Microwave-Ultrasonic Synergistic Preparation of Nano Spherical Dysprosium Oxide AITranslate
Abstract AITranslate
Under the synergistic action of microwave-ultrasonic, Dy2O3 precursor(Dy(OH)CO3·H2O) was prepared by the reaction of a certain concentration of DyCl3 solution with urea as precipitant, and then the nano spherical Dy2O3 was obtained by calcination.The effects of Dy3+ concentration, urea concentration and ultrasonic power on the morphology of Dy2O3 precursor were explored.The morphology and microstructure of Dy2O3 precursor before and after calcination were characterized, and the calcination decomposition mechanism was analyzed by scanning electron microscope, synchronous thermal analyzer, X-ray diffractometer, and Fourier infrared spectrometer.The results show that Dy(OH)CO3·H2O with uniform particle size, smooth surface, good dispersion and particle size of about 220 nm can be obtained under the conditions of Dy3+ concentration of 0.045 mol/L,urea concentration of 2.5 mol/L,microwave power of 500 W,ultrasonic power of 800 W,ultrasonic mode of 1∶2,reaction time of 1 h and reaction temperature of 90 ℃.The precursor can be completely decomposed at the calcination temperature of 800 ℃,and nano spherical Dy2O3 with particle size of about 200 nm can be obtained.
KeyWords AITranslate
1张晓蕾.纳米材料在化学化工领域中的应用研究[J].山东工业技术,2016(16):21-21. 被引量:3
1于军洋,赵鸿滨,陈小强,魏峰.快速热退火对Pt/Dy_(2)O_(3)/Pt阻变特性的影响[J].稀有金属,2020,44(12):1286-1291.
2岳劲松,李梅,丁宁,孙功成,程雪云,高彩云.不同方式辅助H_(2)O_(2)脱硫结果的比较[J].煤炭转化,2021,44(3):11-20. 被引量:4
3胡章记,王彦娜,梁慧锋,王晓楠.氧化石墨/壳聚糖复合水凝胶的制备及其对锌铅离子吸附性能的研究[J].化工技术与开发,2021,50(5):9-14. 被引量:3
4朱倩倩,靳海波,郭晓燕,何广湘,马磊,张荣月,谷庆阳,杨索和.H_(2)O_(2)/乙腈体系下MgO催化环己酮Baeyer-Villiger绿色氧化合成ε-己内酯的研究[J].化工学报,2021,72(5):2638-2646. 被引量:2
5赵星源,肖晋宇,赵丹,陈昉,徐新智.自适应蚁群算法的清洁能源基地选址优化模型[J].测绘科学,2021,46(4):172-177. 被引量:1
6阚燕,孙倩,李晓强,高德康.基于氯化钴改性的纤维素纸比色湿度传感器[J].化工进展,2021,40(5):2703-2709.
7叶伟龙,郑靖川,黄佳倩,赵鹏程,刘柱,马国武.分级电纺复合载药微球辅助牙槽骨增量[J].口腔医学研究,2021,37(5):458-461.
8徐雪山,马心语,彭燕,王煦.pH值对正硅酸乙酯原位改性水性聚氨酯复合乳液性能的影响[J].塑料工业,2021,49(4):32-37. 被引量:1
9蔡斌,陈永华,杜露,何浪君.博落回对铅的耐性、富集及生理响应研究[J].农业现代化研究,2021,42(2):339-348.
10沈慧颖,吕子豪,庄粟裕,曹秀明,王清清.静电纺CA/PpIX多孔纤维膜的制备及其光动力性能[J].材料工程,2021,49(5):89-97. 被引量:1
Basic Information:
DOI:
Chinese Library Classification Number:TF845.3[冶金工程—有色金属冶金]
Citation Information:
Under the synergistic action of microwave-ultrasonic, Dy2O3 precursor(Dy(OH)CO3·H2O) was prepared by the reaction of a certain concentration of DyCl3 solution with urea as precipitant, and then the nano spherical Dy2O3 was obtained by calcination.The effects of Dy3+ concentration, urea concentration and ultrasonic power on the morphology of Dy2O3 precursor were explored.The morphology and microstructure of Dy2O3 precursor before and after calcination were characterized, and the calcination decomposition mechanism was analyzed by scanning electron microscope, synchronous thermal analyzer, X-ray diffractometer, and Fourier infrared spectrometer.The results show that Dy(OH)CO3·H2O with uniform particle size, smooth surface, good dispersion and particle size of about 220 nm can be obtained under the conditions of Dy3+ concentration of 0.045 mol/L,urea concentration of 2.5 mol/L,microwave power of 500 W,ultrasonic power of 800 W,ultrasonic mode of 1∶2,reaction time of 1 h and reaction temperature of 90 ℃.The precursor can be completely decomposed at the calcination temperature of 800 ℃,and nano spherical Dy2O3 with particle size of about 200 nm can be obtained.
quote
| GB/T 7714-2015 | [1] DENG Geng-feng, LI Zhi-wu, ZHOU Xiao-ming. Microwave-Ultrasonic Synergistic Preparation of Nano Spherical Dysprosium Oxide[J]. Rare Metals and Cemented Carbides, 2021(2): 29-35. |
| MLA | [1] DENG Geng-feng, et al., "Microwave-Ultrasonic Synergistic Preparation of Nano Spherical Dysprosium Oxide." Rare Metals and Cemented Carbides, no. 2, 2021, pp. 29-35. |
| APA | [1] DENG Geng-feng, LI Zhi-wu, & ZHOU Xiao-ming. (2021). Microwave-Ultrasonic Synergistic Preparation of Nano Spherical Dysprosium Oxide. Rare Metals and Cemented Carbides(2), 29-35. |
| IEEE | [1] DENG Geng-feng, LI Zhi-wu, and ZHOU Xiao-ming, "Microwave-Ultrasonic Synergistic Preparation of Nano Spherical Dysprosium Oxide," Rare Metals and Cemented Carbides, no. 2, pp. 29-35, 2021. keywords: {microwave-ultrasonic synergy;nano spherical dysprosium oxide;calcination;precursor;DyClsolution;urea;Dy(OH)CO·HO} |