The Crystal Structure of Sr 4Al 14 O 25 ∶Eu,Nd Noctilucent Powder AITranslate
Abstract AITranslate
From the X ray diffraction of Sr 4Al 14 O 25 ∶Eu,Nd noctilucent sample powder,its mixed crystal structure is confirmed. Eu 2+ has replaced Sr 2+ in the matrix while Nd 3+ has replaced Al 3+ . The appearance and size range of the sample is determined by SEM.
KeyWords AITranslate
1唐明道,李长宽,高志武,许少鸿,蒋雪茵,蔡锟.SrAl_2O_4:Eu^(2+)的长余辉发光特性的研究[J].发光学报,1995,16(1):51-56. 被引量:82
2唐明道.-[J].材料导报,1993,(3):3-3.
3末庆梅.-[J].发光学报,1991,12(2):144-144.
1于长凤,刘俊荣,梁耀龙,唐奇,朱小平,张缇.燃烧法制备铝酸锶蓄能发光材料的研究[J].中国陶瓷工业,2014,21(1):1-4. 被引量:1
2丁红,张静娴,刘应亮,杨培慧,冯德雄.燃烧法合成纳米长余辉发光材料BaAl_2O_4:Eu,Nd[J].暨南大学学报:自然科学与医学版,2002,23(3):70-74. 被引量:15
1李东平,缪春燕,刘丽芳,罗昔贤,魏坤,肖志国.燃烧法合成新型蓝色硅酸盐长余辉材料及其发光性能的研究[J].稀有金属,2004,28(4):662-665. 被引量:19
2李庚申,孙家跃,杜海燕,王葳.不球磨无机粉体发光材料制备技术进展[J].化工时刊,2004,18(12):1-7.
3李峻峰,邱克辉,赖雪飞,张春梅,李群.稀土发光材料燃烧合成的研究进展[J].材料导报,2005,19(4):28-30. 被引量:14
4刘晓瑭,刘华鼐,石春山.稀土发光材料的合成方法[J].合成化学,2005,13(3):216-218. 被引量:20
5苏言杰,张德,徐建梅,王辉.柠檬酸盐凝胶自燃烧法合成超细粉体[J].材料导报,2006,20(F05):142-144. 被引量:20
6张瑞军,张玉奇,刘小蕊,张春红.稀土蓝色长余辉发光材料的研究进展[J].山东陶瓷,2006,29(4):14-16. 被引量:4
7孙继兵,王海容,安雅琴,崔春翔,韩丹.长余辉发光材料研究进展[J].稀有金属材料与工程,2008,37(2):189-194. 被引量:17
8黄以万,肖兵.稀土发光材料的研究与应用展望[J].矿产保护与利用,2008,28(6):51-54. 被引量:21
9葛杏心,孙艳辉,刘聪,符远翔.稀土蓝色光致发光材料研究进展[J].稀土,2009,30(1):80-85. 被引量:7
10贺春晖,郑淑华,肖勇,刘应亮.纳米棒状长余辉材料BaAl_2O_4:Eu^(2+),Dy^(3+)的制备与发光性能[J].光谱学与光谱分析,2010,30(1):26-29.
1吴振国,毛向辉,廉世勋.ZnS:Cu,Mn,Tm晶体结构的研究[J].湖南师范大学自然科学学报,1993,16(1):51-54.
2岑绍辉,韩越清.夜光粉发光机理及其制造工艺[J].新技术新工艺,1994(2):37-37.
3长效夜光粉[J].广东有色金属学报,2002,12(2):127-127.
4刘子明.新型夜光粉[J].科学启蒙,2014(3):84-84.
5代红丽,秦云.Al掺杂对ZnO薄膜晶体结构的影响[J].天津理工大学学报,2008,24(4):67-69.
6李岚,熊光楠,娄素云,李炳生,申德振.投影电视的原理及其三基色荧光粉的发光性质[J].热固性树脂,1999,14(4):122-124. 被引量:1
7千元安卓神器Nibiru H1[J].新电脑,2014(4):104-104.
8Wei-Ren Liu,Chun Che Lin,Yi-Chen Chiu,Yao-Tsung Yeh,Shyue-Ming Jang,Ru-Shi Liu.Luminescence Properties of Green-emitting Phosphors-Sr4Al14O25:Eu2+ for LED Applications[J].化学与化工:英文版,2011,5(7):638-643.
9世界杯夜光粉T恤[J].稀土信息,2006,12(8):38-38.
10朱雪珍,叶关荣.点阵液晶在夜光粉发光衰减曲线显示中的应用[J].光学仪器,2003,25(2):20-23. 被引量:1
Basic Information:
DOI:
Chinese Library Classification Number:TN383.04[电子电信—物理电子学]
Citation Information:
From the X ray diffraction of Sr 4Al 14 O 25 ∶Eu,Nd noctilucent sample powder,its mixed crystal structure is confirmed. Eu 2+ has replaced Sr 2+ in the matrix while Nd 3+ has replaced Al 3+ . The appearance and size range of the sample is determined by SEM.
quote
| GB/T 7714-2015 | [1] WU Zhen-guo, LIAN Shi-xun, LI Cheng-zhi, et al. The Crystal Structure of Sr 4Al 14 O 25 ∶Eu,Nd Noctilucent Powder[J]. Rare Metals and Cemented Carbides, 1999(3): 18-20. |
| MLA | [1] WU Zhen-guo, et al., "The Crystal Structure of Sr 4Al 14 O 25 ∶Eu,Nd Noctilucent Powder." Rare Metals and Cemented Carbides, no. 3, 1999, pp. 18-20. |
| APA | [1] WU Zhen-guo, LIAN Shi-xun, LI Cheng-zhi, ZHANG Hua-jing, & MAO Xiang-hui. (1999). The Crystal Structure of Sr 4Al 14 O 25 ∶Eu,Nd Noctilucent Powder. Rare Metals and Cemented Carbides(3), 18-20. |
| IEEE | [1] WU Zhen-guo, LIAN Shi-xun, LI Cheng-zhi, ZHANG Hua-jing, and MAO Xiang-hui, "The Crystal Structure of Sr 4Al 14 O 25 ∶Eu,Nd Noctilucent Powder," Rare Metals and Cemented Carbides, no. 3, pp. 18-20, 1999. keywords: {Sr 4Al 14 O 25 ∶Eu+Nd;noctilucent powder;crystal;structure} |