Abstract AITranslate

Nanoscale control over pore surface properties is a challenging objective for nanopore research and could enable advanced bioanalytical applications, along with enhanced precision and accuracy of existing measurement processes. This work reports a one-pot strategy for the functionalization of thermoplastic polyurethane (TPU) tunable nanopores with polymer brushes. These elastomeric pores are used for tunable resistive pulse sensing (TRPS), which can detect and analyze a broad range of microparticle and nanoparticle species in aqueous electrolytes. Grafting is achieved using the recently developed Graftfast method, via the chemical reduction of diazonium salts. The study focuses on Graftfast of negatively charged poly(acrylic acid) (PAA) brushes. The method is further exemplified through the grafting of neutral brushes with a view to utilizing their possible antifouling properties: zwitterionic poly(sulfobetaine), 2-hydroxyethyl methacrylate, and poly(ethylene glycol) methyl ethermethacrylate. The successful TPU functionalization was characterized using Fourier transform infrared spectroscopy, contact angle measurements, and X-ray photoelectron spectroscopy. For PAA-grafted pores, the TRPS configuration was used for studies of ionic current rectification, streaming potential, and resistive pulse durations for 500-nm-diameter carboxylated polystyrene spheres. Results were consistent with increased negative surface charge on the pore walls, confirming successful pore functionalization.

KeyWords AITranslate

nanopore functionalization graftfast tunable resistive pulse sensing ion current rectification nanopore surface charge
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.0c01087

Chinese Library Classification Number:

Citation Information:

Nanoscale control over pore surface properties is a challenging objective for nanopore research and could enable advanced bioanalytical applications, along with enhanced precision and accuracy of existing measurement processes. This work reports a one-pot strategy for the functionalization of thermoplastic polyurethane (TPU) tunable nanopores with polymer brushes. These elastomeric pores are used for tunable resistive pulse sensing (TRPS), which can detect and analyze a broad range of microparticle and nanoparticle species in aqueous electrolytes. Grafting is achieved using the recently developed Graftfast method, via the chemical reduction of diazonium salts. The study focuses on Graftfast of negatively charged poly(acrylic acid) (PAA) brushes. The method is further exemplified through the grafting of neutral brushes with a view to utilizing their possible antifouling properties: zwitterionic poly(sulfobetaine), 2-hydroxyethyl methacrylate, and poly(ethylene glycol) methyl ethermethacrylate. The successful TPU functionalization was characterized using Fourier transform infrared spectroscopy, contact angle measurements, and X-ray photoelectron spectroscopy. For PAA-grafted pores, the TRPS configuration was used for studies of ionic current rectification, streaming potential, and resistive pulse durations for 500-nm-diameter carboxylated polystyrene spheres. Results were consistent with increased negative surface charge on the pore walls, confirming successful pore functionalization.

quote

GB/T 7714-2015 [1] Anupama Rao Gulur Srinivas, Rafiq Hilali, Mona Damavandi, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.0c01087.
MLA [1] Anupama Rao Gulur Srinivas, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.0c01087.
APA [1] Anupama Rao Gulur Srinivas, Rafiq Hilali, Mona Damavandi, Jenny Malmstrom, David Barker, Eva Weatherall, Geoff Willmott, & Jadranka TravasSejdic. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.0c01087
IEEE [1] Anupama Rao Gulur Srinivas, Rafiq Hilali, Mona Damavandi, Jenny Malmstrom, David Barker, Eva Weatherall, Geoff Willmott, and Jadranka TravasSejdic, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.0c01087. keywords: {nanopore functionalization;graftfast;tunable resistive pulse sensing;ion current rectification;nanopore surface charge}