Experimental Study on Direct Acid Leaching of Scandium from V-Ti Magnetite Tailings AITranslate
Abstract AITranslate
The content of Sc2O3in the tailings of Bijigou vanadium-titanium magnetite in Yang County,Shaanxi Province is 97.08 g/t.In order to fully recover the rare earth resources,scandium was leached by direct acid leaching,and the effects of acid type and dosage,aid-leaching agent type and dosage,leaching temperature,leaching liquid-solid ratio,leaching time,and feed fineness on the leaching rate of scandium were systematically studied.The results show that without the addition of aid-leaching agent,the leaching effects of H2SO4,HCl,H2SO4+HF,and HCl+HF on scandium in tailings are very poor,but the leaching rate by HCl is higher than that by H2SO4.Adding 2#aid-leaching agent in HCl system can significantly increase the leaching rate of scandium.When the tailings are ground to a fineness of-0.075 mm paticles accounting for 80%,the leaching rate of scandium can reach 89.53%under the optimal conditions of 2#aid-leaching agent dosage of 15%,HCl concentration of 6 mol/L,liquid-solid ratio of 3∶1,leaching temperature of 90℃,and leaching time of 6 h.The direct acid leaching process has a high leaching rate of scandium and is more operatable,which can promote the development of recovering scandium from tailings.
KeyWords AITranslate
1孙军,刘云龙,崔滔.我国钪矿资源概况及产业发展建议[J].资源与产业,2019,21(2):74-79. 被引量:11
2刘勇,刘珍珍,刘牡丹,周吉奎,马致远.稀有金属富集渣中稀土和钪的提取[J].有色金属:冶炼部分,2017(12):40-42. 被引量:2
3董方,高利坤,陈龙,王鹏,马方通.钪的资源及回收提取技术发展现状[J].矿产综合利用,2016,0(4):21-26. 被引量:17
4樊艳金,何航军,张建飞,黄泰元.钛白废酸与赤泥联合提取氧化钪的工艺研究[J].有色金属:冶炼部分,2015(5):55-57. 被引量:17
5刘蕊,陈金珠,刘子琪,任家樑.从拜耳法赤泥中提取钪[J].应用化工,2021,50(6):1743-1745. 被引量:4
6许延辉,马升峰,赵文怡,孟志军,刘海蛟,王英杰.氯化钙焙烧盐酸分解提取白云鄂博选铌尾矿中的钪[J].稀土,2014,35(6):106-109. 被引量:15
7黄霞光,罗国清,李亚平.攀西钒钛磁铁矿中钪的赋存状态研究[J].有色金属:选矿部分,2016(6):1-4. 被引量:16
8谭俊峰,张桂芳,张昱,张宗华.复杂硅酸盐含钪精矿钪浸出助浸剂试验研究[J].稀有金属,2012,36(2):304-310. 被引量:9
9李梅,耿金龙,高凯,张栋梁,周富强,郭财胜.白云鄂博尾矿中钪的浸出及铌富集物制备工艺研究[J].稀土,2017,38(5):111-119. 被引量:7
10黄雯孝,卢可可.攀西钒钛磁铁矿尾矿中钪的提取工艺研究[J].矿产综合利用,2020(2):135-139. 被引量:10
1葛阳阳,孟建卫,张凯熙,郭静粉.含氟助剂两段酸浸提取钒钛磁铁矿尾矿中的钪[J].稀土,2022,43(4):73-80. 被引量:2
2滕青,杨志超,王洪君.直接酸浸-溶剂萃取法从废油加氢催化剂中回收钒和镍[J].中国有色金属学报:英文版,2023,33(1):325-336. 被引量:1
3黄开良,温武深,黄乐,廖蔚峰.从退役磷酸铁锂电池拆解极粉回收电池级磷酸铁研究[J].当代化工研究,2023(2):28-30.
4王威,杨星晨,柳林,刘红召,王洪亮,曹耀华.低共熔溶剂浸出废旧锰酸锂电池正极材料锂和锰的研究[J].矿产保护与利用,2023,43(1):128-131.
5方娴.提高某选矿厂金回收率的试验研究[J].有色冶金设计与研究,2023,44(1):5-7.
6徐灏.燃气轮机组SCR脱硝中试试验研究[J].中文科技期刊数据库(全文版)工程技术,2023(4):0005-0009.
7安浩,曾曼,余浩然,张文艺,彭明国,毛林强.基于响应曲面法的钠化焙烧-水浸法回收废加氢催化剂中有价金属工艺优化[J].环境工程学报,2023,17(1):259-267.
8陈炳旭,杜浩,李兰杰,王少娜,刘彪,李昊男,祁健,周冰晶.失活硫酸催化剂资源化利用研究进展[J].河北冶金,2022(10):1-8.
9余洪,程彦玲,宋文强,陈官华,张汉泉,刘明霞.黄铁矿伴生金回收研究进展[J].武汉工程大学学报,2023,45(1):9-14.
10罗平坤,刘博锐.攀西钒钛磁铁矿尾矿库生态恢复方案研究[J].中国科技期刊数据库 工业A,2021(9):0069-0069.
Basic Information:
DOI:
Chinese Library Classification Number:TF854[冶金工程—有色金属冶金]
Citation Information:
The content of Sc2O3in the tailings of Bijigou vanadium-titanium magnetite in Yang County,Shaanxi Province is 97.08 g/t.In order to fully recover the rare earth resources,scandium was leached by direct acid leaching,and the effects of acid type and dosage,aid-leaching agent type and dosage,leaching temperature,leaching liquid-solid ratio,leaching time,and feed fineness on the leaching rate of scandium were systematically studied.The results show that without the addition of aid-leaching agent,the leaching effects of H2SO4,HCl,H2SO4+HF,and HCl+HF on scandium in tailings are very poor,but the leaching rate by HCl is higher than that by H2SO4.Adding 2#aid-leaching agent in HCl system can significantly increase the leaching rate of scandium.When the tailings are ground to a fineness of-0.075 mm paticles accounting for 80%,the leaching rate of scandium can reach 89.53%under the optimal conditions of 2#aid-leaching agent dosage of 15%,HCl concentration of 6 mol/L,liquid-solid ratio of 3∶1,leaching temperature of 90℃,and leaching time of 6 h.The direct acid leaching process has a high leaching rate of scandium and is more operatable,which can promote the development of recovering scandium from tailings.
quote
| GB/T 7714-2015 | [1] LIANG Xiao, NIU Fang-yin, WANG Yong-hai, et al. Experimental Study on Direct Acid Leaching of Scandium from V-Ti Magnetite Tailings[J]. Rare Metals and Cemented Carbides, 2023(1): 5-9. |
| MLA | [1] LIANG Xiao, et al., "Experimental Study on Direct Acid Leaching of Scandium from V-Ti Magnetite Tailings." Rare Metals and Cemented Carbides, no. 1, 2023, pp. 5-9. |
| APA | [1] LIANG Xiao, NIU Fang-yin, WANG Yong-hai, GUO Cai-lian, & GUO Yue-qin. (2023). Experimental Study on Direct Acid Leaching of Scandium from V-Ti Magnetite Tailings. Rare Metals and Cemented Carbides(1), 5-9. |
| IEEE | [1] LIANG Xiao, NIU Fang-yin, WANG Yong-hai, GUO Cai-lian, and GUO Yue-qin, "Experimental Study on Direct Acid Leaching of Scandium from V-Ti Magnetite Tailings," Rare Metals and Cemented Carbides, no. 1, pp. 5-9, 2023. keywords: {V-Ti magnetite tailings;scandium;aid-leaching agent;acid leaching;HCl} |