daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Phosphine Oxide-Containing Multifunctional Polymer via RAFT Polymerization and Its High-Density Post-Polymerization Modification in Water AITranslate

Huazhong University of Science and Technology (HUST); Huazhong University of Science and Technology (HUST); Huazhong University of Science and Technology (HUST); Hubei Minzu University; Huazhong University of Science and Technology (HUST)
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Reactive polymers with two or more reactive groups in each repeat unit were less reported, and these kinds of polymers were regarded as useful precursors for further multifunctionalization. Here, an alkali-soluble polymer with the bis(hydroxymethyl)phosphine oxide pendant group was first prepared by reversible addition–fragmentation transfer (RAFT) polymerization from a phosphine-containing monomer, namely (4-vinylbenzyl)-bis-hydroxymethyl phosphine oxide (VBzBHPO). The well-defined homopolymers were characterized by Fourier transform infrared spectroscopy, nuclear magnetic resonance, and gel permeation chromatography. The molecular weights of both homopolymers and block polymers can be designed by changing RAFT polymerization parameters while still maintaining the narrow molecular weight distributions (mostly Mw/Mn < 1.2). The linear polymerization kinetics and successful chain extension polymerization with styrene or VBzBHPO confirmed the features of controlled/living radical polymerization. Attractively, the resulting polyVBzBHPO showed high solubility in alkaline solution but only lightly swelled in pure water. Such a distinguishing feature of the polymer material provided the possibility of carrying out post-polymerization modification in water with high functionality density and high modification efficiency.

KeyWords AITranslate

phosphinecontaining polymer RAFT chemical fixation of phosphine gas multifunctional polymer aqueous postpolymerization Show More
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c00403

Chinese Library Classification Number:

Citation Information:

Reactive polymers with two or more reactive groups in each repeat unit were less reported, and these kinds of polymers were regarded as useful precursors for further multifunctionalization. Here, an alkali-soluble polymer with the bis(hydroxymethyl)phosphine oxide pendant group was first prepared by reversible addition–fragmentation transfer (RAFT) polymerization from a phosphine-containing monomer, namely (4-vinylbenzyl)-bis-hydroxymethyl phosphine oxide (VBzBHPO). The well-defined homopolymers were characterized by Fourier transform infrared spectroscopy, nuclear magnetic resonance, and gel permeation chromatography. The molecular weights of both homopolymers and block polymers can be designed by changing RAFT polymerization parameters while still maintaining the narrow molecular weight distributions (mostly Mw/Mn < 1.2). The linear polymerization kinetics and successful chain extension polymerization with styrene or VBzBHPO confirmed the features of controlled/living radical polymerization. Attractively, the resulting polyVBzBHPO showed high solubility in alkaline solution but only lightly swelled in pure water. Such a distinguishing feature of the polymer material provided the possibility of carrying out post-polymerization modification in water with high functionality density and high modification efficiency.

quote

GB/T 7714-2015 [1] Jian Sun, Chang Wang, YuLin Hong, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.1c00403.
MLA [1] Jian Sun, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.1c00403.
APA [1] Jian Sun, Chang Wang, YuLin Hong, ZhiWei Tan, & ChengMei Liu. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.1c00403
IEEE [1] Jian Sun, Chang Wang, YuLin Hong, ZhiWei Tan, and ChengMei Liu, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.1c00403. keywords: {phosphinecontaining polymer;RAFT;chemical fixation of phosphine gas;multifunctional polymer;aqueous postpolymerization;Show More}