Ac]) that are covalently tethered to amorphous porous silicon nanoparticles (ap-Si NPs). We found that the addition of ap-Si NPs confer to the ILs a pronounced boost in the electrocatalytic activity, and in mixtures of ap-Si NPs and [bmim] [SCN], the room-temperature current transport is enhanced by more than 5 times compared to bare [bmim] [SCN]. A detailed structural investigation by transmission electron microscope (TEM) showed that the ap-Si NPs were well dispersed, stabilized and highly aggregated in [bmim] [SCN], [emim] [BF4] and [bmim] [Ac] ILs, respectively. These observations correlate well with the enhanced current transport observed in ap-Si NPs/[bmim] [SCN] evidenced by electrochemical measurements. We interpreted these observations by the use of UV–vis absorbance, photoluminescence (PL), FTIR and solid-state NMR spectroscopy. We found that the ap-Si NPs/[bmim] [SCN] hybrid stands out due to its stability and optical transparency. This behavior is attributed to the iron(III) thiocyanate complexion as per the experimental findings. Furthermore, we found that the addition of NPs to [emim] [BF4] alters the equilibrium of the IL, which consequently improved the stability of the NPs through intermolecular interactions with the two ionic layers (anionic and cationic layers) of the IL. While in the case of [bmim] [Ac], the dispersion of ap-Si NPs was restrained because of the high viscosity of this IL. Graphical abstract Download : Download high-res image (193KB) Download : Download full-size image
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1016/j.apmt.2017.04.011
Chinese Library Classification Number:
Citation Information:
Ionic liquids (ILs) and ionic liquid-nanoparticle (IL-NP) hybrid electrolytes have garnered a lot of interest due to their unique properties that stimulate their use in various applications. Herein, we investigate the electrochemical and photo-physical properties of organic-inorganic hybrid electrolytes based on three imidazolium-based ionic liquids, i.e., 1-buthyl-3-methylimidazolium thiocyanate ([bmim] [SCN]), 1-ethyl-3-methylimidazolium tetrafluoroborate ([emim] [BF4]) and 1-buthyl-3-methylimidazolium acetate ([bmim] [Ac]) that are covalently tethered to amorphous porous silicon nanoparticles (ap-Si NPs). We found that the addition of ap-Si NPs confer to the ILs a pronounced boost in the electrocatalytic activity, and in mixtures of ap-Si NPs and [bmim] [SCN], the room-temperature current transport is enhanced by more than 5 times compared to bare [bmim] [SCN]. A detailed structural investigation by transmission electron microscope (TEM) showed that the ap-Si NPs were well dispersed, stabilized and highly aggregated in [bmim] [SCN], [emim] [BF4] and [bmim] [Ac] ILs, respectively. These observations correlate well with the enhanced current transport observed in ap-Si NPs/[bmim] [SCN] evidenced by electrochemical measurements. We interpreted these observations by the use of UV–vis absorbance, photoluminescence (PL), FTIR and solid-state NMR spectroscopy. We found that the ap-Si NPs/[bmim] [SCN] hybrid stands out due to its stability and optical transparency. This behavior is attributed to the iron(III) thiocyanate complexion as per the experimental findings. Furthermore, we found that the addition of NPs to [emim] [BF4] alters the equilibrium of the IL, which consequently improved the stability of the NPs through intermolecular interactions with the two ionic layers (anionic and cationic layers) of the IL. While in the case of [bmim] [Ac], the dispersion of ap-Si NPs was restrained because of the high viscosity of this IL. Graphical abstract Download : Download high-res image (193KB) Download : Download full-size image
quote
| GB/T 7714-2015 | [1] Mohamed R. Tchalala, Jehad K. ElDemellawi, Edy AbouHamad, et al. Applied Materials Today, 2017(9). DOI:10.1016/j.apmt.2017.04.011. |
| MLA | [1] Mohamed R. Tchalala, et al., Applied Materials Today, no. 9, 2017, https://doi.org/10.1016/j.apmt.2017.04.011. |
| APA | [1] Mohamed R. Tchalala, Jehad K. ElDemellawi, Edy AbouHamad, José Ramón Durán Retamal, Purushothaman Varadhan, JrHau He, & Sahraoui Chaieb. (2017). Applied Materials Today(9). https://doi.org/10.1016/j.apmt.2017.04.011 |
| IEEE | [1] Mohamed R. Tchalala, Jehad K. ElDemellawi, Edy AbouHamad, José Ramón Durán Retamal, Purushothaman Varadhan, JrHau He, and Sahraoui Chaieb, Applied Materials Today, no. 9, 2017, doi: 10.1016/j.apmt.2017.04.011. |