Solubility of Nd2O3in the NaF-AlF3Molten Salt System AITranslate
Abstract AITranslate
The solubility of Nd2O3in the NaF-AlF3molten salt system was systematically determined using the isothermal saturation method,with a focus on the effects of molten salt temperature(1010~1070℃)and NaF/AlF3molar ratio(2.0~2.6)on its solubility.A first-order regression model correlating the solubility of Nd2O3with molten salt temperature and NaF/AlF3molar ratio was established through experimental data fitting.The results demonstrate that the dissolution equilibrium of Nd2O3in the NaF-AlF3molten salt is achieved in no less than 60 min,and the solubility significantly increases with increasing molten salt temperature and higher NaF/AlF3molar ratio.The solubility of Nd2O3reaches a maximum value of 6.20%at 1070℃with a NaF/AlF3molar ratio of 2.6.Within the experimental parameter range,the constructed regression model achieves a coefficient of determination(R2)of 0.983.
KeyWords AITranslate
Basic Information:
DOI:
Chinese Library Classification Number:TF845.6[冶金工程—有色金属冶金]
Citation Information:
The solubility of Nd2O3in the NaF-AlF3molten salt system was systematically determined using the isothermal saturation method,with a focus on the effects of molten salt temperature(1010~1070℃)and NaF/AlF3molar ratio(2.0~2.6)on its solubility.A first-order regression model correlating the solubility of Nd2O3with molten salt temperature and NaF/AlF3molar ratio was established through experimental data fitting.The results demonstrate that the dissolution equilibrium of Nd2O3in the NaF-AlF3molten salt is achieved in no less than 60 min,and the solubility significantly increases with increasing molten salt temperature and higher NaF/AlF3molar ratio.The solubility of Nd2O3reaches a maximum value of 6.20%at 1070℃with a NaF/AlF3molar ratio of 2.6.Within the experimental parameter range,the constructed regression model achieves a coefficient of determination(R2)of 0.983.
quote
| GB/T 7714-2015 | [1] HUANG Yi-peng, YANG Jun, QI Deng-rui, et al. Solubility of Nd2O3in the NaF-AlF3Molten Salt System[J]. Rare Metals and Cemented Carbides, 2025(5): 7-13. |
| MLA | [1] HUANG Yi-peng, et al., "Solubility of Nd2O3in the NaF-AlF3Molten Salt System." Rare Metals and Cemented Carbides, no. 5, 2025, pp. 7-13. |
| APA | [1] HUANG Yi-peng, YANG Jun, QI Deng-rui, & YANG Feng-li. (2025). Solubility of Nd2O3in the NaF-AlF3Molten Salt System. Rare Metals and Cemented Carbides(5), 7-13. |
| IEEE | [1] HUANG Yi-peng, YANG Jun, QI Deng-rui, and YANG Feng-li, "Solubility of Nd2O3in the NaF-AlF3Molten Salt System," Rare Metals and Cemented Carbides, no. 5, pp. 7-13, 2025. keywords: {NdO;solubility;NaF-AlFmolten salt;isothermal saturation method;regression model;molten salt temperature;NaF/AlFmolar ratio} |