Interfacial Treatment by 1,4-Phenyldiammonium Diiodide to Significantly Improve the Performance of Carbon-Based CsPbI2Br Solar Cells Interfacial Treatment by 1,4-Phenyldiammonium Diiodide to Significantly Improve the Performance of Carbon-Based CsPbI2Br Solar Cells AITranslate
Abstract AITranslate
Herein, a facile treatment to the interface of the CsPbI2Br layer and the carbon electrode using 1,4-phenyldiammonium diiodide (PhDADI) is reported for significantly improving the power conversion efficiency (PCE) of the corresponding CsPbI2Br solar cells based on a carbon electrode without a hole transport material. Owing to the positive contribution of the PhDADI treatment including the reduced defect density, improved crystallinity, and decreased surface roughness of CsPbI2Br, all key device parameters such as the open-circuit voltage, short-circuit current density, and fill factor are improved, thus leading to the PCE promotion from 11.80% for the control device without the PhDADI modification to 14.20%. Moreover, the stability test indicates that the PhDADI-modified device has the superior stability to the control device without PhDADI.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsaelm.3c01125
Chinese Library Classification Number:
Citation Information:
Herein, a facile treatment to the interface of the CsPbI2Br layer and the carbon electrode using 1,4-phenyldiammonium diiodide (PhDADI) is reported for significantly improving the power conversion efficiency (PCE) of the corresponding CsPbI2Br solar cells based on a carbon electrode without a hole transport material. Owing to the positive contribution of the PhDADI treatment including the reduced defect density, improved crystallinity, and decreased surface roughness of CsPbI2Br, all key device parameters such as the open-circuit voltage, short-circuit current density, and fill factor are improved, thus leading to the PCE promotion from 11.80% for the control device without the PhDADI modification to 14.20%. Moreover, the stability test indicates that the PhDADI-modified device has the superior stability to the control device without PhDADI.
quote
| GB/T 7714-2015 | [1] Zhe Gao, Yali Li, Wenxuan Li, et al. ACS Applied Electronic Materials, 2023(5). DOI:10.1021/acsaelm.3c01125. |
| MLA | [1] Zhe Gao, et al., ACS Applied Electronic Materials, no. 5, 2023, https://doi.org/10.1021/acsaelm.3c01125. |
| APA | [1] Zhe Gao, Yali Li, Wenxuan Li, Yanzhou Wang, Guodong Wan, Xiaoyang Liu, Yujun Fu, Qiming Liu, Deyan He, & Junshuai Li. (2023). ACS Applied Electronic Materials(5). https://doi.org/10.1021/acsaelm.3c01125 |
| IEEE | [1] Zhe Gao, Yali Li, Wenxuan Li, Yanzhou Wang, Guodong Wan, Xiaoyang Liu, Yujun Fu, Qiming Liu, Deyan He, and Junshuai Li, ACS Applied Electronic Materials, no. 5, 2023, doi: 10.1021/acsaelm.3c01125. keywords: {CsPbI2Br solar cells interface engineering 1;4phenyldiammonium diiodide carbon electrode stability} |