Research on the Friction Properties of Boron Carbide AITranslate
Abstract AITranslate
In this article ,the main production methods, the friction properties and the ultra low friction mechanism of boron carbide materials are briefly introduced,The ways to get ultralow friction coefficient are presented,and the exising problems and the forecasting of future is also pointed out.
KeyWords AITranslate
1周荣兴,邓克勤,杨菊美.耐蚀耐磨碳化硼轴承材料的研制[J].硬质合金,1995,12(2):102-106. 被引量:4
2(罗)伊留克(IuanI.Iliuc)著,汪一麟,陈耕.薄层摩擦学[M]机械工业出版社,1986.
3J. C VIALA,J BOUIX,G GONZALEZ,C ESNOUF. Chemical reactivity of aluminium with boron carbide[J] 1997,Journal of Materials Science(17):4559~4573
4V. A. Lavrenko,Yu. G. Gogotsi. Influence of oxidation on the composition and structure of the surface layer of hot-pressed boron carbide[J] 1988,Oxidation of Metals(3-4):193~202
1吕亮,朱华,Feng TANG.碳化硼增强铝基复合材料的摩擦磨损性能[J].机械工程材料,2007,31(10):64-66. 被引量:7
2李青松,罗震,李中伟,张东文.铝合金电阻点焊电极延寿技术的研究[J].电焊机,2009,39(7):59-61. 被引量:3
1刘国强,刘炳.颗粒增强型铝基复合材料摩擦磨损性能研究现状与展望[J].汽车零部件,2009(9):59-61. 被引量:1
2张友法,余新泉,陈锋,于良.B4C/Al复合材料摩擦磨损特性研究[J].特种铸造及有色合金,2010(10):901-904. 被引量:2
3胡望杰,闫洪,周冰锋.B_4C颗粒对AZ 61蠕变及磨损性能影响的研究[J].现代制造工程,2011(5):10-13. 被引量:1
4任鑫磊,邱然锋,关精伟,梁欣,李娜.热补偿电阻点焊铝合金接头的性能[J].电焊机,2011,41(6):46-50.
5吴松,王敏,程轩挺,吴嘉元,孙游.铝合金电阻点焊研究现状及工业应用[J].电焊机,2013,43(9):10-16. 被引量:10
6迟长志,李世欣,张永胜.SiC_p对铝基复合材料组织和磨损性能的影响[J].特种铸造及有色合金,2014(4):426-429. 被引量:6
7李敬勇,刘涛,郭宇文.搅拌摩擦加工铝基复合材料的高温摩擦磨损性能[J].材料工程,2015,43(6):21-25. 被引量:3
8元琳琳.含硼金属复合材料的研究与应用[J].有色金属与稀土应用,2016,0(3):4-23.
9刘磊,纵荣荣,李乐乐,王洪玮,齐乐.轻量化汽车电阻点焊技术的研究与应用[J].时代汽车,2019(3):131-134. 被引量:4
10胡琴,杨越,曹雷刚.高温热处理气氛对B_(4)C/Al复合材料微观组织的影响[J].金属材料与冶金工程,2021,49(4):15-19.
1陈中.关于摩擦因素λ的计算[J].化工设计通讯,1990,16(1):51-53. 被引量:2
2Jank.,AF,王占山.W/B4C X射多层膜反射镜[J].光机电世界,1993,10(3):61-68.
3邹娣,刘晓.高酸值乙醇润滑下几种活塞环材料的摩擦学性能[J].重庆工商大学学报:自然科学版,2006,23(1):89-92. 被引量:2
4刘晓,李生华,赵晚成,金元生.低酸度乙醇润滑下几种活塞环材料的摩擦学性能研究[J].润滑与密封,2005,30(4):36-38.
5袁国洲,姚萍屏,樊毅.SiO_2和B_4C组合对铁铜基摩擦材料性能的影响[J].非金属矿,1999(4):47-49. 被引量:16
6王国亮,蔡星会,姬国勋,卢江仁.B_4C陶瓷摩擦学性能研究现状与分析[J].材料导报,2012,26(7):45-48. 被引量:1
7安琪.NuSil公司推出低摩擦因数的有机硅涂层[J].橡胶科技市场,2010(11):22-22.
8吕俊霞,马月英,张俊平,王占山,曹健林.工作波长短于10nm的软X射线多层膜[J].光学精密工程,1996,4(2):19-24. 被引量:2
9张传伟,荆翠妮,古乐,马欣新.陶瓷球表面类金刚石碳膜均匀沉积机构设计及运动仿真[J].中国科技论文,2012,7(8):598-602. 被引量:1
10侯立飞,易荣清,杜华冰,李朝光,何小安,黎航,刘慎业,朱京涛,赵屹东,崔明启.软X光多层镜反射率的标定与修正[J].光子学报,2009,38(4):827-831.
Basic Information:
DOI:
Chinese Library Classification Number:TH117[机械工程—机械设计及理论];TQ174.758[化学工程—陶瓷工业]
Citation Information:
In this article ,the main production methods, the friction properties and the ultra low friction mechanism of boron carbide materials are briefly introduced,The ways to get ultralow friction coefficient are presented,and the exising problems and the forecasting of future is also pointed out.
quote
| GB/T 7714-2015 | [1] FANG Shan-feng, WANG Ling-sen, WU Fang. Research on the Friction Properties of Boron Carbide[J]. Rare Metals and Cemented Carbides, 2000(4): 39-43. |
| MLA | [1] FANG Shan-feng, et al., "Research on the Friction Properties of Boron Carbide." Rare Metals and Cemented Carbides, no. 4, 2000, pp. 39-43. |
| APA | [1] FANG Shan-feng, WANG Ling-sen, & WU Fang. (2000). Research on the Friction Properties of Boron Carbide. Rare Metals and Cemented Carbides(4), 39-43. |
| IEEE | [1] FANG Shan-feng, WANG Ling-sen, and WU Fang, "Research on the Friction Properties of Boron Carbide," Rare Metals and Cemented Carbides, no. 4, pp. 39-43, 2000. keywords: {B 4C;production method;friction property;mechanism} |