HfTaOx Rectifying Layer for HfOx-Based RRAM for High-Accuracy Neuromorphic Computing Applications HfTaOx Rectifying Layer for HfOx-Based RRAM for High-Accuracy Neuromorphic Computing Applications AITranslate

National Cheng Kung University; National Cheng Kung University; National Cheng Kung University; National Cheng Kung University; National Cheng Kung University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

In this study, a Ta2O5-doped HfOx (HfTaOx) thin film was deposited by cosputtering to serve as the rectifying layer for HfOx-based resistive random-access memory (RRAM) with a final structure of Pt/HfOx/HfTaOx/TiN/SiO2/Si. Incorporating the appropriate proportion of lattice and nonlattice O in the rectifying layer enabled forming-free RRAM operation. Moreover, by modifying the compliance current and making use of the deep reset operation, multilevel resistance states were realized. In neuromorphic computing, when mimicking artificial synapses, potentiation and depression were successfully induced, and low nonlinearity was demonstrated, implying efficient weight modulation and reduced energy and time for neural network training. Software-comparable Modified National Institute of Standards and Technology (MNIST) handwritten digit database inference accuracy (97.54%) was achieved for an RRAM-based fully connected neural network with the HfTaOx rectifying layer.

KeyWords AITranslate

RF sputtering Ta2O5 doping rectifying layer high accuracy neuromorphic computing RRAM
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.3c00026

Chinese Library Classification Number:

Citation Information:

In this study, a Ta2O5-doped HfOx (HfTaOx) thin film was deposited by cosputtering to serve as the rectifying layer for HfOx-based resistive random-access memory (RRAM) with a final structure of Pt/HfOx/HfTaOx/TiN/SiO2/Si. Incorporating the appropriate proportion of lattice and nonlattice O in the rectifying layer enabled forming-free RRAM operation. Moreover, by modifying the compliance current and making use of the deep reset operation, multilevel resistance states were realized. In neuromorphic computing, when mimicking artificial synapses, potentiation and depression were successfully induced, and low nonlinearity was demonstrated, implying efficient weight modulation and reduced energy and time for neural network training. Software-comparable Modified National Institute of Standards and Technology (MNIST) handwritten digit database inference accuracy (97.54%) was achieved for an RRAM-based fully connected neural network with the HfTaOx rectifying layer.

quote

GB/T 7714-2015 [1] TingJia Chang, HoangHiep Le, ChengYing Li, et al. ACS Applied Electronic Materials, 2023(5). DOI:10.1021/acsaelm.3c00026.
MLA [1] TingJia Chang, et al., ACS Applied Electronic Materials, no. 5, 2023, https://doi.org/10.1021/acsaelm.3c00026.
APA [1] TingJia Chang, HoangHiep Le, ChengYing Li, ShengYuan Chu, & Darsen D. Lu. (2023). ACS Applied Electronic Materials(5). https://doi.org/10.1021/acsaelm.3c00026
IEEE [1] TingJia Chang, HoangHiep Le, ChengYing Li, ShengYuan Chu, and Darsen D. Lu, ACS Applied Electronic Materials, no. 5, 2023, doi: 10.1021/acsaelm.3c00026. keywords: {RF sputtering Ta2O5 doping rectifying layer high accuracy neuromorphic computing RRAM}