daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Superwetting Polypropylene Nonwoven Fabrics Modified by a Catechol-Based Biomimetic Strategy for Oil/Water Separation AITranslate

Zhejiang Sci-Tech University; Zhejiang Sci-Tech University; Zhejiang Sci-Tech University; Zhejiang Sci-Tech University; Zhejiang Sci-Tech University; Zhejiang Sci-Tech University; Zhejiang Sci-Tech University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The superwetting membrane with superhydrophilic/underwater superoleophobic properties is one of the ideal materials for treating oily wastewater. We combined a catechol/silane biomimetic composite coating system and a metal-phenolic network structure to co-deposit a dopamine-like superhydrophilic coating on polypropylene nonwoven fabrics. The modified fabric separated oil–water mixtures with a filtration efficiency of up to 99%. Besides, the as-prepared material has the property of nonstick oil underwater and outstanding stability. After 30 cycles of separation tests, the pure water flux can be restored to 94.5% of the initial value after rinsing with deionized water. It maintained underwater superoleophobic properties after being immersed in a harsh environment of pH 1 or 13 for 1 h. Compared with dopamine hydrophilic modification, this method was more economical and time-consuming and could fabricate a full-scale separation material.

KeyWords AITranslate

superwetting nonwoven fabric surface modification metalphenolic network oil/water separation codeposition
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c02382

Chinese Library Classification Number:

Citation Information:

The superwetting membrane with superhydrophilic/underwater superoleophobic properties is one of the ideal materials for treating oily wastewater. We combined a catechol/silane biomimetic composite coating system and a metal-phenolic network structure to co-deposit a dopamine-like superhydrophilic coating on polypropylene nonwoven fabrics. The modified fabric separated oil–water mixtures with a filtration efficiency of up to 99%. Besides, the as-prepared material has the property of nonstick oil underwater and outstanding stability. After 30 cycles of separation tests, the pure water flux can be restored to 94.5% of the initial value after rinsing with deionized water. It maintained underwater superoleophobic properties after being immersed in a harsh environment of pH 1 or 13 for 1 h. Compared with dopamine hydrophilic modification, this method was more economical and time-consuming and could fabricate a full-scale separation material.

quote

GB/T 7714-2015 [1] Jing Li, Yining Sun, Xiaodong Yang, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c02382.
MLA [1] Jing Li, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c02382.
APA [1] Jing Li, Yining Sun, Xiaodong Yang, Zhuan Fu, Xiangxiang Zhu, Hui Sun, & Bin Yu. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c02382
IEEE [1] Jing Li, Yining Sun, Xiaodong Yang, Zhuan Fu, Xiangxiang Zhu, Hui Sun, and Bin Yu, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c02382. keywords: {superwetting nonwoven fabric;surface modification;metalphenolic network;oil/water separation;codeposition}