Several solid solutions including(W,Ti)C,(Ta,Nb)C,(W,Ti,Ta)C and(W,Ti,Ta,Nb)C were synthesized via one-step reduction method.Ti,Ta and Nb were added to WC-7%Co cemented carbides in the forms of single carbide and solid solution,respectively.The effect of carbide addition methods on the microstructure and mechanical properties of WC-7%Co cemented carbides was investigated.The results show that the mechanical properties of WC-7%Co cemented carbides can be improved by adding the solid solution of(W,Ti,Ta,Nb)C,and bending strength,Vickers hardness and fracture toughness are 2289.9 MPa,1683 HV and 9.67 MPa·m^1/2,respectively.
KeyWords AITranslate
1张烈华,Zhigang Zak Fang,许林.WC-Co硬质合金表面渗碳强化工艺研究与应用[J].金属热处理,2016,41(2):84-87. 被引量:4
2左洪松,栾道成,王正云,李亚军,秦琴.不同含量复式碳化物对细晶硬质合金性能的影响[J].中国钨业,2011,26(6):27-30. 被引量:6
3朱运锋,叶金文,刘颖,朱军,马世卿,张蛟.(V,Ti)(C,N)固溶体粉末对WC-8%Co硬质合金性能的影响[J].功能材料,2013,44(15):2239-2243. 被引量:6
4张岩,王洪福,何泠,王海鹏,罗伟,王俊元.WC-Co截齿的材料成分及硬度分析[J].热加工工艺,2017,46(2):109-112. 被引量:2
5曹瑞军,林晨光,马旭东.WC-Co硬质合金磨损性能研究进展[J].硬质合金,2014,31(3):179-183. 被引量:15
1邝宏有,戴炳蔚,吴育藩.WC-11%(Ti,W)(Ta,Nb)C-11%Co合金制取过程中碳量和球磨时间的优化[J].硬质合金,2022,39(2):111-117.
1代新英,赵旭东,王娟.三氯化钛还原法测定铁矿石中全铁含量的方法验证[J].标准科学,2019,0(12):140-143. 被引量:2
2王齐宏.超临界机组T91/TP347H异种钢焊接接头组织与性能研究[J].电子乐园,2019,0(20):0194-0194.
3宋飞飞,曹晓,陈文婷,黄钰婕,何文胜.无机硒对桑黄(SH623)菌株菌丝生长影响研究[J].福建农业科技,2019,0(11):25-30. 被引量:1
4李芷萱.不同载体电催化剂对氢氧燃料电池的影响[J].化工设计通讯,2019,45(11):200-201.
Basic Information:
DOI:
Chinese Library Classification Number:TG135.5[一般工业技术—材料科学与工程]
Citation Information:
Several solid solutions including(W,Ti)C,(Ta,Nb)C,(W,Ti,Ta)C and(W,Ti,Ta,Nb)C were synthesized via one-step reduction method.Ti,Ta and Nb were added to WC-7%Co cemented carbides in the forms of single carbide and solid solution,respectively.The effect of carbide addition methods on the microstructure and mechanical properties of WC-7%Co cemented carbides was investigated.The results show that the mechanical properties of WC-7%Co cemented carbides can be improved by adding the solid solution of(W,Ti,Ta,Nb)C,and bending strength,Vickers hardness and fracture toughness are 2289.9 MPa,1683 HV and 9.67 MPa·m^1/2,respectively.
quote
| GB/T 7714-2015 | [1] JNG Zheng-biao, CHEN Yun, RAN Long-jiao, et al. Effect of Quaternary Composite Carbide Addition Methods on Microstructure and Mechanical Properties of WC-Co Cemented Carbides[J]. Rare Metals and Cemented Carbides, 2019(6): 79-84. |
| MLA | [1] JNG Zheng-biao, et al., "Effect of Quaternary Composite Carbide Addition Methods on Microstructure and Mechanical Properties of WC-Co Cemented Carbides." Rare Metals and Cemented Carbides, no. 6, 2019, pp. 79-84. |
| APA | [1] JNG Zheng-biao, CHEN Yun, RAN Long-jiao, GONG Yi-long, FENG Wei, & WANG Chen-xi. (2019). Effect of Quaternary Composite Carbide Addition Methods on Microstructure and Mechanical Properties of WC-Co Cemented Carbides. Rare Metals and Cemented Carbides(6), 79-84. |
| IEEE | [1] JNG Zheng-biao, CHEN Yun, RAN Long-jiao, GONG Yi-long, FENG Wei, and WANG Chen-xi, "Effect of Quaternary Composite Carbide Addition Methods on Microstructure and Mechanical Properties of WC-Co Cemented Carbides," Rare Metals and Cemented Carbides, no. 6, pp. 79-84, 2019. keywords: {WC-Co cemented carbide;one-step reduction method;solid solution;composite carbide;addition method;microstructure;mechanical property} |