daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Achieving Remarkable Energy Storage Performances under Low Electric Field in Bi0.5N0.5TiO3-SrTiO3-Based Relaxor Ferroelectric Ceramics via a Heterostructure Doping Strategy Achieving Remarkable Energy Storage Performances under Low Electric Field in Bi0.5N0.5TiO3-SrTiO3-Based Relaxor Ferroelectric Ceramics via a Heterostructure Doping Strategy AITranslate

Hangzhou Dianzi University; Hangzhou Dianzi University; Hangzhou Dianzi University; Hangzhou Dianzi University; Hangzhou Dianzi University; Hangzhou Dianzi University; Hangzhou Dianzi University; Hangzhou Dianzi University; Hangzhou Dianzi University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The rapid growth of the electronics industry and increasing concern about environmental issues present great demands for lead-free dielectric ceramic capacitors with remarkable energy storage performances (ESPs). Lead-free perovskite ferroelectric and antiferroelectric systems are deemed as the most promising candidates, and homostructure linear dielectric doping is a widely used strategy to boost ESPs. However, the heavy doping of a linear dielectric usually leads to a great reduction of the polarization, for which an extremely high electric field is needed to achieve a large energy storage density (Wrec). In this study, a Bi0.5N0.5TiO3-SrTiO3 (BNT-ST)-based relaxor ferroelectric system was designed via a heterostructure doping strategy in which a tetragonal tungsten bronze ferroelectric phase Sr2NaNb5O15 (SNN) was introduced into the perovskite matrix. It was found that a small SNN heterostructure doping amount could effectively enhance the relaxor behavior of the BNT-ST ceramic and depress the remnant polarization, while keeping a large maximum polarization. Moreover, the introduction of the tungsten bronze ferroelectric phase obviously decreased the grain size (G) of the BNT-ST ceramic, giving rise to an improved electric breakdown strength (Eb). Finally, a remarkable Wrec of 5.22 J/cm3 and excellent efficiency (η) of 93.87% were attained under a low electric field of 340 kV/cm, which make the Bi0.5N0.5TiO3-SrTiO3-xSr2NaNb5O15 (BNT-ST-xSNN) ceramic system a promising choice for the dielectric energy storage field. These results demonstrate that the heterostructure doping strategy might be a feasible method to develop lead-free perovskite dielectric ceramics with remarkable ESPs under low electric fields.

KeyWords AITranslate

Leadfree Dielectric ceramics Energy storage BNTST Heterostructure doping
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.3c00739

Chinese Library Classification Number:

Citation Information:

The rapid growth of the electronics industry and increasing concern about environmental issues present great demands for lead-free dielectric ceramic capacitors with remarkable energy storage performances (ESPs). Lead-free perovskite ferroelectric and antiferroelectric systems are deemed as the most promising candidates, and homostructure linear dielectric doping is a widely used strategy to boost ESPs. However, the heavy doping of a linear dielectric usually leads to a great reduction of the polarization, for which an extremely high electric field is needed to achieve a large energy storage density (Wrec). In this study, a Bi0.5N0.5TiO3-SrTiO3 (BNT-ST)-based relaxor ferroelectric system was designed via a heterostructure doping strategy in which a tetragonal tungsten bronze ferroelectric phase Sr2NaNb5O15 (SNN) was introduced into the perovskite matrix. It was found that a small SNN heterostructure doping amount could effectively enhance the relaxor behavior of the BNT-ST ceramic and depress the remnant polarization, while keeping a large maximum polarization. Moreover, the introduction of the tungsten bronze ferroelectric phase obviously decreased the grain size (G) of the BNT-ST ceramic, giving rise to an improved electric breakdown strength (Eb). Finally, a remarkable Wrec of 5.22 J/cm3 and excellent efficiency (η) of 93.87% were attained under a low electric field of 340 kV/cm, which make the Bi0.5N0.5TiO3-SrTiO3-xSr2NaNb5O15 (BNT-ST-xSNN) ceramic system a promising choice for the dielectric energy storage field. These results demonstrate that the heterostructure doping strategy might be a feasible method to develop lead-free perovskite dielectric ceramics with remarkable ESPs under low electric fields.

quote

GB/T 7714-2015 [1] Yuzhe Lin, Ruifeng Wan, Peng Zheng, et al. ACS Applied Electronic Materials, 2023(5). DOI:10.1021/acsaelm.3c00739.
MLA [1] Yuzhe Lin, et al., ACS Applied Electronic Materials, no. 5, 2023, https://doi.org/10.1021/acsaelm.3c00739.
APA [1] Yuzhe Lin, Ruifeng Wan, Peng Zheng, Zhihao Li, Yikai Wang, Qiaolan Fan, Liang Zheng, Yang Zhang, & Wangfeng Bai. (2023). ACS Applied Electronic Materials(5). https://doi.org/10.1021/acsaelm.3c00739
IEEE [1] Yuzhe Lin, Ruifeng Wan, Peng Zheng, Zhihao Li, Yikai Wang, Qiaolan Fan, Liang Zheng, Yang Zhang, and Wangfeng Bai, ACS Applied Electronic Materials, no. 5, 2023, doi: 10.1021/acsaelm.3c00739. keywords: {Leadfree Dielectric ceramics Energy storage BNTST Heterostructure doping}