Effect of Rare Earths on the Microstructure and the Performance of WC-8Co Cemented Carbides AITranslate
Abstract AITranslate
The optimizing mechanism for the microstructure and the performance of WC8Co cemented carbides by adding ultrafine mixed powder of rare earths oxidate has been explored. The results show that, the mixed powder of rare earths oxidate can not only fine the WC grain, eliminate the uncontinuous growth WC grain and raise the fee Co-phase content inalloy, but also can evidently raise the macro pressure stress on alloy surface.
KeyWords AITranslate
1郝建民,王利杰,刘寿荣,梁福起.Co相变的X射线衍射研究[J].金属学报,1994,30(1). 被引量:13
2郝庆顺,李规华,严兰英.稀土元素对WC-Co硬质合金WC晶粒尺寸的影响[J]稀土,1988(06).
3赵慕岳,易屏华,王伏生.的新型钨基合金的研究[J]稀有金属材料与工程,1988(03).
4姚萱,黄培云,吕海波.稀土氧化物对钴的马氏体相变及机械性能的影响[J]粉末冶金技术,1987(04).
5李规华,严兰英,李忠昌.稀土元素在硬质合金中的应用[J]粉末冶金技术,1986(01).
1杨世莹,贺子凯,黄鑫.添加剂对硬质合金性能的影响[J].粉末冶金工业,2005,15(6):22-25. 被引量:9
2吴其山.超细WC-Co硬质合金研究综述[J].中国钨业,2005,20(6):35-40. 被引量:19
3姜爱民,蒋显全,陈巧旺,陈异.晶粒长大抑制剂在硬质合金中的应用概况[J].硬质合金,2010,27(4):252-257. 被引量:13
4周显虎,胡如好.高炉开口钻机及其钻具产品类型与发展[J].凿岩机械气动工具,2016,42(1):41-46. 被引量:2
5李炯义,曹顺华,林信平.硬质合金中的晶粒长大抑制剂[J].硬质合金,2004,21(1):56-60. 被引量:23
1张宇,钟敏霖,刘文今.送粉激光熔覆合成制备WC/Ni硬质合金涂层及其耐磨性[J].金属热处理,2005,30(11):1-5. 被引量:26
2吴其山.超细WC-Co硬质合金研究综述[J].中国钨业,2005,20(6):35-40. 被引量:19
3张利平,张国珍,张久兴,周美玲.叠层加压SPS烧结制备梯度硬质合金[J].稀有金属材料与工程,2006,35(1):70-73. 被引量:3
4邱友绪,李宁,张伟,文玉华,张勇,周永贵.WC-Co超细晶硬质合金晶粒长大抑制剂及其机理的研究[J].硬质合金,2006,23(4):254-257. 被引量:21
5阳浩,蒋显全,李纯迟.VC和Cr_3C_2抑制剂的应用和图解优化设计[J].硬质合金,2007,24(3):188-191. 被引量:5
6孙亚丽.以紫钨为原料制备超细WC-Co硬质合金[J].中国钨业,2007,22(5):27-29. 被引量:7
7刘文彬,宋晓艳,张久兴,张国珍,刘雪梅.WC-20%Co复合粉的制备及其放电等离子烧结的研究[J].功能材料,2007,38(A10):3786-3789.
8刘书祯.超细晶硬质合金晶粒长大抑制剂的研究[J].稀有金属与硬质合金,2007,35(4):51-56. 被引量:21
9李广生.超细WC-Co硬质合金的磁性能和金相分析[J].中国钨业,2008,23(2):33-35. 被引量:12
10孙东平.晶粒长大抑制剂对WC-8%Co超细硬质合金性能的影响[J].稀有金属与硬质合金,2009,37(2):7-11. 被引量:7
1刘寿荣.稀土优化WC-Co硬质合金强韧性机理[J].有色金属,1997,49(4):76-81. 被引量:6
2刘政,林继兴.复合变质对Mg_2Si/Al复合材料组织的影响[J].轻金属,2007(1):50-53. 被引量:1
3郭爽,袁春龙.铝合金热处理工艺及其注意事项[J].黑龙江科技信息,2014,0(21):20-20. 被引量:1
4唐靖林,曾大本.铝、镁合金铸造在汽车领域的应用及发展(下)[J].金属加工:热加工,2008(7):50-53.
5刘小梅,刘岚.碳酸盐与稀土氧化物复合变质对Mg_2Si/Al20Si10Mg合金凝固组织的影响[J].江西理工大学学报,2008,29(3):45-48. 被引量:1
6魏仕勇,万珍珍,付青峰,陈志宝.混合稀土氧化物与再生WC-Co粉制备YG8硬质合金的研究[J].热加工工艺,2015,44(14):55-58. 被引量:3
7丰达明.示波极谱法测定混合稀土氧化物中铕[J].广东有色金属学报,1994,4(2):141-144. 被引量:3
8卢宏,刘毅.稀土矿物及其混合稀土氧化物[J].江西冶金,1997,17(5):85-89. 被引量:1
9林继兴.复合变质对原位Mg_2Si/Al-Si复合材料组织优化研究[J].轻合金加工技术,2008,36(11):11-14. 被引量:1
10林继兴.复合变质与热处理对不同Mg量增强过共晶Al-Si合金自生复合材料耐磨性的影响[J].铸造技术,2009,30(3):374-376.
Basic Information:
DOI:
Chinese Library Classification Number:TG135.5[一般工业技术—材料科学与工程]
Citation Information:
The optimizing mechanism for the microstructure and the performance of WC8Co cemented carbides by adding ultrafine mixed powder of rare earths oxidate has been explored. The results show that, the mixed powder of rare earths oxidate can not only fine the WC grain, eliminate the uncontinuous growth WC grain and raise the fee Co-phase content inalloy, but also can evidently raise the macro pressure stress on alloy surface.
quote
| GB/T 7714-2015 | [1] LIANG Fu-qi, HAO Jian-min, HU Ming, et al. Effect of Rare Earths on the Microstructure and the Performance of WC-8Co Cemented Carbides[J]. Rare Metals and Cemented Carbides, 1997(2): 22-26. |
| MLA | [1] LIANG Fu-qi, et al., "Effect of Rare Earths on the Microstructure and the Performance of WC-8Co Cemented Carbides." Rare Metals and Cemented Carbides, no. 2, 1997, pp. 22-26. |
| APA | [1] LIANG Fu-qi, HAO Jian-min, HU Ming, YANG Rui, & LIU Shou-rong. (1997). Effect of Rare Earths on the Microstructure and the Performance of WC-8Co Cemented Carbides. Rare Metals and Cemented Carbides(2), 22-26. |
| IEEE | [1] LIANG Fu-qi, HAO Jian-min, HU Ming, YANG Rui, and LIU Shou-rong, "Effect of Rare Earths on the Microstructure and the Performance of WC-8Co Cemented Carbides," Rare Metals and Cemented Carbides, no. 2, pp. 22-26, 1997. keywords: {cemented carbide, mixed powder of rare earths oxidate} |