daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Electroless Metallization of the Elements: Survey and Progress Electroless Metallization of the Elements: Survey and Progress AITranslate

The Ohio State University Department of Chemistry & Biochemistry Columbus;The Ohio State University Department of Chemistry & Biochemistry Columbus
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The electroless plating of metals and their alloys, oxides, and chalcogenides represents a critically important technology for the automotive, aerospace, machine tools, and, especially, the electronics industries. Since the initial efforts involving the plating of industrially important metals, such as Ni, Co, Cu, Ag, and Au, in the mid-20th century, the process has evolved to encompass a growing number of elements. At the same time, this expansion in the palette of accessible metals has enabled progress in these industries and evoked new nonconventional applications. In this review, we collect and survey available electroless processes in aqueous and organic solvent systems for each element organized according to position in the Periodic Table as a resource for the reader. Examples illustrating progress in the field are presented and are described in sufficient detail to be useful and understandable for both the expert and nonexpert. Given the historical importance of electronics as a driver for development of electroless processes, examples are electronics-related where possible. However, we strive to also include examples of applications in nontraditional fields to provide the reader with a sense of generality available for electroless methods. The review closes with an outlook for the field and a challenge to scientists and engineers to adapt electroless processes for new applications to continue the growth of the field.

KeyWords AITranslate

electroless plating galvanic immersion elements metals
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.2c01195

Chinese Library Classification Number:

Citation Information:

The electroless plating of metals and their alloys, oxides, and chalcogenides represents a critically important technology for the automotive, aerospace, machine tools, and, especially, the electronics industries. Since the initial efforts involving the plating of industrially important metals, such as Ni, Co, Cu, Ag, and Au, in the mid-20th century, the process has evolved to encompass a growing number of elements. At the same time, this expansion in the palette of accessible metals has enabled progress in these industries and evoked new nonconventional applications. In this review, we collect and survey available electroless processes in aqueous and organic solvent systems for each element organized according to position in the Periodic Table as a resource for the reader. Examples illustrating progress in the field are presented and are described in sufficient detail to be useful and understandable for both the expert and nonexpert. Given the historical importance of electronics as a driver for development of electroless processes, examples are electronics-related where possible. However, we strive to also include examples of applications in nontraditional fields to provide the reader with a sense of generality available for electroless methods. The review closes with an outlook for the field and a challenge to scientists and engineers to adapt electroless processes for new applications to continue the growth of the field.

quote

GB/T 7714-2015 [1] Claudia Turro, Walter J. Dressick. ACS Applied Electronic Materials, 2022(4). DOI:10.1021/acsaelm.2c01195.
MLA [1] Claudia Turro, and Walter J. Dressick. ACS Applied Electronic Materials, no. 4, 2022, https://doi.org/10.1021/acsaelm.2c01195.
APA [1] Claudia Turro, & Walter J. Dressick. (2022). ACS Applied Electronic Materials(4). https://doi.org/10.1021/acsaelm.2c01195
IEEE [1] Claudia Turro and Walter J. Dressick, ACS Applied Electronic Materials, no. 4, 2022, doi: 10.1021/acsaelm.2c01195. keywords: {electroless plating galvanic immersion elements metals}