Hydrothermal Preparation and Properties of Flaky-cluster Co_3O_4 Super-hydrophobic Surface with Micro/Nano-sized Microstructure AITranslate
Abstract AITranslate
Flaky-cluster Co3O4super-hydrophobic surface was successfully prepared on on aluminum substrate via hydrothermal method.The phase composition and surface morphology of the precursor and terminal product were detected by X-ray diffraction and scanning electron microscopy.The effect of reaction time on Co3O4 surface morphology was investigated,and microstructure evolution with reaction time was analyzed in details.The lubrication performance of Co3O4super-hydrophobic surfaces were analyzed with Cassie-Baxter composite model.Finally,the impact resistant stability of Co3O4super-hydrophobic surface was tested with high pressure water column.The results show that flaky-cluster Co3O4super-hydrophobic surface prepared by 10 hreaction has the best super-hydrophobic performance and good water impact resistant stability.
KeyWords AITranslate
1傅爱红,李春福.超疏水表面的研究进展及制备技术[J].材料导报,2012,26(9):46-51. 被引量:6
2李松梅,周思卓,刘建华.铝合金表面原位自组装超疏水膜层的制备及耐蚀性能[J].物理化学学报,2009,25(12):2581-2589. 被引量:27
3江雷.从自然到仿生的超疏水纳米界面材料[J].科技导报,2005,23(2):4-8. 被引量:100
4Jie Yang,Wen Li.Preparation of superhydrophobic surfaces on Al substrates and the anti-icing behavior[J]. Journal of Alloys and Compounds . 2013
5Cheng, Qunfeng,Li, Mingzhu,Zheng, Yongmei,Su, Bin,Wang, Shutao,Jiang, Lei.Janus interface materials: Superhydrophobic air/solid interface and superoleophobic water/solid interface inspired by a lotus leaf. Soft Matter . 2011
6Cassie A B D,Baxter S.Wettability of porous surfaces. Transactions of the Faraday Society . 1944
7Wang, Taoye,Isimjan, Tayirjan T.,Chen, Jianfeng,Rohani, Sohrab.Transparent nanostructured coatings with UV-shielding and superhydrophobicity properties. Nanotechnology . 2011
1田野,李萍,王久林,薛克敏,林泉.高压扭转压力对304不锈钢组织及性能影响[J].塑性工程学报,2016,23(2):98-102. 被引量:7
2郭于田,孙晓晗,许月伟,龙瑞.在木材表面制备一种稳定且耐久的超疏水涂层的方法[J].广东化工,2018,45(12):19-20. 被引量:4
3蒋炜,杨超,袁绍军,梁斌.仿生超疏水金属材料制备技术及在化工领域应用进展[J].化工进展,2019,38(1):344-364. 被引量:11
1刘巧玲.盐酸生产氧化铝工艺废水治理技术研究[J].环境科学与管理,2019,44(3):80-85. 被引量:1
2孙晓晗,郭于田,龙瑞,许月伟,王成毓.磁性超疏水棉布的制备及应用[J].森林工程,2019,35(3):54-62. 被引量:5
3薛克敏,孙建辉,纪小虎,郭威威,李萍.高压扭转工艺对TA15钛合金组织和性能的影响[J].稀有金属材料与工程,2019,48(4):1189-1194. 被引量:4
4薛克敏,胡勇,时迎宾,纪小虎,甘国强,李萍.Ti2AlNb基合金(B2+O)相区多向锻造微观组织[J].稀有金属材料与工程,2019,48(8):2556-2561. 被引量:4
5杨玉山,沈华杰,邱坚.基于纳米SiO2-PDMS体系的耐磨超疏水木材表面构建与特性评价[J].西南林业大学学报:自然科学,2019,39(6):160-166. 被引量:9
6丁元迪,周潼,王若云,刘磊,胡文彬.金属基体上超疏水表面的制备及其机械耐久性的研究进展[J].表面技术,2019,48(12):68-86. 被引量:18
7吴新宇,吴燕,徐颖异,孔璋倩,苏小卿,贾焕亮.木材表面疏水涂层的制备及耐久性测试[J].家具,2020,41(1):19-22. 被引量:8
8杨智强,起华荣,吕潍威,苏晨.304L不锈钢等径角挤压有限元模拟研究[J].铸造技术,2020,41(5):490-494.
