daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

High-Performance Degradable Poly(hexahydrotriazine)s and Their Potential for Tribological Applications AITranslate

Henan University of Science and Technology; Jiangsu University; Jiangsu University; Jiangsu University; Jiangsu University; Jiangsu University; Jiangsu University; Tiangong University; Tiangong University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The isomeric poly(hexahydrotriazine)s (PHTs) were prepared, based on their hemiaminal dynamic covalent networks via a facile method at 50 °C, through 1,3-bis(4-aminophenoxy)-benzene (TPE-R) and 1,4-bis(4-aminophenoxy)-benzene (TPE-Q) with formaldehyde. The influence of chain isomerism on thermal stability, mechanical properties, tribological properties, and the degradation rate of PHTs was investigated. The advantage of (TPE-Q)-PHTs compared with that of (TPE-R)-PHTs is that they possessed a higher glass transition temperature (Tg) of 187 °C, a higher Yang’s modulus of 10.7 GPa, and rapid degradation rate. Additionally, the (TPE-Q)-PHTs exhibited outstanding self-lubricating performance as compared to (TPE-Q)-PHTs because the para-connecting isomers showed lower surface energy, lower surface roughness, and higher hardness that effectively weakened the bonding force between friction pairs. Overall, the study of PHTs facilitates their practical application of energy conservation and environmental protection in the tribological industry.

KeyWords AITranslate

isomeric poly(hexahydrotriazine)s synthesis mechanical properties tribological properties degradation
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c01049

Chinese Library Classification Number:

Citation Information:

The isomeric poly(hexahydrotriazine)s (PHTs) were prepared, based on their hemiaminal dynamic covalent networks via a facile method at 50 °C, through 1,3-bis(4-aminophenoxy)-benzene (TPE-R) and 1,4-bis(4-aminophenoxy)-benzene (TPE-Q) with formaldehyde. The influence of chain isomerism on thermal stability, mechanical properties, tribological properties, and the degradation rate of PHTs was investigated. The advantage of (TPE-Q)-PHTs compared with that of (TPE-R)-PHTs is that they possessed a higher glass transition temperature (Tg) of 187 °C, a higher Yang’s modulus of 10.7 GPa, and rapid degradation rate. Additionally, the (TPE-Q)-PHTs exhibited outstanding self-lubricating performance as compared to (TPE-Q)-PHTs because the para-connecting isomers showed lower surface energy, lower surface roughness, and higher hardness that effectively weakened the bonding force between friction pairs. Overall, the study of PHTs facilitates their practical application of energy conservation and environmental protection in the tribological industry.

quote

GB/T 7714-2015 [1] Chunying Min, Yuzi Yang, Hongyu Liang, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.1c01049.
MLA [1] Chunying Min, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.1c01049.
APA [1] Chunying Min, Yuzi Yang, Hongyu Liang, Zengbao He, Qiuying Li, Jinfeng Zhu, Kan Zhang, Haiting Shi, & Wei Wang. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.1c01049
IEEE [1] Chunying Min, Yuzi Yang, Hongyu Liang, Zengbao He, Qiuying Li, Jinfeng Zhu, Kan Zhang, Haiting Shi, and Wei Wang, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.1c01049. keywords: {isomeric poly(hexahydrotriazine)s;synthesis;mechanical properties;tribological properties;degradation}