Freezing-Tolerant Hydrogel Composed of Sulfonated Chitosan and Poly(vinyl alcohol) Featuring Excellent Stretchability and High Proton Conduction AITranslate

Nanjing Tech University; Nanjing Tech University; Nanjing Tech University; Nanjing Tech University; Nanjing University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites
111111

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Antifreezing and highly proton-conductive hydrogels show promising applications in flexible electrochemical devices owing to their inherent stretchability and safety. In this study, we chose an ethylene glycol/water (EG/H2O) binary mixture as the solvent, sulfonated chitosan (CS-SO3H) as the proton-conducting component, and the blend of CS-SO3H and poly(vinyl alcohol) (PVA) as a gelator to prepare double-network hydrogels, CS-SO3H@PVA-X (X represents the mass ratio of CS-SO3H and PVA with a value of 0, 0.5, 1.0, and 1.5), which are characterized by different techniques, including microanalysis, IR, 1H and 13C NMR spectra, TG, PXRD, and so on. CS-SO3H@PVA-X hydrogels exhibit excellent tensile strength, toughness, and a freezing-tolerant feature. Importantly, CS-SO3H@PVA-1.5 hydrogel displays not only high proton conduction in a wide range of temperatures from −35 to 70 °C, with proton conductivities of 7.2 × 10–4 S cm–1 at −35 °C and 4.56 × 10–2 S cm–1 at 70 °C and ambient humidity, but also exceptional mechanical performance, with a tensile strength of 3.11 MPa and an elongation at break of 423%, indicative of a potential application in electrochemical devices relying on proton transport and operating at extreme conditions. It is also discovered for the first time that the double-network micelles are entangled together to form the spiral crimped texture in hydrogels CS-SO3H@PVA-X (X = 1.0 and 1.5).

KeyWords AITranslate

sulfonated chitosan poly(vinyl alcohol) antifreezing hydrogel doublenetwork hydrogel widetemperature Show More
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c01824

Chinese Library Classification Number:

Citation Information:

Antifreezing and highly proton-conductive hydrogels show promising applications in flexible electrochemical devices owing to their inherent stretchability and safety. In this study, we chose an ethylene glycol/water (EG/H2O) binary mixture as the solvent, sulfonated chitosan (CS-SO3H) as the proton-conducting component, and the blend of CS-SO3H and poly(vinyl alcohol) (PVA) as a gelator to prepare double-network hydrogels, CS-SO3H@PVA-X (X represents the mass ratio of CS-SO3H and PVA with a value of 0, 0.5, 1.0, and 1.5), which are characterized by different techniques, including microanalysis, IR, 1H and 13C NMR spectra, TG, PXRD, and so on. CS-SO3H@PVA-X hydrogels exhibit excellent tensile strength, toughness, and a freezing-tolerant feature. Importantly, CS-SO3H@PVA-1.5 hydrogel displays not only high proton conduction in a wide range of temperatures from −35 to 70 °C, with proton conductivities of 7.2 × 10–4 S cm–1 at −35 °C and 4.56 × 10–2 S cm–1 at 70 °C and ambient humidity, but also exceptional mechanical performance, with a tensile strength of 3.11 MPa and an elongation at break of 423%, indicative of a potential application in electrochemical devices relying on proton transport and operating at extreme conditions. It is also discovered for the first time that the double-network micelles are entangled together to form the spiral crimped texture in hydrogels CS-SO3H@PVA-X (X = 1.0 and 1.5).

quote

GB/T 7714-2015 [1] Qiao Qiao, ZhiRong Feng, YaRu Kong, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.1c01824.
MLA [1] Qiao Qiao, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.1c01824.
APA [1] Qiao Qiao, ZhiRong Feng, YaRu Kong, YuPing Wu, & XiaoMing Ren. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.1c01824
IEEE [1] Qiao Qiao, ZhiRong Feng, YaRu Kong, YuPing Wu, and XiaoMing Ren, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.1c01824. keywords: {sulfonated chitosan;poly(vinyl alcohol);antifreezing hydrogel;doublenetwork hydrogel;widetemperature;Show More}