9刘楠,张相宁,杨桂英,席乃园,刘艳.低表面能修饰工艺对涂层接触角的影响研究[J].电焊机,2020,50(8):86-90.
10程甜甜.超疏水材料的制备技术及在工业领域的应用[J].化工管理,2020(28):101-102. 被引量:2
1吴建锋,张敏,徐晓虹,李坤.氨和胺在水热法合成ZnO花簇微晶中的作用[J].武汉理工大学学报,2009,31(10):1-5. 被引量:2
2雷春.花簇状ZnS:Mn微球的制备及荧光性能研究[J].广州化工,2011,39(13):70-73. 被引量:1
3于欢,王卫伟.表面活性剂对Mg-Al层状双金属氢氧化物生长影响[J].山东理工大学学报:自然科学版,2016,30(6):36-39. 被引量:1
4雷楠楠,刘鲁梅,胡正水.聚乙烯吡咯烷酮/溶剂辅助合成SnO_2纳米晶体[J].青岛科技大学学报:自然科学版,2013,34(1):22-27.
5王晓红,谢文静,郝臣,张鹏飞,傅小奇,司乃潮.木素磺酸钙模板法液相合成花簇状ZnO及其光催化性能[J].金属学报,2013,49(9):1098-1104. 被引量:2
6张耀军,万刚强,颜磊,马庆昌,李东祥,赵继宽.种子生长法制备ZnO纳米棒组装结构[J].山东大学学报:理学版,2016,51(1):14-19.
7时海燕,胡仁,林昌健.羟基磷灰石涂层的电化学可控制备及生物性能的初步表征[J].电化学,2005,11(4):440-445. 被引量:4
8邵纯红,王路,李芬,姜安玺.乙醇对纳米CuO晶型及脱硫性能的影响[J].功能材料,2009,40(10):1744-1746. 被引量:2
9邢光建,李钰梅,孙璞.不同形貌的SrMoO_4材料的微乳液及其辅助的溶剂热法制备[J].无机化学学报,2010,26(9):1651-1656.
10孟祥龙,李洪义,王金淑.脉冲电沉积法制备Pt-TiO_2纳米管电极及其电催化性能[J].高等学校化学学报,2012,33(5):1021-1024. 被引量:8
Basic Information:
DOI:
Chinese Library Classification Number:O614.812[理学—无机化学]
Citation Information:
Flaky-cluster Co3O4super-hydrophobic surface was successfully prepared on on aluminum substrate via hydrothermal method.The phase composition and surface morphology of the precursor and terminal product were detected by X-ray diffraction and scanning electron microscopy.The effect of reaction time on Co3O4 surface morphology was investigated,and microstructure evolution with reaction time was analyzed in details.The lubrication performance of Co3O4super-hydrophobic surfaces were analyzed with Cassie-Baxter composite model.Finally,the impact resistant stability of Co3O4super-hydrophobic surface was tested with high pressure water column.The results show that flaky-cluster Co3O4super-hydrophobic surface prepared by 10 hreaction has the best super-hydrophobic performance and good water impact resistant stability.
quote
| GB/T 7714-2015 | [1] JIANG Chun-long, LI Wen, JIA Jun. Hydrothermal Preparation and Properties of Flaky-cluster Co_3O_4 Super-hydrophobic Surface with Micro/Nano-sized Microstructure[J]. Rare Metals and Cemented Carbides, 2015(1): 39-45. |
| MLA | [1] JIANG Chun-long, et al., "Hydrothermal Preparation and Properties of Flaky-cluster Co_3O_4 Super-hydrophobic Surface with Micro/Nano-sized Microstructure." Rare Metals and Cemented Carbides, no. 1, 2015, pp. 39-45. |
| APA | [1] JIANG Chun-long, LI Wen, & JIA Jun. (2015). Hydrothermal Preparation and Properties of Flaky-cluster Co_3O_4 Super-hydrophobic Surface with Micro/Nano-sized Microstructure. Rare Metals and Cemented Carbides(1), 39-45. |
| IEEE | [1] JIANG Chun-long, LI Wen, and JIA Jun, "Hydrothermal Preparation and Properties of Flaky-cluster Co_3O_4 Super-hydrophobic Surface with Micro/Nano-sized Microstructure," Rare Metals and Cemented Carbides, no. 1, pp. 39-45, 2015. keywords: {hydrothermal method;flaky-cluster Co3O4 super-hydrophobic surface;micro/nano-sized micro-structure;property;preparation} |