Broadband Photosensitive Medium Based on Amorphous Equichalcogenides Broadband Photosensitive Medium Based on Amorphous Equichalcogenides AITranslate
Abstract AITranslate
A photosensitive medium based on amorphous equichalcogenide thin films containing germanium and antimony is proposed with characteristics promising for applications in all-chalcogenide photonics, sensors, and photovoltaics. Optical properties, temperature, and exposure wavelength dependence of DC electrical conductivity are shown to be comparable with those for halide perovskites, which potentially makes amorphous equichalcogenides a very attractive alternative. The change in dark resistivity with temperature is found to follow exponential decay, covering 2 orders of magnitude over a 70 K temperature interval. Light exposure leads to several orders of relative changes in a current when compared to its dark value. A strong photocurrent response is observed under low power (milliwatts range) exposure across the entire 400–1000 nm range of the investigated wavelengths. An increase in temperature leads to a decrease in the photoresponse of the developed material, which is found to vanish at temperatures higher than 120 °C when only a few milliwatts of exposure power is used.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsaelm.2c01075
Chinese Library Classification Number:
Citation Information:
A photosensitive medium based on amorphous equichalcogenide thin films containing germanium and antimony is proposed with characteristics promising for applications in all-chalcogenide photonics, sensors, and photovoltaics. Optical properties, temperature, and exposure wavelength dependence of DC electrical conductivity are shown to be comparable with those for halide perovskites, which potentially makes amorphous equichalcogenides a very attractive alternative. The change in dark resistivity with temperature is found to follow exponential decay, covering 2 orders of magnitude over a 70 K temperature interval. Light exposure leads to several orders of relative changes in a current when compared to its dark value. A strong photocurrent response is observed under low power (milliwatts range) exposure across the entire 400–1000 nm range of the investigated wavelengths. An increase in temperature leads to a decrease in the photoresponse of the developed material, which is found to vanish at temperatures higher than 120 °C when only a few milliwatts of exposure power is used.
quote
| GB/T 7714-2015 | [1] Roman Golovchak, Jarres Plummer, Andriy Kovalskiy, et al. ACS Applied Electronic Materials, 2022(4). DOI:10.1021/acsaelm.2c01075. |
| MLA | [1] Roman Golovchak, et al., ACS Applied Electronic Materials, no. 4, 2022, https://doi.org/10.1021/acsaelm.2c01075. |
| APA | [1] Roman Golovchak, Jarres Plummer, Andriy Kovalskiy, Yuriy Holovchak, Tetyana Ignatova, Kyle Nowlin, Anthony Trofe, Yaroslav Shpotyuk, Catherine BoussardPledel, & Bruno Bureau. (2022). ACS Applied Electronic Materials(4). https://doi.org/10.1021/acsaelm.2c01075 |
| IEEE | [1] Roman Golovchak, Jarres Plummer, Andriy Kovalskiy, Yuriy Holovchak, Tetyana Ignatova, Kyle Nowlin, Anthony Trofe, Yaroslav Shpotyuk, Catherine BoussardPledel, and Bruno Bureau, ACS Applied Electronic Materials, no. 4, 2022, doi: 10.1021/acsaelm.2c01075. keywords: {chalcogenide glass photocurrent light sensitivity wavelength dependence temperature dependence} |