Stiff, Strong, Tough, and Highly Stretchable Hydrogels Based on Dual Stimuli-Responsive Semicrystalline Poly(urethane–urea) Copolymers AITranslate

Centre Català del Plàstic (CCP), Universitat Politècnica de Catalunya Barcelona Tech (EEBE-UPC);Univ. Lille;Univ. Lille; Institute of Materials (IMX);Institut des Sciences et Ingénierie Chimiques (ISIC), École Polytechnique Fédérale de Lausanne (EPFL); Koc University; Koc University; Turkey|Sabanci University Integrated Manufacturing Technologies Research and Application Center & Composite Technologies Center of Excellence; Turkey|Sabanci University Integrated Manufacturing Technologies Research and Application Center & Composite Technologies Center of Excellence
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

There has been a considerable interest in developing stiff, strong, tough, and highly stretchable hydrogels in various fields of science and technology including biomedical and sensing applications. However, simultaneous optimization of stiffness, strength, toughness, and extensibility is a challenge for any material, and hydrogels are well-known to be mechanically weak materials. Here, we demonstrate that poly(ethylene oxide)-based dual stimuli-responsive semicrystalline poly(urethane–urea) (PU) copolymers with high hard segment contents (30 and 40%) can be utilized as stiff, strong, tough, and highly stretchable hydrogels with an elastic modulus (4–10 MPa) tens to hundreds of times higher than that of conventional hydrogels (0.01–0.1 MPa), strength (7–13 MPa) and toughness (53–74 MJ·m–3) fairly comparable to those of the toughest hydrogels reported in the literature, and stretchability beyond 10 times their initial length (1000–1250%). In addition, the shape-memory program has been used to tune the room temperature stiffness and strength of the studied PU copolymers. Finally, the materials show fast shape recovery (less than 10 s) during both heat- and water-activated shape memory cycles, which can be adjusted by a simple modulation of the hard segment content and/or soft segment molecular weight. Our findings may be of interest in emerging biomedical and sensing applications.

KeyWords AITranslate

poly(urethane−urea) poly(ethylene oxide) stimuliresponsiveness shape memory hydrogels toughening
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c00969

Chinese Library Classification Number:

Citation Information:

There has been a considerable interest in developing stiff, strong, tough, and highly stretchable hydrogels in various fields of science and technology including biomedical and sensing applications. However, simultaneous optimization of stiffness, strength, toughness, and extensibility is a challenge for any material, and hydrogels are well-known to be mechanically weak materials. Here, we demonstrate that poly(ethylene oxide)-based dual stimuli-responsive semicrystalline poly(urethane–urea) (PU) copolymers with high hard segment contents (30 and 40%) can be utilized as stiff, strong, tough, and highly stretchable hydrogels with an elastic modulus (4–10 MPa) tens to hundreds of times higher than that of conventional hydrogels (0.01–0.1 MPa), strength (7–13 MPa) and toughness (53–74 MJ·m–3) fairly comparable to those of the toughest hydrogels reported in the literature, and stretchability beyond 10 times their initial length (1000–1250%). In addition, the shape-memory program has been used to tune the room temperature stiffness and strength of the studied PU copolymers. Finally, the materials show fast shape recovery (less than 10 s) during both heat- and water-activated shape memory cycles, which can be adjusted by a simple modulation of the hard segment content and/or soft segment molecular weight. Our findings may be of interest in emerging biomedical and sensing applications.

quote

GB/T 7714-2015 [1] Nicolas Candau, Gregory Stoclet, JeanFrançois Tahon, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.1c00969.
MLA [1] Nicolas Candau, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.1c00969.
APA [1] Nicolas Candau, Gregory Stoclet, JeanFrançois Tahon, Adrien Demongeot, Pascal Schouwink, Emel Yilgor, Iskender Yilgor, Yusuf Z. Menceloglu, & Oguzhan Oguz. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.1c00969
IEEE [1] Nicolas Candau, Gregory Stoclet, JeanFrançois Tahon, Adrien Demongeot, Pascal Schouwink, Emel Yilgor, Iskender Yilgor, Yusuf Z. Menceloglu, and Oguzhan Oguz, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.1c00969. keywords: {poly(urethane−urea);poly(ethylene oxide);stimuliresponsiveness;shape memory;hydrogels;toughening}