Prediction of the drying shrinkage of alkali-activated materials using artificial neural networks AITranslate
Abstract AITranslate
Alkali-activated materials (AAMs) are qualitatively and quantitatively evaluated with an emphasis on the ultimate drying shrinkage. We systematically evaluated AAMs based on the mix design and curing conditions, utilizing a total of 452 AAM mixtures extracted from 44 papers. Finally, a predictive model for the ultimate drying shrinkage of AAMs was constructed using an artificial neural network (ANN) with high accuracy, in which the reactivity of binder, geopolymer paste volume, liquid-to-binder ratio, alkali activator modulus, aggregate volumetric ratio, curing temperature, relative humidity and specimen size were set as inputs. This model shows great generality by compiling various AAM mixtures and is easy-handling without preparation of samples for acquiring specific properties. Moreover, the efficiency of three commonly used models for predicting the drying shrinkage—the Bažant-Baweja model, Gardner and Lockman model, and multi-linear regression model—were evaluated and compared to the proposed ANN model, revealing a better prediction performance of ANN model. This study will advance the understanding of the drying shrinkage behaviors of AAMs and provide practical guidelines for designing AAM mixtures with high durability.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1016/j.cscm.2022.e01166
Chinese Library Classification Number:
Citation Information:
Alkali-activated materials (AAMs) are qualitatively and quantitatively evaluated with an emphasis on the ultimate drying shrinkage. We systematically evaluated AAMs based on the mix design and curing conditions, utilizing a total of 452 AAM mixtures extracted from 44 papers. Finally, a predictive model for the ultimate drying shrinkage of AAMs was constructed using an artificial neural network (ANN) with high accuracy, in which the reactivity of binder, geopolymer paste volume, liquid-to-binder ratio, alkali activator modulus, aggregate volumetric ratio, curing temperature, relative humidity and specimen size were set as inputs. This model shows great generality by compiling various AAM mixtures and is easy-handling without preparation of samples for acquiring specific properties. Moreover, the efficiency of three commonly used models for predicting the drying shrinkage—the Bažant-Baweja model, Gardner and Lockman model, and multi-linear regression model—were evaluated and compared to the proposed ANN model, revealing a better prediction performance of ANN model. This study will advance the understanding of the drying shrinkage behaviors of AAMs and provide practical guidelines for designing AAM mixtures with high durability.
quote
| GB/T 7714-2015 | [1] Y.K. Kong, Kiyofumi Kurumisawa. Case Studies in Construction Materials, 2022(17). DOI:10.1016/j.cscm.2022.e01166. |
| MLA | [1] Y.K. Kong, and Kiyofumi Kurumisawa. Case Studies in Construction Materials, no. 17, 2022, https://doi.org/10.1016/j.cscm.2022.e01166. |
| APA | [1] Y.K. Kong, & Kiyofumi Kurumisawa. (2022). Case Studies in Construction Materials(17). https://doi.org/10.1016/j.cscm.2022.e01166 |
| IEEE | [1] Y.K. Kong and Kiyofumi Kurumisawa, Case Studies in Construction Materials, no. 17, 2022, doi: 10.1016/j.cscm.2022.e01166. keywords: {AAMs Alkaliactivated materials;Alkaliactivated materials;ANN Artificial neural network;Artificial neural network;BPNN Backpropagation training algorithm;Backpropagation training algorithm;FA C Fly ash class C;Fly ash class C;FA F Fly ash class F;Fly ash class F;GGBFS Ground granulated blastfurnace slag;Ground granulated blastfurnace slag;GPV Geopolymer paste volume;Geopolymer paste volume;MAE Mean absolute error;Mean absolute error;MLR Multilinear regression;Multilinear regression;PC Portland cement;Portland cement;RH Relative humidity;Relative humidity;RMSE Root mean squared error;Root mean squared error;SCM Supplementary cementitious material;Supplementary cementitious material;SF Silica fume;Silica fume;UDS Ultimate drying shrinkage;Ultimate drying shrinkage;Alkaliactivated materials;Artificial Neural Networks;Drying shrinkage;Mix design;Prediction} |