Natural wood has been used for construction, fuel, and furniture for thousands of years because of its versatility, renewability, and aesthetic appeal. However, new opportunities for wood are arising as researchers have developed ways to tune the material`s optical, thermal, mechanical, and ionic transport properties by chemically and physically modifying wood`s naturally porous structure and chemical composition. Such modifications can be used to produce sustainable, functional materials for various emerging applications such as automobiles, construction, energy storage, and environmental remediation. In this review, we highlight recent advancements in engineered wood for sustainable technologies, including thermal and light management, environmental remediation, nanofluidics, batteries, and structural materials with high strength-to-weight ratios. Additionally, the current challenges, opportunities, and future of wood research are discussed, providing a guideline for the further development of next-generation, sustainable wood-based materials.
Soft robotics aims to close the performance gap between built and biological machines through materials design. Soft robots are constructed from soft, actuatable materials to be physically intelligent, or to have traits that living organisms possess such as passive adaptability and morphological computation through their compliant, deformable bodies. However, materials selection for physical intelligence often involves low-performance and/or energy-inefficient, stimuli-responsive materials for actuation. Additional challenges in soft robot sensorization and control further limit the practical utility of these machines. Recognizing that electrically controllable materials are crucial for the development of soft machines that are both physically and computationally intelligent, we review progress in the development of electroprogrammable materials for soft robotic actuation. We focus on thermomechanical, electrostatic, and electrochemical actuation strategies that are directly controlled by electric currents and fields. We conclude with an outlook on the design and fabrication of next-generation robotic materials that will facilitate true bioinspired autonomy.
Noncentrosymmetric (NCS) materials feature an exciting array of functionalities such as nonlinear optical (NLO) responses and topological spin textures (skyrmions). While NLO materials and magnetic skyrmions display two different sets of physical properties, their design strategies are deeply connected in terms of atomic-scale precision, structural customization, and electronic tunability. Despite impressive progress in studying these systems separately, a joint road map for navigating the chemical principles for NCS materials remains elusive. This review unites two subtopics of NCS systems, NLO materials and magnetic skyrmions, offering a multifaceted narrative of how to translate the often-abstract fundamentals to the targeted functionalities while inviting innovative approaches from the community. We outline the design principles central to the desired properties by exemplifying relevant examples in the field. We supplement materials chemistry with pertinent electronic structures to demonstrate the power of the fundamentals to create systems integration relevant to foreseeable societal impacts in frequency-doubling instrumentation and spin-based electronics.
Superconductors offer major advantages for the electric power grid, including high current and power capacity, high efficiency arising from the lossless current flow, and a unique current-limiting functionality arising from a superconductor-to-resistive transition. These advantages can be brought to bear on equipment such as underground power cables, fault current limiters, rotating machinery, transformers, and energy storage. The first round of significant commercial-scale superconductor power-equipment demonstrations, carried out during the past decade, relied on a first-generation high-temperature superconductor (HTS) wire. However, during the past few years, with the recent commercial availability of high-performance second-generation HTS wires, power-equipment demonstrations have increasingly been carried out with these new wires, which bring important advantages. The foundation is being laid for commercial expansion of this important technology into the power grid.
Natural wood has been used for construction, fuel, and furniture for thousands of years because of its versatility, renewability, and aesthetic appeal. However, new opportunities for wood are arising as researchers have developed ways to tune the material`s optical, thermal, mechanical, and ionic transport properties by chemically and physically modifying wood`s naturally porous structure and chemical composition. Such modifications can be used to produce sustainable, functional materials for various emerging applications such as automobiles, construction, energy storage, and environmental remediation. In this review, we highlight recent advancements in engineered wood for sustainable technologies, including thermal and light management, environmental remediation, nanofluidics, batteries, and structural materials with high strength-to-weight ratios. Additionally, the current challenges, opportunities, and future of wood research are discussed, providing a guideline for the further development of next-generation, sustainable wood-based materials.
Soft robotics aims to close the performance gap between built and biological machines through materials design. Soft robots are constructed from soft, actuatable materials to be physically intelligent, or to have traits that living organisms possess such as passive adaptability and morphological computation through their compliant, deformable bodies. However, materials selection for physical intelligence often involves low-performance and/or energy-inefficient, stimuli-responsive materials for actuation. Additional challenges in soft robot sensorization and control further limit the practical utility of these machines. Recognizing that electrically controllable materials are crucial for the development of soft machines that are both physically and computationally intelligent, we review progress in the development of electroprogrammable materials for soft robotic actuation. We focus on thermomechanical, electrostatic, and electrochemical actuation strategies that are directly controlled by electric currents and fields. We conclude with an outlook on the design and fabrication of next-generation robotic materials that will facilitate true bioinspired autonomy.
Natural wood has been used for construction, fuel, and furniture for thousands of years because of its versatility, renewability, and aesthetic appeal. However, new opportunities for wood are arising as researchers have developed ways to tune the material`s optical, thermal, mechanical, and ionic transport properties by chemically and physically modifying wood`s naturally porous structure and chemical composition. Such modifications can be used to produce sustainable, functional materials for various emerging applications such as automobiles, construction, energy storage, and environmental remediation. In this review, we highlight recent advancements in engineered wood for sustainable technologies, including thermal and light management, environmental remediation, nanofluidics, batteries, and structural materials with high strength-to-weight ratios. Additionally, the current challenges, opportunities, and future of wood research are discussed, providing a guideline for the further development of next-generation, sustainable wood-based materials.
Soft robotics aims to close the performance gap between built and biological machines through materials design. Soft robots are constructed from soft, actuatable materials to be physically intelligent, or to have traits that living organisms possess such as passive adaptability and morphological computation through their compliant, deformable bodies. However, materials selection for physical intelligence often involves low-performance and/or energy-inefficient, stimuli-responsive materials for actuation. Additional challenges in soft robot sensorization and control further limit the practical utility of these machines. Recognizing that electrically controllable materials are crucial for the development of soft machines that are both physically and computationally intelligent, we review progress in the development of electroprogrammable materials for soft robotic actuation. We focus on thermomechanical, electrostatic, and electrochemical actuation strategies that are directly controlled by electric currents and fields. We conclude with an outlook on the design and fabrication of next-generation robotic materials that will facilitate true bioinspired autonomy.
Noncentrosymmetric (NCS) materials feature an exciting array of functionalities such as nonlinear optical (NLO) responses and topological spin textures (skyrmions). While NLO materials and magnetic skyrmions display two different sets of physical properties, their design strategies are deeply connected in terms of atomic-scale precision, structural customization, and electronic tunability. Despite impressive progress in studying these systems separately, a joint road map for navigating the chemical principles for NCS materials remains elusive. This review unites two subtopics of NCS systems, NLO materials and magnetic skyrmions, offering a multifaceted narrative of how to translate the often-abstract fundamentals to the targeted functionalities while inviting innovative approaches from the community. We outline the design principles central to the desired properties by exemplifying relevant examples in the field. We supplement materials chemistry with pertinent electronic structures to demonstrate the power of the fundamentals to create systems integration relevant to foreseeable societal impacts in frequency-doubling instrumentation and spin-based electronics.