daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Degradable Poly(butylene-co-divanillyl adipate) with Intrinsic Free Radical Scavenging and Antibacterial Performance AITranslate

Jiangnan University; Jiangnan University; Jiangnan University; Nanjing Forestry University; Jiangnan University; Jiangnan University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Bioactive polyesters with antibacterial and free radical scavenging functionalities help inhibit the spread of bacteria and eliminate the inflammation, which are of great significance for improving human health. In this study, a bioactive and degradable polyester was designed. First, divanillyl alcohol (DA) was synthesized from vanillin, and the copolymerization of DA, butanediol, adipic acid, and isophorone diisocyanate was conducted to obtain three kinds of polymers: polybutylene adipate (PBA), poly(butylene-co-divanillyl adipate) (PBDA), and chain extended PBDA (named as PBDAU). The H1 NMR and infrared spectra illustrated the successful synthesis of the polymers. Their Tg values are −30.5, −31.0, and −28.7 °C, respectively. Interestingly, PBDAU showed intrinsic free radical scavenging activity (RSA). The RSA efficiency of PBDAU can reach up to 100%, while PBDA has 78% and PBA shows no RSA. Furthermore, PBDAU showed inhibition of bacterial growth, especially for the Escherichia coli. The excellent free radical scavenging and antibacterial performance for PBDAU should be associated with the stabilization of phenoxy radicals (Ar–O•), and the easily split-off H•/H+, which will then couple with the free radicals, like “the eagle catches the mouse”. Meanwhile, the polyesters can be degraded under both acidolysis and alkalinolysis conditions. This study is expected to contribute a solution to the synthesis of a bioactive and degradable polyester.

KeyWords AITranslate

poly(butylenecodivanillyl adipate) free radical scavenging antibacterial degradation mechanism
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c01473

Chinese Library Classification Number:

Citation Information:

Bioactive polyesters with antibacterial and free radical scavenging functionalities help inhibit the spread of bacteria and eliminate the inflammation, which are of great significance for improving human health. In this study, a bioactive and degradable polyester was designed. First, divanillyl alcohol (DA) was synthesized from vanillin, and the copolymerization of DA, butanediol, adipic acid, and isophorone diisocyanate was conducted to obtain three kinds of polymers: polybutylene adipate (PBA), poly(butylene-co-divanillyl adipate) (PBDA), and chain extended PBDA (named as PBDAU). The H1 NMR and infrared spectra illustrated the successful synthesis of the polymers. Their Tg values are −30.5, −31.0, and −28.7 °C, respectively. Interestingly, PBDAU showed intrinsic free radical scavenging activity (RSA). The RSA efficiency of PBDAU can reach up to 100%, while PBDA has 78% and PBA shows no RSA. Furthermore, PBDAU showed inhibition of bacterial growth, especially for the Escherichia coli. The excellent free radical scavenging and antibacterial performance for PBDAU should be associated with the stabilization of phenoxy radicals (Ar–O•), and the easily split-off H•/H+, which will then couple with the free radicals, like “the eagle catches the mouse”. Meanwhile, the polyesters can be degraded under both acidolysis and alkalinolysis conditions. This study is expected to contribute a solution to the synthesis of a bioactive and degradable polyester.

quote

GB/T 7714-2015 [1] Weijun Yang, Liqiang Xiao, Binbao Lu, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c01473.
MLA [1] Weijun Yang, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c01473.
APA [1] Weijun Yang, Liqiang Xiao, Binbao Lu, Jiaqi Guo, Pengwu Xu, & Piming Ma. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c01473
IEEE [1] Weijun Yang, Liqiang Xiao, Binbao Lu, Jiaqi Guo, Pengwu Xu, and Piming Ma, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c01473. keywords: {poly(butylenecodivanillyl adipate);free radical scavenging;antibacterial;degradation;mechanism}