Defect-Engineering of Anionic Porous Aromatic Frameworks for Ammonia Capture AITranslate

East China University of Science and Technology; East China University of Science and Technology; East China University of Science and Technology; East China University of Science and Technology; Shanghai Advanced Research Institute (SARI); East China University of Science and Technology; East China University of Science and Technology; East China University of Science and Technology; East China University of Science and Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Defects in many types of porous materials have been demonstrated for controlling the pore size distribution and specific surface area as well as manipulating chemical functionality, which strongly affects their mass-transport pathways and gas adsorption behaviors. Here, unraveled structural evidence for the presence of defects in porous ionic polymers (PIPs) with weakly coordinating anions is presented. We present the concise synthesis of a tetraphenylborate-based anionic porous framework, which allows for the construction of PIPs with tricoordinated boron vacancies via a defect-engineering strategy. The resultant PIP-X possesses a high surface area of 935 m2 g–1 and displays excellent chemical stability in water and organic solvents. Importantly, the controllable vacancies and porosity of polymers were investigated using the solid-state nuclear magnetic technique. The prepared polymer (Cu@PIP-X) has multiple active sites that contain charged skeletons, Lewis acid defects, and metal ions and thus exhibits improved ammonia (NH3) adsorption performance compared with a neutral polymer (PAF-1) and a defect-free polymer (PIP-H). Notably, the strong interactions between the gas molecules and the PIP-X are reversible with simple heating to 100 °C and display outstanding recyclable ability without structure collapse. This work thereby provides a perspective to develop defective anionic polymers as a versatile type of ion-exchange material for gas uptake.

KeyWords AITranslate

defectengineering porous polymers anionic porous aromatic frameworks ammonia capture adsorption mechanism
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c00589

Chinese Library Classification Number:

Citation Information:

Defects in many types of porous materials have been demonstrated for controlling the pore size distribution and specific surface area as well as manipulating chemical functionality, which strongly affects their mass-transport pathways and gas adsorption behaviors. Here, unraveled structural evidence for the presence of defects in porous ionic polymers (PIPs) with weakly coordinating anions is presented. We present the concise synthesis of a tetraphenylborate-based anionic porous framework, which allows for the construction of PIPs with tricoordinated boron vacancies via a defect-engineering strategy. The resultant PIP-X possesses a high surface area of 935 m2 g–1 and displays excellent chemical stability in water and organic solvents. Importantly, the controllable vacancies and porosity of polymers were investigated using the solid-state nuclear magnetic technique. The prepared polymer (Cu@PIP-X) has multiple active sites that contain charged skeletons, Lewis acid defects, and metal ions and thus exhibits improved ammonia (NH3) adsorption performance compared with a neutral polymer (PAF-1) and a defect-free polymer (PIP-H). Notably, the strong interactions between the gas molecules and the PIP-X are reversible with simple heating to 100 °C and display outstanding recyclable ability without structure collapse. This work thereby provides a perspective to develop defective anionic polymers as a versatile type of ion-exchange material for gas uptake.

quote

GB/T 7714-2015 [1] YuShu Han, Shuhao An, Jialin Dai, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.1c00589.
MLA [1] YuShu Han, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.1c00589.
APA [1] YuShu Han, Shuhao An, Jialin Dai, Jun Hu, Qing Xu, Fan Song, Mingyan Li, Changjun Peng, & Honglai Liu. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.1c00589
IEEE [1] YuShu Han, Shuhao An, Jialin Dai, Jun Hu, Qing Xu, Fan Song, Mingyan Li, Changjun Peng, and Honglai Liu, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.1c00589. keywords: {defectengineering;porous polymers;anionic porous aromatic frameworks;ammonia capture;adsorption mechanism}