daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Investigation on Technology for Carbon-added Production of Low-O_2 Ta Rod from High-O_2 Ta Powder AITranslate

Zhuzhou Cemented Carbide Factory Tantalum Niobium Products Branch
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Investigation is made on the production process of Low O 2 Ta rod from high-O 2 Ta powder,The results show that the Low-O 2 quality Ta rod can be obtained by carbon added pre-sintering and reduction of high-O 2 Ta Powder.The process is simple,energy-saving with less loss and distinct economic benefits.

KeyWords AITranslate

high-O 2 Ta powder carbon addition pre-stntering reduction Low-O 2 Ta rod

1胡小锋,许茜,吴艳.钽粉制备工艺研究进展[J].材料导报,2005,19(10):97-99. 被引量:11

2杨国启,何季麟,郑爱国,罗文,周小军,李军义.电容器级高比容钽粉制备工艺研究进展[J].湖南有色金属,2014,30(1):48-52. 被引量:17

3张延宾,郑侠.钽条高温真空烧结炉的研制[J].工业加热,2018,47(1):31-33. 被引量:1

4王晖,李延超,张新,王峰,梁静,张小明.高温烧结Ta-W合金条工艺研究[J].有色金属材料与工程,2019,40(2):21-24. 被引量:1

1蒋柏泉,黄庆荣,郑典模,全水清,曾庆芳.溶剂浸取法制备低氟高纯氧化钽研究[J].南昌大学学报:工科版,2008,30(2):120-122. 被引量:1

2梁栋,侯击波,殷涛,尚福军,史洪刚,黄伟,史文璐.感应等离子工艺参数对制备电容器级钽粉性能的影响[J].兵器材料科学与工程,2010,33(3):46-50. 被引量:5

3王东新,李军义,孙本双,任晓,何季麟.钽粉制备新工艺研究进展[J].湖南有色金属,2011,27(3):34-37. 被引量:19

4王东新,李军义,孙本双,任晓,何季麟.还原氧化钽制备钽粉工艺研究进展[J].中国材料进展,2011,30(10):54-58. 被引量:1

5杨国启,何季麟,郑爱国,罗文,周小军,李军义.电容器级高比容钽粉制备工艺研究进展[J].湖南有色金属,2014,30(1):48-52. 被引量:17

6李仲香,杨国启,程越伟,陈学清,李霞.表面活性剂在钽粉球磨工艺中的应用研究[J].湖南有色金属,2016,32(6):40-43. 被引量:1

7李慧,雒国清,程越伟,马跃忠,杨国启,柏林,马海燕.高比容钽粉的微观结构及电性能特性的研究[J].湖南有色金属,2017,33(1):48-52. 被引量:4

8杨国启,孙宇,李仲香,陈学清,林辅坤,程越伟,雒国清.高压高比容钽粉的制备及性能表征[J].湖南有色金属,2017,33(2):43-47. 被引量:3

9雒国清,李慧,赵春霞,马海燕.不同粒度高比容钽粉性能分析[J].湖南有色金属,2017,33(5):45-48. 被引量:2

10李丽君,杨国启,梁宏源,马应会.KCl/NaCl中pH的测定[J].湖南有色金属,2017,33(5):71-73.

1王时光,高灿华.高氧钽粉用镁处理降氧的研究[J].稀有金属与硬质合金,1989(1):9-12. 被引量:2

2洪顺章,文希孟.钽粉生产用钠净化装置[J].中国原子能科学研究院年报,2001(1):145-145.

3PrabhatKumar,HenningUhlenhut,李学芳,佘建芳.粉末冶金钽制品的最新进展[J].国外难熔金属与硬质材料,2003,19(2):57-63. 被引量:2

Basic Information:

DOI:

Chinese Library Classification Number:TF125.242[冶金工程—粉末冶金]

Citation Information:

Investigation is made on the production process of Low O 2 Ta rod from high-O 2 Ta powder,The results show that the Low-O 2 quality Ta rod can be obtained by carbon added pre-sintering and reduction of high-O 2 Ta Powder.The process is simple,energy-saving with less loss and distinct economic benefits.

quote

GB/T 7714-2015 [1] LI Shi-lin. Investigation on Technology for Carbon-added Production of Low-O_2 Ta Rod from High-O_2 Ta Powder[J]. Rare Metals and Cemented Carbides, 2001(4): 13-17.
MLA [1] LI Shi-lin. "Investigation on Technology for Carbon-added Production of Low-O_2 Ta Rod from High-O_2 Ta Powder." Rare Metals and Cemented Carbides, no. 4, 2001, pp. 13-17.
APA [1] LI Shi-lin. (2001). Investigation on Technology for Carbon-added Production of Low-O_2 Ta Rod from High-O_2 Ta Powder. Rare Metals and Cemented Carbides(4), 13-17.
IEEE [1] LI Shi-lin, "Investigation on Technology for Carbon-added Production of Low-O_2 Ta Rod from High-O_2 Ta Powder," Rare Metals and Cemented Carbides, no. 4, pp. 13-17, 2001. keywords: {high-O 2 Ta powder;carbon addition;pre-stntering;reduction;Low-O 2 Ta rod}