Preparation and Adsorption Properties of Polyaluminum Ferric Chloride from Red Mud AITranslate

College of Chemistry and Chemical Engineering,Henan Polytechnic University;College of Chemistry and Chemical Engineering,Henan Polytechnic University;College of Chemistry and Chemical Engineering,Henan Polytechnic University;College of Chemistry and Chemical Engineering,Henan Polytechnic University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Polyaluminum ferric chloride(PAFC) was prepared from acid leaching solution obtained by hydrochloric acid leaching of red mud,and its performance of kaolin wastewater treatment was studied.The effects of hydrochloric acid concentration,leaching temperature,leaching time and liquid-solid ratio on the leaching rate of Al and Fe in red mud were investigated.Also the effects of PAFC dosage,kaolin quality concentration,wastewater pH value and water temperature on the turbidity removal rate of kaolin during wastewater treatment with PAFC were studied.The experimental results show that the leaching rate of Al and Fe is 76.5% and 33.7%,respectively,under the conditions of 50% hydrochloric acid concentration,80 ℃ leaching temperature,1.5 h leaching time and 5 mL/g liquid-solid ratio.The highest turbidity removal rate of PAC for kaolin wastewater treatment is 90%,while that of self-made PAFC is 94%,under the conditions of PAC/PAFC dosage of 8 mL(10 g/L),wastewater pH value of 7.0,kaolin suspension(mass concentration 125 mg/L) volume of 500 mL and wastewater temperature of 20 ℃.

KeyWords AITranslate

red mud acid leaching polyaluminum ferric chloride kaolin wastewater turbidity removal rate

1王倩,周律,羊小玉.复合混凝剂PAFC-PDA制备及处理模拟废水的效果[J].工业水处理,2018,38(1):15-19. 被引量:3

2常军,邵延海,李硕,蒋丰祥,张校熔.赤泥中有价金属元素综合回收研究现状及进展[J].矿冶,2017,26(3):59-63. 被引量:18

3廖春发,卢惠明,邱定蕃,许秀莲.从赤泥中综合回收有价金属工艺的研究进展[J].轻金属,2003(10):18-22. 被引量:56

4孙康康,张凌燕,刘理根,李成伟.赤泥强磁尾矿制备水处理陶粒滤料的研究[J].硅酸盐通报,2016,35(7):2270-2275. 被引量:8

5李望,朱晓波,管学茂.赤泥化学选矿制备富钛渣的研究[J].稀有金属与硬质合金,2016,44(4):25-27. 被引量:5

6王清涛,李森,于华芹,李峰芝,乔海波,徐会君,刘俊成,杜庆洋.利用赤泥制备轻质高强保温装饰一体化建筑材料[J].硅酸盐通报,2018,37(4):1393-1398. 被引量:17

7梁媛,陈均宁.赤泥的危害及综合利用[J].大众科技,2014,16(7):33-34. 被引量:19

8南相莉,张廷安,刘燕,豆志河.我国赤泥综合利用分析[J].过程工程学报,2010,10(S1):264-270. 被引量:127

9刘万超,闫琨,和新忠,张朝普,吴国亮.拜耳法赤泥制备地聚物类无机聚合材料的研究进展[J].硅酸盐通报,2016,35(2):453-457. 被引量:13

1朱晓波,巩文辉,李望.赤泥活化焙烧-联合浸出制备富钛料及组分溶解行为[J].中国有色金属学报,2021,31(8):2227-2237. 被引量:8

2李望,白雪雨,朱晓波.以赤泥为原料制备聚合铝铁絮凝剂进行高浊度废水处理的综合性实验[J].实验技术与管理,2022,39(1):126-129. 被引量:3

3黄涛,黄自力,肖硕,郑洁淼,刘晓峰.用盐酸从强磁铁尾矿中浸出铁及其动力学研究[J].湿法冶金,2023,42(1):13-17.

4王丽娟,燕可洲,郭志强,赵仲鹤,郭彦霞,程芳琴.钠盐活化赤泥-煤矸石酸浸液制备聚合氯化铝[J].无机盐工业,2023,55(4):76-83.

1陈雪,何林兰,罗登丽,郑雪梅,马爱元.赤泥常规干燥工艺实验研究[J].当代化工研究,2022(8):152-154.

2黄小芬,李先海,卯松,沈智慧.基于专题实验的矿物加工研究方法教学实践[J].集成电路应用,2022,39(7):277-279.

3阮耀阳,邓博纳,刘明霞,周芳.赤泥中有价组分梯级分离综合性实验[J].实验技术与管理,2022,39(8):167-171.

4王玲,周晨晨,范燕青,马保中,王成彦,傅昕.赤泥转型-碱溶提铝过程钛的矿相转化[J].中国有色金属学报,2022,32(9):2714-2725.

5武兵强,高建军,万新宇,齐渊洪.赤泥铁精粉直接还原实验研究[J].矿冶工程,2022,42(6):139-141. 被引量:1

6杨小慧,李望,朱晓波.D751螯合树脂吸附酸性溶液中钒(Ⅳ)离子的机制[J].中国有色金属学报,2022,32(12):3862-3870.

