daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Precise Filtering of Micro sized and Submicro sized Sticky Particles and Washing of Filter Cake AITranslate

Shanghai Dongou Microporous Filtration Technology Research and Development Center
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The paper described the characteristics of micro sized and submicro sized sticky particles during filtering and washing,especially detailed on the property of the high efficient precise micro porous filter and successful operation of filtering and washing of micro sized particles.

KeyWords AITranslate

micrormeter submicrometer precise micro porous filter filter cake washing

1张有新,赵中伟,陈爱良,霍广生.精密微孔过滤机在超细粉末过滤与洗涤应用[J].有色金属:冶炼部分,2008(5):47-49. 被引量:7

2胡世杰,高斌,宋显洪.卧式超细粉体过滤洗涤压干机[J].轻工机械,2010,28(3):78-81. 被引量:3

3闫琨,陈湘清.铝土矿选精矿过滤设备应用与展望[J].铝镁通讯,2011(2):7-9.

4张红,杜启云,刘恩华.PVDF管式膜过滤TiO_2悬浮液性能研究[J].膜科学与技术,2011,31(4):79-83. 被引量:1

5李峰杰.中美铝业铝酸钠溶液精制影响因素探讨[J].轻金属,2019,0(9):13-17.

6金倬敏,徐斌,曹果林,郇泽泉,王祝华.PGZ平板式全自动下部卸料离心机在镍钴粉体材料生产中的应用[J].粉末冶金工业,2013,23(2):55-59. 被引量:4

7韩建设.氧化铌生产工艺及装备的进展[J].稀有金属与硬质合金,2003,31(1):35-38. 被引量:14

1黄秋硕.高性能氧化铌粉体制备工艺研究[J].冶金管理,2020(15):70-71.

2韩建设,周勇.钽铌萃取分离工艺与设备进展[J].稀有金属与硬质合金,2004,32(2):15-20. 被引量:16

3邓小芬,王才明.降低Nb_2O_5中氟含量的研究[J].稀有金属与硬质合金,2005,33(1):11-13. 被引量:2

4郑典模,王振希,全水清,蒋柏泉,庄叶凯.萃取法制备高纯低氟氧化铌的研究[J].南昌大学学报:工科版,2005,27(2):71-73. 被引量:1

5韩建设,赵明智,王才明,张劲,周勇.钽铌湿法冶炼的“三废”综合治理工艺探讨[J].稀有金属与硬质合金,2006,34(4):40-44. 被引量:12

6王伟,李辉,郑培生.低品位钽铌原料的湿法冶金新工艺研究[J].稀有金属快报,2008,27(4):31-36. 被引量:10

7蒋柏泉,黄庆荣,郑典模,全水清,曾庆芳.溶剂浸取法制备低氟高纯氧化钽研究[J].南昌大学学报:工科版,2008,30(2):120-122. 被引量:1

8曹七林,姚卫东.陶瓷电容器用Nb_2O_5的制备[J].稀有金属与硬质合金,2008,36(3):43-44. 被引量:2

9崔佳娜,谌启明.立式自动压滤机及其在钽铌冶炼生产中的应用[J].稀有金属与硬质合金,2009,37(1):35-39.

10胡世杰,高斌,宋显洪.卧式超细粉体过滤洗涤压干机[J].轻工机械,2010,28(3):78-81. 被引量:3

1宋显洪.微米与亚微米级粘细微粒的精密过滤与滤饼洗涤[J].化工催化剂及甲醇技术,2000(5):86-89.

2蔡龙.湿法磷酸过滤系统对磷酸浓度及滤饼洗涤的影响[J].磷肥与复肥,1993,8(1):66-67.

3宋显洪.水玻璃液的精密微孔过滤[J].无机盐工业,2001,33(1):45-46.

4程淑莲,刘晓红,刘守信,王华,邹美捷,李建敏.从锂厂废液中回收铝的实验研究[J].江西化工,2008,24(4):153-156.

5张贤彬,杨德武,汤明东,马岩.饱和滤饼洗涤性能研究[J].辽宁化工,2006,35(11):627-629. 被引量:4

6黎国华,朱昆泉.超微细高效精密气流分级机的研究[J].适用技术市场,1994(8):21-21.

7陈勇.Φ2.5×40m立筒预热器窑改窑外分解窑成功实例简介[J].四川水泥,2000(4):18-20.

8季尚行.预分解窑100%燃无烟煤煅烧熟料成功实例[J].水泥工程,2000(5):6-7. 被引量:1

9葛祥荣.关于电刷镀技术在表面工程技术中定位的探讨[J].电刷镀技术,2003(3):32-37.

10宋显洪,宋志黎,陈金富.稀有金属超细粉体的精密微孔过滤[J].稀有金属与硬质合金,2009,37(3):48-51. 被引量:3

Basic Information:

DOI:

Chinese Library Classification Number:TQ028.53[化学工程]

Citation Information:

The paper described the characteristics of micro sized and submicro sized sticky particles during filtering and washing,especially detailed on the property of the high efficient precise micro porous filter and successful operation of filtering and washing of micro sized particles.

quote

GB/T 7714-2015 [1] SONG Xian-hong. Precise Filtering of Micro sized and Submicro sized Sticky Particles and Washing of Filter Cake[J]. Rare Metals and Cemented Carbides, 2001(1): 50-53.
MLA [1] SONG Xian-hong. "Precise Filtering of Micro sized and Submicro sized Sticky Particles and Washing of Filter Cake." Rare Metals and Cemented Carbides, no. 1, 2001, pp. 50-53.
APA [1] SONG Xian-hong. (2001). Precise Filtering of Micro sized and Submicro sized Sticky Particles and Washing of Filter Cake. Rare Metals and Cemented Carbides(1), 50-53.
IEEE [1] SONG Xian-hong, "Precise Filtering of Micro sized and Submicro sized Sticky Particles and Washing of Filter Cake," Rare Metals and Cemented Carbides, no. 1, pp. 50-53, 2001. keywords: {micrormeter,submicrometer;precise micro porous filter;filter cake washing}