Study of Technological Conditions of Chemically-plated Ni-B Alloy AITranslate

Kunming Metallurgical Research Institute;Kunming Metallurgical Research Institute;Kunming Metallurgical Research Institute
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Study is made of the impact of plating solution composition and technological conditions on the sedimentation velocity of Ni-B alloy. Proper technological conditions of chemically-plated Ni-B alloy is selected, based on which amorphous Ni-B alloy layer is obtained containing 4.508% boron with good corrosion resistance.

KeyWords AITranslate

chemical-plating amorphous Ni-B alloy technological condition corrosion resistance

1王丽丽.化学镀Ni-B合金工艺[J].电镀与精饰,1998,20(5):38-41. 被引量:6

2陶开斌.铝基体化学镀镍硼合金探讨[A]..北京:中国电子学会电镀专业委员会第七届电子电镀年会论文集[C].,1998.196.

3王孝镕,顾慰中.化学镀镍磷合金工艺研究[J].电镀与涂饰,1999,18(2):43-46. 被引量:16

4沃尔夫冈 里德尔.化学镀镍[M].上海:交通大学出版社,1996..

5叶康明.金属腐蚀与防护理论[M].北京:高等教育出版社,1993..

1张祖军.长效自润滑耐磨耐蚀复合镀层制备工艺及性能研究[J].腐蚀与防护,2008,29(2):69-70. 被引量:1

2闫洪.2004年云南金属材料与加工年评[J].云南冶金,2005,34(2):40-49.

3张祖军,王勇.铝合金化学镀Ni-P/Ni-B双层复合镀层及其性能研究[J].材料导报,2006,20(F11):342-344. 被引量:5

4陈四海,彭奇龄,周海晖,余强,旷亚非.碳纤维表面电沉积合金(复合)镀层初步研究[J].电镀与涂饰,2008,27(7):1-3. 被引量:1

5周晓荣,胡宇,方华,徐玉玲,陈红梅,程四清.碱性条件下Fe-P-B合金电镀[J].材料保护,2009,42(10):37-39. 被引量:1

6陈艳芳,李倩,苌清华,高战,韩剑,熊毅.镀液pH值对铝合金表面化学镀Ni-P合金镀层性能的影响[J].轻合金加工技术,2010,38(8):47-49. 被引量:1

7苌清华,吴继龙,林亚威,关鹏娜,陈奎元,熊毅.还原剂对AZ31B镁合金表面化学镀Ni-B合金性能的影响[J].轻合金加工技术,2011,39(5):52-54. 被引量:1

1赵斌,董世知.铝合金化学镀Ni-P合金的研究进展[J].电镀与涂饰,2008,27(1):24-26. 被引量:9

2张立红,李宁,尹显明.P含量对Ni-P镀层的性能影响分析[J].洛阳理工学院学报:自然科学版,2009,19(3):21-24. 被引量:6

3王崇蕊,郝建军,董春艳,刘新院.代银镀层技术研究进展[J].电镀与精饰,2011,33(2):24-27. 被引量:1

4王锦,李东红,仓向辉,张明惠.络合剂对铝基化学镀Ni-Cu-P合金性能的影响[J].轻金属,2011(8):68-71. 被引量:3

5孟栋,宣天鹏,王峰.电沉积三元铁基非晶磁性合金薄膜的研究进展[J].电镀与精饰,2012,34(5):12-16. 被引量:1

6袁庆龙,凌文丹,李平.电刷镀Ni-Co-W/Y_2O_3复合镀层的组织与摩擦磨损特性[J].稀有金属,2012,36(4):557-562. 被引量:4

7冯立,何为,黄雨新,何杰,徐缓.改善印制电路板化学镀镍耐蚀性的研究进展[J].电镀与涂饰,2013,32(9):39-42. 被引量:1

8王丽雪,王春艳,于久灏,郭丽丽.碳纤维表面化学镀预处理工艺研究[J].黑龙江工程学院学报,2017,31(2):49-52. 被引量:3

9张红娟,南雁,乔平,朱光辉,刘谦文.机载统型模块防腐性能研究[J].科技风,2020,0(2):148-149.

10孔琳,刘品潇,孔斌.A3钢表面化学镀Ni-P/Ni-Mo-P双层镀层[J].电镀与精饰,2021,43(1):25-30. 被引量:2

1陈艳芳,陈春梅,介亚菲,孟龙,熊毅.温度对AZ31B镁合金表面化学镀Ni-B合金性能的影响[J].轻合金加工技术,2011,39(2):39-41. 被引量:4

2胡石林,刘利辉.化学镀非晶态Ni-B合金的研究[J].核化学与放射化学,1989,11(3):183-188. 被引量:1

3闫洪.非晶态Ni-B合金镀层的组织结构和耐蚀性的实验研究[J].冶金标准化与质量,2005,43(6):23-25. 被引量:1

4苌清华,苌真真,盛俊豪,彭叠.主盐对镁合金表面化学镀Ni-B合金性能的影响[J].热加工工艺,2011,40(6):109-111.

5陈儒军,伍翠兰,洪小丽,潘建新.热处理对化学镀Ni-B合金镀层微观结构的影响[J].金属热处理,2011,36(12):102-104. 被引量:1

6杨昌英,潘家荣,李昕,周俊婷,李远志.以非晶态Ni-B合金阴极电解还原葡萄糖[J].三峡大学学报:自然科学版,2002,24(4):382-384. 被引量:1

7郭春科,刘静安.减少铝合金棒材缩尾的工艺条件研究[J].铝加工,2007,30(1):39-42.

8陈儒军,伍翠兰,潘建新,刘恺.化学镀Ni-B合金镀层的微观结构[J].金属热处理,2011,36(7):88-91. 被引量:3

9宣天鹏,邓宗钢.热处理对化学镀Ni-B合金层结构和耐磨性的影响[J].金属热处理学报,1994,15(1):37-41. 被引量:2

10陈儒军,伍翠兰,洪小丽,潘建新.化学镀层的微观结构研究方法探讨[J].热加工工艺,2011,40(20):122-125. 被引量:1

Basic Information:

DOI:

Chinese Library Classification Number:TG139.8[一般工业技术—材料科学与工程]

Citation Information:

Study is made of the impact of plating solution composition and technological conditions on the sedimentation velocity of Ni-B alloy. Proper technological conditions of chemically-plated Ni-B alloy is selected, based on which amorphous Ni-B alloy layer is obtained containing 4.508% boron with good corrosion resistance.

quote

GB/T 7714-2015 [1] YAN Hong, ZUO Jing, DU Qiang. Study of Technological Conditions of Chemically-plated Ni-B Alloy[J]. Rare Metals and Cemented Carbides, 2004(1): 11-15.
MLA [1] YAN Hong, et al., "Study of Technological Conditions of Chemically-plated Ni-B Alloy." Rare Metals and Cemented Carbides, no. 1, 2004, pp. 11-15.
APA [1] YAN Hong, ZUO Jing, & DU Qiang. (2004). Study of Technological Conditions of Chemically-plated Ni-B Alloy. Rare Metals and Cemented Carbides(1), 11-15.
IEEE [1] YAN Hong, ZUO Jing, and DU Qiang, "Study of Technological Conditions of Chemically-plated Ni-B Alloy," Rare Metals and Cemented Carbides, no. 1, pp. 11-15, 2004. keywords: {chemical-plating;amorphous Ni-B alloy;technological condition;corrosion resistance}