Antifogging Hybrid Materials Based on Amino-Functionalized Polysilsesquioxanes AITranslate

Hiroshima University; Hiroshima University; Hiroshima University; Hiroshima University; Hiroshima University; Hiroshima University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The hybrid antifogging materials poly(3-aminopropyl)silsesquioxane (PAPS) and poly(3-(2-aminoethylaminopropyl)silsesquioxane) (PAEAPS) were prepared by sol–gel reactions that are autocatalyzed by the amine moieties of the monomers. PAPS and PAEAPS show good film-forming abilities, and the films obtained were found to be uniform and pinhole-free. X-ray diffraction analysis of PAPS and PAEAPS films indicated the formation of ladder-like structures. The PAPS and PAEAPS films exhibit high water uptakes of 34 and 42%, which are 1.2 and 1.5 times that of the typical antifogging polymer poly(vinyl alcohol) (PVA), respectively. Furthermore, the PAEAPS film exhibits a scratch resistance 4–6 times that of PVA, and a glass substrate bearing a PAEAPS film remained transparent after removal from a refrigerator. Thus, PAEAPS films exhibit high transparency under humidified conditions and show good antifogging ability.

KeyWords AITranslate

polysilsesquioxane sol−gel reaction antifogging amine moiety hybrid material water uptake scratch resistance
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c00155

Chinese Library Classification Number:

Citation Information:

The hybrid antifogging materials poly(3-aminopropyl)silsesquioxane (PAPS) and poly(3-(2-aminoethylaminopropyl)silsesquioxane) (PAEAPS) were prepared by sol–gel reactions that are autocatalyzed by the amine moieties of the monomers. PAPS and PAEAPS show good film-forming abilities, and the films obtained were found to be uniform and pinhole-free. X-ray diffraction analysis of PAPS and PAEAPS films indicated the formation of ladder-like structures. The PAPS and PAEAPS films exhibit high water uptakes of 34 and 42%, which are 1.2 and 1.5 times that of the typical antifogging polymer poly(vinyl alcohol) (PVA), respectively. Furthermore, the PAEAPS film exhibits a scratch resistance 4–6 times that of PVA, and a glass substrate bearing a PAEAPS film remained transparent after removal from a refrigerator. Thus, PAEAPS films exhibit high transparency under humidified conditions and show good antifogging ability.

quote

GB/T 7714-2015 [1] Tetsuya Maeda, Takashi Hamada, Satoru Tsukada, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.1c00155.
MLA [1] Tetsuya Maeda, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.1c00155.
APA [1] Tetsuya Maeda, Takashi Hamada, Satoru Tsukada, Daiji Katsura, Kenta Okada, & Joji Ohshita. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.1c00155
IEEE [1] Tetsuya Maeda, Takashi Hamada, Satoru Tsukada, Daiji Katsura, Kenta Okada, and Joji Ohshita, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.1c00155. keywords: {polysilsesquioxane;sol−gel reaction;antifogging;amine moiety;hybrid material;water uptake;scratch resistance}