Experimental validation of analytical solutions for estimating the minimum required strength of side-exposed backfill in underground mines AITranslate

Polytechnique Montreal;Research Institute on Mines and the Environment(RIME UQAT-Polytechnique)
AITranslate
Publisher: Youke Publishing Co., Ltd.
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

In underground mining with backfill,it is essential to evaluate the minimum required strength of side-exposed backfill.An analytical solution proposed by Mitchell and coworkers in 1982 is largely used.Since 2012,Li and coworkers have published several improved solutions,accounting for several limitations in the Mitchell 1982 model.However,the improved solutions have not fully been validated by experimental results.Experimental work is necessary.As such,box instability tests were performed using an uncemented paste backfill under undrained conditions with a high aspect ratio stope.The unconfined compressive strength of the backfill was measured.Comparisons between experimental results and analytical results were made.A part of the experimental results was used to obtain the missing parameters through calibration.The other part of experimental results was then used to test the predictive capability of the calibrated analytical solutions.The results show that the improved analytical solutions provide a better agreement with the experimental results than the original Mitchell solution,at least for short-term stability of side-exposed backfill submitted to quasi-unconsolidated and undrained conditions.More experimental works are necessary to test the validity of the improved solutions under wider conditions.

KeyWords AITranslate

box instability tests experimental validation paste backfill side-exposed backfill Mitchell's solution
No data

Basic Information:

DOI:

Chinese Library Classification Number:TD803[矿业工程—矿山开采]

Citation Information:

In underground mining with backfill,it is essential to evaluate the minimum required strength of side-exposed backfill.An analytical solution proposed by Mitchell and coworkers in 1982 is largely used.Since 2012,Li and coworkers have published several improved solutions,accounting for several limitations in the Mitchell 1982 model.However,the improved solutions have not fully been validated by experimental results.Experimental work is necessary.As such,box instability tests were performed using an uncemented paste backfill under undrained conditions with a high aspect ratio stope.The unconfined compressive strength of the backfill was measured.Comparisons between experimental results and analytical results were made.A part of the experimental results was used to obtain the missing parameters through calibration.The other part of experimental results was then used to test the predictive capability of the calibrated analytical solutions.The results show that the improved analytical solutions provide a better agreement with the experimental results than the original Mitchell solution,at least for short-term stability of side-exposed backfill submitted to quasi-unconsolidated and undrained conditions.More experimental works are necessary to test the validity of the improved solutions under wider conditions.

quote

GB/T 7714-2015 [1] Islem Titey, Li Li. MetaResource, 2026(1): 62-71.
MLA [1] Islem Titey, and Li Li. MetaResource, no. 1, 2026, pp. 62-71.
APA [1] Islem Titey, & Li Li. (2026). MetaResource(1), 62-71.
IEEE [1] Islem Titey and Li Li, MetaResource, no. 1, pp. 62-71, 2026.