7黄钰华,莫伟,封金鹏,任汝龙,何春彦,苏秀娟.硫酸/草酸体系下拜耳法赤泥中铁铝浸出行为的差异[J].有色金属:冶炼部分,2023(2):34-43. 被引量:1

8吴小华,李雯霏.广西高铁赤泥高值化综合利用途径[J].中国有色冶金,2023,52(2):104-115. 被引量:2

9王虹,方树林.阳离子淀粉-聚硅酸复合絮凝剂制备及污水处理性能[J].化学工程师,2023,37(4):47-51.

10杨慧,房辉,程志远,郭丰佳,汲庆涛,麻芳,彭倩倩.赤泥资源化综合利用研究进展[J].中国资源综合利用,2023,41(6):109-115.

1肖彩霞,薛廉吉.粗制钴盐常压氨浸工艺研究[J].有色设备,2019,0(4):16-19. 被引量:2

2马巧珊,范方方.赤泥基聚合硫酸铝铁絮凝剂的制备与应用研究[J].山东化工,2018,47(24):201-203. 被引量:3

3杨轶霞,陈浩龙.PLC在污水处理模糊控制中的应用[J].数字技术与应用,2019,37(8):9-9.

4陆淑娟,张伟东,郭明,王英华,孙鲲,张淑芳.人工流产手术后PAC服务的临床研究[J].医学信息:医学与计算机应用,2014,0(4):101-101. 被引量:1

5王卫杰,张勇,金旭,田洋名,崔科丛,姚菊明.纤维素-丝胶全降解绿色絮凝材料制备及其混凝性能评价[J].浙江理工大学学报:自然科学版,2018,39(2):157-162. 被引量:2

6车贤.保护碱对焙烧氰化工艺金银浸出率影响的试验研究[J].中国资源综合利用,2019,37(10):14-16. 被引量:1

7郭学益,张磊,田庆华,于大伟,石靖,易宇.富铅锑含砷烟尘中砷的选择性脱除(英文)[J].中国有色金属学报:英文版,2019,29(10):2213-2221. 被引量:7

8尹升华,陈威,刘家明,宋庆.次生硫化铜矿制粒试验[J].工程科学学报,2019,0(9):1127-1134. 被引量:5

9朱啸林,徐存英,唐杰,华一新,张启波,刘海,王祥,黄梦婷.利用氯化胆碱基低共熔溶剂从氧化锌烟尘中选择性回收锌(英文)[J].中国有色金属学报:英文版,2019,29(10):2222-2228. 被引量:7

10李鹭.医院污水处理工艺和消毒剂的选择[J].环境与发展,2019,31(10):70-70. 被引量:3

Basic Information:

DOI:

Chinese Library Classification Number:X705[环境科学与工程—环境工程]

Citation Information:

Polyaluminum ferric chloride(PAFC) was prepared from acid leaching solution obtained by hydrochloric acid leaching of red mud,and its performance of kaolin wastewater treatment was studied.The effects of hydrochloric acid concentration,leaching temperature,leaching time and liquid-solid ratio on the leaching rate of Al and Fe in red mud were investigated.Also the effects of PAFC dosage,kaolin quality concentration,wastewater pH value and water temperature on the turbidity removal rate of kaolin during wastewater treatment with PAFC were studied.The experimental results show that the leaching rate of Al and Fe is 76.5% and 33.7%,respectively,under the conditions of 50% hydrochloric acid concentration,80 ℃ leaching temperature,1.5 h leaching time and 5 mL/g liquid-solid ratio.The highest turbidity removal rate of PAC for kaolin wastewater treatment is 90%,while that of self-made PAFC is 94%,under the conditions of PAC/PAFC dosage of 8 mL(10 g/L),wastewater pH value of 7.0,kaolin suspension(mass concentration 125 mg/L) volume of 500 mL and wastewater temperature of 20 ℃.

quote

GB/T 7714-2015 [1] ZHAO Heng, LI Wang, NIU Ze-peng, et al. Preparation and Adsorption Properties of Polyaluminum Ferric Chloride from Red Mud[J]. Rare Metals and Cemented Carbides, 2019(5): 64-68.
MLA [1] ZHAO Heng, et al., "Preparation and Adsorption Properties of Polyaluminum Ferric Chloride from Red Mud." Rare Metals and Cemented Carbides, no. 5, 2019, pp. 64-68.
APA [1] ZHAO Heng, LI Wang, NIU Ze-peng, & ZHU Xiao-bo. (2019). Preparation and Adsorption Properties of Polyaluminum Ferric Chloride from Red Mud. Rare Metals and Cemented Carbides(5), 64-68.
IEEE [1] ZHAO Heng, LI Wang, NIU Ze-peng, and ZHU Xiao-bo, "Preparation and Adsorption Properties of Polyaluminum Ferric Chloride from Red Mud," Rare Metals and Cemented Carbides, no. 5, pp. 64-68, 2019. keywords: {red mud;acid leaching;polyaluminum ferric chloride;kaolin wastewater;turbidity removal rate}