The negative Poisson’s (NPR) ratio in a two-dimensional (2D) material is a counterintuitive mechanical property that facilitates the development of nanoscale devices with sophisticated functionality. Inspired by the peculiar buckled lower-symmetric, trilayered geometry of pentagonal monolayers, we theoretically predict penta-SiCN, a ternary auxetic metallic monolayer with highly tunable NPR. The penta-SiCN is structurally, thermally, dynamically, and mechanically stable, and sustainable at and beyond room temperature with experimental feasibility. It possesses nontrivial geometrical and mechanical isotropy and relatively moderate thickness. Remarkably, the shorter and quasi sp3-hybridized C–N bond and the rigidity against the strain allow the monolayer to possess a high value of NPR (−0.136), even higher than that of black phosphorene, extendable up to −0.639 by 4% of biaxial stretching. On the other hand, the 2D Young’s modulus of 129.88 N/m decreases to 41.34 N/m at equivalent stretching, indicating relative softening and flexibility. Interestingly, a buckled-to-planar phase transition is identified at 10% biaxial strain before it suffers the fracture at 16%. Additionally, the strong optical anisotropy, absorbance (up to 6.51× 105 cm–1), and presence of plasmon frequency demonstrate its potential application in optomechanical and plasmonics.

KeyWords AITranslate

density functional theory pentaSiCN negative Poisson’s ratio mechanical properties strains effect electronic propertiesShow More
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.2c00265

Chinese Library Classification Number:

Citation Information:

The negative Poisson’s (NPR) ratio in a two-dimensional (2D) material is a counterintuitive mechanical property that facilitates the development of nanoscale devices with sophisticated functionality. Inspired by the peculiar buckled lower-symmetric, trilayered geometry of pentagonal monolayers, we theoretically predict penta-SiCN, a ternary auxetic metallic monolayer with highly tunable NPR. The penta-SiCN is structurally, thermally, dynamically, and mechanically stable, and sustainable at and beyond room temperature with experimental feasibility. It possesses nontrivial geometrical and mechanical isotropy and relatively moderate thickness. Remarkably, the shorter and quasi sp3-hybridized C–N bond and the rigidity against the strain allow the monolayer to possess a high value of NPR (−0.136), even higher than that of black phosphorene, extendable up to −0.639 by 4% of biaxial stretching. On the other hand, the 2D Young’s modulus of 129.88 N/m decreases to 41.34 N/m at equivalent stretching, indicating relative softening and flexibility. Interestingly, a buckled-to-planar phase transition is identified at 10% biaxial strain before it suffers the fracture at 16%. Additionally, the strong optical anisotropy, absorbance (up to 6.51× 105 cm–1), and presence of plasmon frequency demonstrate its potential application in optomechanical and plasmonics.

quote

GB/T 7714-2015 [1] Shambhu Bhandari Sharma, Issam A. Qattan, Meghnath Jaishi, et al. ACS Applied Electronic Materials, 2022(4). DOI:10.1021/acsaelm.2c00265.
MLA [1] Shambhu Bhandari Sharma, et al., ACS Applied Electronic Materials, no. 4, 2022, https://doi.org/10.1021/acsaelm.2c00265.
APA [1] Shambhu Bhandari Sharma, Issam A. Qattan, Meghnath Jaishi, & Durga Paudyal. (2022). ACS Applied Electronic Materials(4). https://doi.org/10.1021/acsaelm.2c00265
IEEE [1] Shambhu Bhandari Sharma, Issam A. Qattan, Meghnath Jaishi, and Durga Paudyal, ACS Applied Electronic Materials, no. 4, 2022, doi: 10.1021/acsaelm.2c00265. keywords: {density functional theory pentaSiCN negative Poisson’s ratio mechanical properties strains effect electronic propertiesShow More}