Abstract AITranslate

Brief description is made of the main features and applications of laser technology in the field of material processing in respect of perforing,cutting and welding. And the laser surface modification and la- ser new material preparation is also introduced. Its prospect for development in the near future is pointed out.

KeyWords AITranslate

laser technology material processing development application sintering

1邱小林.激光熔覆TiC金属基陶瓷涂层的研究[J].热加工工艺,2006,35(10):19-22. 被引量:18

2唐英,杨杰.激光熔覆镍基粉末涂层的研究[J].热加工工艺,2004,33(2):16-17. 被引量:14

3Smeggil J G,Funkenbusch A W,Bornstein N S. A relationship between indigenous impurity elements and protective oxide scale adherence characteristics[J]. Metal Trans A,986,17(7) :923-932.

4Tawancy H M,Abbas N M,Bennett A. Role of Y during high temperature oxidation of an M-Cr-Al-Y coating on an Ni-based superalloy[J]. Surf Coat Technol, 1994,68 (2):10-16.

5Czech N, Schmitz F, Stamm W. Improvement of MCr AIY coating by addition of rhenium[J].Surf Coat Technol, 1994,69(7) : 17-21.

6Liu C A, Humphries M J,Krutenat R C. Production of Fe-Cr-Al-Y and Co-Cr-Al-Y coatings by laser surface fusion and their oxidation behavior [J]. Thin Solid Films,1983,107(3):269-275.

7任爱国,王晓静,丁静.激光熔覆止裂技术研究[J].表面技术,2006,35(2):69-71. 被引量:18

8陈畅源,邓琦林,宋建丽.Ni含量及超声振动对激光熔覆中裂纹的影响[J].南京航空航天大学学报,2005,37(B11):44-48. 被引量:42

9宋传旺,李明喜.纳米CeO_2对激光熔覆Ni基合金层组织与性能的影响[J].激光技术,2006,30(3):228-231. 被引量:14

10祝柏林,胡木林,陈俐,谢长生.激光熔覆层开裂问题的研究现状[J].金属热处理,2000,25(7):1-4. 被引量:59

1姚智宏.一种轴承在线激光打标自动送料系统的结构设计[J].激光杂志,2010,31(5):48-49.

2张雷,姚劲松,邢利娜,贾继强,金光.激光加工技术在空间光机结构制造中的应用[J].光机电信息,2011,28(11):8-12. 被引量:1

3何琼,杨晟,范有雄,王英.一种双棒串接大功率固体激光切割系统[J].激光杂志,2012,33(2):44-45.

4姚蔡翔.激光加工的原理、应用现状与展望[J].山东工业技术,2013(15):12-14. 被引量:12

5孟超.钢的表面淬火和化学热处理研究[J].科技致富向导,2014(21):144-144. 被引量:1

6林远添,郭亮,张庆茂,程黄彬,云志强.超短脉冲激光钢箔打孔效果及锥度改善[J].应用激光,2015,35(3):356-362. 被引量:3

7刘晓婉.激光加工技术的研究发展现状[J].中国新技术新产品,2016(18):54-55. 被引量:5

8张文,曾小安,王浩然,邱长军.锆合金表面涂层技术研究现状[J].机械工程师,2017(1):45-47. 被引量:3

9王书亮,付朝政,苏晓慧,付春艳,刘丽,任呈强.激光表面处理技术在石油工业中的应用现状与发展趋势[J].材料保护,2017,50(6):72-78. 被引量:3

10李振华.浅谈现代材料加工技术发展趋势[J].智能城市,2018,4(7):31-32.

1袁荷伟,杨涛.不同金属的激光精细加工技术实验研究[J].应用激光,2020(6):1086-1091. 被引量:6

2李密,胡浩,李建民,邬映臣,雷军,吕文强,石勇,赵娜.激光二极管阵列端面抽运高功率板条激光器技术研究[J].光学学报,2013,33(5):166-170. 被引量:8

3林基辉,李耀,郭栋,戴姣燕,陈垚,徐金富.45钢激光表面铬合金化的制备工艺[J].金属热处理,2018,43(12):170-173. 被引量:9

4李青,王丽红,周波.浅析激光加工技术在光电显示玻璃生产中的发展现状[J].应用激光,2016,36(3):357-362. 被引量:4

5单东栋,赵作福,李鑫,齐锦刚,王建中.20CrMnTi钢渗碳工艺研究进展[J].辽宁工业大学学报:自然科学版,2017,37(2):111-115. 被引量:6

6郭亮,何哲,陈祚堡,朱晓玲,黄龙虎,蔡小军.超快激光合成革透湿性结构制备[J].应用激光,2017,37(3):403-408.

7胡明龙.激光加工技术在无碳小车制作中的应用[J].科技视界,2017(11):105-105. 被引量:2

8程格,栗子林.激光加工技术在五金刀剪行业中的应用分析[J].科技与创新,2018(10):148-149. 被引量:1

9周军,樊湘芳,李涛,邱长军,李怀林.弧电流对多弧离子镀TiAlN涂层表面形貌和性能的影响[J].材料保护,2018,51(6):74-78. 被引量:3

10周黎明,华洋,左忠栋,郭华锋,倪琪,闫士长.基于CAE分析的激光雕刻机设计[J].科技创新导报,2017,14(15):70-72.

1邹日荣.广东省铸造·压铸新技术交流会[J].机电工程技术,2005,34(12).

2Deck.,RF,赵量.马氏体时效钢的近期发展[J].国外低合金钢:合金钢,1989(1):6-10.

3邹敦叙,贾天聪.Ti3Al基合金的近期发展[J].国外金属材料,1990(4):10-16. 被引量:1

4于影霞,何柏林,李力.国内外模具材料的现状及发展趋势[J].热加工工艺,2009,38(2):45-48. 被引量:26

5第十届铸铁科学与加工国际研讨会(SPCI10)[J].现代铸铁,2014(3):24-24.

6沈卓身,汪崧,黄震中.高耐蚀奥氏体合金的新进展[J].石油化工腐蚀与防护,1997,14(3):7-11. 被引量:10

7孙国雄.铸造技术的近期发展[J].国际学术动态,2001(2):19-20.

8沈庆通.感应加热技术的近期发展[J].机械工人:热加工,2005,29(6):12-15. 被引量:6

9吴树森.冲天炉熔技术的近期发展[J].机械工人:冷加工,2000(10):5-6.

10马立群,舒光冀,陈锋.金属熔体在超声场中凝固的研究[J].材料科学与工程,1995,13(4):2-7. 被引量:63

Basic Information:

DOI:

Chinese Library Classification Number:TG156.99[金属学及工艺—热处理]

Citation Information:

Brief description is made of the main features and applications of laser technology in the field of material processing in respect of perforing,cutting and welding. And the laser surface modification and la- ser new material preparation is also introduced. Its prospect for development in the near future is pointed out.

quote

GB/T 7714-2015 [1] QIU Xing-wu. Development and Application of Laser Technology in the Field of Material Processing[J]. Rare Metals and Cemented Carbides, 2010(1): 60-63.
MLA [1] QIU Xing-wu. "Development and Application of Laser Technology in the Field of Material Processing." Rare Metals and Cemented Carbides, no. 1, 2010, pp. 60-63.
APA [1] QIU Xing-wu. (2010). Development and Application of Laser Technology in the Field of Material Processing. Rare Metals and Cemented Carbides(1), 60-63.
IEEE [1] QIU Xing-wu, "Development and Application of Laser Technology in the Field of Material Processing," Rare Metals and Cemented Carbides, no. 1, pp. 60-63, 2010. keywords: {laser technology;material processing;development;application;sintering}