Electrically Controlled Reversible Polarization Fatigue–Recovery in Ferroelectric Thin Film Capacitors Electrically Controlled Reversible Polarization Fatigue–Recovery in Ferroelectric Thin Film Capacitors AITranslate

Indian Institute of Science Education and Research Berhampur;Nanoelektronik, Technische Fakultät;Nanoelektronik, Technische Fakultät; Indian Institute of Science Education and Research Berhampur
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Spontaneous polarization switchable by the externally applied electric field in ferroelectrics is a crucial feature for its technological applications; however, the reduction in switchable polarization due to bipolar electric cycling primarily hampers its potential application in nonvolatile memory. Among others, electric-field-controlled polarization recovery would be highly desirable from fundamental and technological viewpoints. In spite of recent progress in electrically controlled polarization recovery, polarization reversal behavior in fatigued and recovered states, associated device resistance change, and repeatability and reproducibility of fatigue–recovery cycles remain poorly understood. This study provides an in-depth insight into the recovery of fatigued polarization by an electric field for epitaxially grown Pb(Zr0.3Ti0.7)O3 thin film capacitor with oxide electrodes. Systematic analysis of time- and field-dependent polarization switching kinetics in pristine, fatigued, and recovered states using a suitable statistical model enabled the precise extraction of microscopic switching parameters such as mean characteristic switching times and effective activation fields. Our results demonstrate that fatigue and recovery are possibly mediated by domain pinning–depinning because of defect redistribution and trapping–detrapping of charges at nonelectroneutral domain walls. In addition, the consecutive fatigue–recovery cycles elucidate the repeatability and applicability of electric field controlled polarization recovery in ferroelectric capacitors.

KeyWords AITranslate

polarization fatigue recovery resistance defect redistribution domain wall pinning switching kinetics
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.1c01347

Chinese Library Classification Number:

Citation Information:

Spontaneous polarization switchable by the externally applied electric field in ferroelectrics is a crucial feature for its technological applications; however, the reduction in switchable polarization due to bipolar electric cycling primarily hampers its potential application in nonvolatile memory. Among others, electric-field-controlled polarization recovery would be highly desirable from fundamental and technological viewpoints. In spite of recent progress in electrically controlled polarization recovery, polarization reversal behavior in fatigued and recovered states, associated device resistance change, and repeatability and reproducibility of fatigue–recovery cycles remain poorly understood. This study provides an in-depth insight into the recovery of fatigued polarization by an electric field for epitaxially grown Pb(Zr0.3Ti0.7)O3 thin film capacitor with oxide electrodes. Systematic analysis of time- and field-dependent polarization switching kinetics in pristine, fatigued, and recovered states using a suitable statistical model enabled the precise extraction of microscopic switching parameters such as mean characteristic switching times and effective activation fields. Our results demonstrate that fatigue and recovery are possibly mediated by domain pinning–depinning because of defect redistribution and trapping–detrapping of charges at nonelectroneutral domain walls. In addition, the consecutive fatigue–recovery cycles elucidate the repeatability and applicability of electric field controlled polarization recovery in ferroelectric capacitors.

quote

GB/T 7714-2015 [1] Somnath Kale, Adrian Petraru, Hermann Kohlstedt, et al. ACS Applied Electronic Materials, 2022(4). DOI:10.1021/acsaelm.1c01347.
MLA [1] Somnath Kale, et al., ACS Applied Electronic Materials, no. 4, 2022, https://doi.org/10.1021/acsaelm.1c01347.
APA [1] Somnath Kale, Adrian Petraru, Hermann Kohlstedt, & Rohit Soni. (2022). ACS Applied Electronic Materials(4). https://doi.org/10.1021/acsaelm.1c01347
IEEE [1] Somnath Kale, Adrian Petraru, Hermann Kohlstedt, and Rohit Soni, ACS Applied Electronic Materials, no. 4, 2022, doi: 10.1021/acsaelm.1c01347. keywords: {polarization fatigue recovery resistance defect redistribution domain wall pinning switching kinetics}