Material interactions in laser polishing powder bed additive manufactured Ti6Al4V components AITranslate
Abstract AITranslate
Laser polishing (LP) is an emerging technique with the potential to be used for post-build, or in-situ, precision smoothing of rough, fatigue-initiation prone, surfaces of additive manufactured (AM) components. LP uses a laser to re-melt a thin surface layer and smooths the surface by exploiting surface tension effects in the melt pool. However, rapid re-solidification of the melted surface layer and the associated substrate thermal exposure can significantly modify the subsurface material. This study has used an electron beam melted (EBM) Ti6Al4V component, representing the worst case scenario in terms of roughness for a powder bed process, as an example to investigate these issues and evaluate the capability of the LP technique for improving the surface quality of AM parts. Experiments have shown that the surface roughness can be reduced to below Sa = 0.51 μm, which is comparable to a CNC machined surface, and high stress concentrating defects inherited from the AM process were removed by LP. However, the re-melted layer underwent a change in texture, grain structure, and a martensitic transformation, which was subsequently tempered in-situ by repeated beam rastering and resulted in a small increase in sub-surface hardness. In addition, a high level of near-surface tensile residual stresses was generated by the process, although they could be relaxed to near zero by a standard stress relief heat treatment. Graphical abstract Download : Download high-res image (385KB) Download : Download full-size image
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1016/j.addma.2017.12.010
Chinese Library Classification Number:
Citation Information:
Laser polishing (LP) is an emerging technique with the potential to be used for post-build, or in-situ, precision smoothing of rough, fatigue-initiation prone, surfaces of additive manufactured (AM) components. LP uses a laser to re-melt a thin surface layer and smooths the surface by exploiting surface tension effects in the melt pool. However, rapid re-solidification of the melted surface layer and the associated substrate thermal exposure can significantly modify the subsurface material. This study has used an electron beam melted (EBM) Ti6Al4V component, representing the worst case scenario in terms of roughness for a powder bed process, as an example to investigate these issues and evaluate the capability of the LP technique for improving the surface quality of AM parts. Experiments have shown that the surface roughness can be reduced to below Sa = 0.51 μm, which is comparable to a CNC machined surface, and high stress concentrating defects inherited from the AM process were removed by LP. However, the re-melted layer underwent a change in texture, grain structure, and a martensitic transformation, which was subsequently tempered in-situ by repeated beam rastering and resulted in a small increase in sub-surface hardness. In addition, a high level of near-surface tensile residual stresses was generated by the process, although they could be relaxed to near zero by a standard stress relief heat treatment. Graphical abstract Download : Download high-res image (385KB) Download : Download full-size image
quote
| GB/T 7714-2015 | [1] Yingtao Tian, Wojciech S. Gora, Aldara Pan Cabo, et al. Additive Manufacturing, 2018(20). DOI:10.1016/j.addma.2017.12.010. |
| MLA | [1] Yingtao Tian, et al., Additive Manufacturing, no. 20, 2018, https://doi.org/10.1016/j.addma.2017.12.010. |
| APA | [1] Yingtao Tian, Wojciech S. Gora, Aldara Pan Cabo, Lakshmi L. Parimi, Duncan P. Hand, Samuel TammasWilliams, & Philip B. Prangnell. (2018). Additive Manufacturing(20). https://doi.org/10.1016/j.addma.2017.12.010 |
| IEEE | [1] Yingtao Tian, Wojciech S. Gora, Aldara Pan Cabo, Lakshmi L. Parimi, Duncan P. Hand, Samuel TammasWilliams, and Philip B. Prangnell, Additive Manufacturing, no. 20, 2018, doi: 10.1016/j.addma.2017.12.010. |