Secondary Energy Conversion Devices Based on Cylindrical Liquid Crystalline Elastomer-Assisted Triboelectric Generators Secondary Energy Conversion Devices Based on Cylindrical Liquid Crystalline Elastomer-Assisted Triboelectric Generators AITranslate

National Cheng Kung University; National Cheng Kung University; National Cheng Kung University; National Cheng Kung University; National Cheng Kung University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

In this study, we demonstrate the preparation of an available secondary energy conversion device that is based on cylindrical liquid crystal elastomers (CLCE) that are equipped with a triboelectric energy generator. Near-infrared energy was changed to mechanical energy and then to electric power. A series of thermally responsive CLCE actuators were fabricated, which show reversible thermal responsive shortening and lengthening actuations. To enhance the near-infrared (NIR) sensitivity, polydopamine (PDA) was coated on the CLCE actuator surface to acquire reversible NIR-responsive actuations. To develop secondary energy conversion devices, a poly(acrylamide)-lithium chloride (PAAm-LiCl) hydrogel was used as a polymeric electrolyte, which was further encapsulated with polydimethylsiloxane (PDMS). The fabricated PDA-coated CLCE actuators were combined with a PAAm-LiCl hydrogel-assembled triboelectric nanogenerator (TENG) to create a photomechanical–electrical secondary energy conversion device. By tapping the PAAm-LiCl hydrogel-assembled TENG, an output voltage of 200 V and a current of 2.5 μA were generated, which lit up 8 LEDs. For CLCE-assisted TENGs, the fabricated secondary energy conversion device generated a voltage of 2.1 V with a current of 90 nA, which lit up a green LED. Based on the results, an available method for fabricating secondary energy conversion devices via predesigned CLCEs was demonstrated successfully, which shows great potential for applications in the field of energy conversion systems.

KeyWords AITranslate

cylindrical liquid crystalline elastomers triboelectric nanogenerator photosensitive actuators hydrogels Michael addition
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.1c01307

Chinese Library Classification Number:

Citation Information:

In this study, we demonstrate the preparation of an available secondary energy conversion device that is based on cylindrical liquid crystal elastomers (CLCE) that are equipped with a triboelectric energy generator. Near-infrared energy was changed to mechanical energy and then to electric power. A series of thermally responsive CLCE actuators were fabricated, which show reversible thermal responsive shortening and lengthening actuations. To enhance the near-infrared (NIR) sensitivity, polydopamine (PDA) was coated on the CLCE actuator surface to acquire reversible NIR-responsive actuations. To develop secondary energy conversion devices, a poly(acrylamide)-lithium chloride (PAAm-LiCl) hydrogel was used as a polymeric electrolyte, which was further encapsulated with polydimethylsiloxane (PDMS). The fabricated PDA-coated CLCE actuators were combined with a PAAm-LiCl hydrogel-assembled triboelectric nanogenerator (TENG) to create a photomechanical–electrical secondary energy conversion device. By tapping the PAAm-LiCl hydrogel-assembled TENG, an output voltage of 200 V and a current of 2.5 μA were generated, which lit up 8 LEDs. For CLCE-assisted TENGs, the fabricated secondary energy conversion device generated a voltage of 2.1 V with a current of 90 nA, which lit up a green LED. Based on the results, an available method for fabricating secondary energy conversion devices via predesigned CLCEs was demonstrated successfully, which shows great potential for applications in the field of energy conversion systems.

quote

GB/T 7714-2015 [1] HungYi Chen, BingHan Wu, SzuYin Ou, et al. ACS Applied Electronic Materials, 2022(4). DOI:10.1021/acsaelm.1c01307.
MLA [1] HungYi Chen, et al., ACS Applied Electronic Materials, no. 4, 2022, https://doi.org/10.1021/acsaelm.1c01307.
APA [1] HungYi Chen, BingHan Wu, SzuYin Ou, ChaoHui Zhuang, & ChunYen Liu. (2022). ACS Applied Electronic Materials(4). https://doi.org/10.1021/acsaelm.1c01307
IEEE [1] HungYi Chen, BingHan Wu, SzuYin Ou, ChaoHui Zhuang, and ChunYen Liu, ACS Applied Electronic Materials, no. 4, 2022, doi: 10.1021/acsaelm.1c01307. keywords: {cylindrical liquid crystalline elastomers triboelectric nanogenerator photosensitive actuators hydrogels Michael addition}