daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

One-Pot, One-Step to Access Cyclic Amphiphilic Block Copoly(carbonate-b-ester) AITranslate

Nanjing Tech University; Nanjing Tech University; Nanjing Tech University; Nanjing Tech University;Institute of Nanjing Advanced Biomaterials and Processing Equipment; Nanjing Tech University; Nanjing Tech University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Amphiphilic block copolymers containing a cyclic topology exhibit distinct physical properties that can be exploited to obtain fascinating nanostructures for various applications. So far, these copolymers have been generally prepared via multistep approaches. Herein, we report the simultaneous zwitterionic copolymerization of δ-valerolactone (VL) and triethylene glycol carbonate (3EG) mediated by N-heterocyclic carbene to yield a cyclic amphiphilic block copoly(ester-b-carbonate) in a one-pot, one-step strategy. The copolymerization temperature has a considerable impact on the block length (LVL and L3EG); thus, a block copolymer (LVL = 12.7 and L3EG = 10.1) is obtained at a low temperature (−25 °C), whereas a random copolymer is obtained at 50 °C with a high overall conversion (≥95%). The copolymerization proceeds with a 150 times faster consumption of VL compared to that of 3EG with reactivity ratios (r) rVL ≫ r3EG (rVL ≈ 5, r3EG ≈ 0.055), determined using the error-in-variables-model method, demonstrating the VL block chain during copolymerization. Moreover, a theoretical study indicates that the obtained copolymer is not a kinetically controlled product but rather a thermodynamically controlled product. Scanning and transmission electron microscopies revealed that the copoly(ester-b-carbonate) self-assembled in a tetrahydrofuran/water solvent mixture (VTHF/VH2O = 1:5) to form a cubic nanostructure.

KeyWords AITranslate

Onestep copolymerization Amphiphilic copolymer Zwitterionic ringopening polymerization Selfassembly Copolyester
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c01795

Chinese Library Classification Number:

Citation Information:

Amphiphilic block copolymers containing a cyclic topology exhibit distinct physical properties that can be exploited to obtain fascinating nanostructures for various applications. So far, these copolymers have been generally prepared via multistep approaches. Herein, we report the simultaneous zwitterionic copolymerization of δ-valerolactone (VL) and triethylene glycol carbonate (3EG) mediated by N-heterocyclic carbene to yield a cyclic amphiphilic block copoly(ester-b-carbonate) in a one-pot, one-step strategy. The copolymerization temperature has a considerable impact on the block length (LVL and L3EG); thus, a block copolymer (LVL = 12.7 and L3EG = 10.1) is obtained at a low temperature (−25 °C), whereas a random copolymer is obtained at 50 °C with a high overall conversion (≥95%). The copolymerization proceeds with a 150 times faster consumption of VL compared to that of 3EG with reactivity ratios (r) rVL ≫ r3EG (rVL ≈ 5, r3EG ≈ 0.055), determined using the error-in-variables-model method, demonstrating the VL block chain during copolymerization. Moreover, a theoretical study indicates that the obtained copolymer is not a kinetically controlled product but rather a thermodynamically controlled product. Scanning and transmission electron microscopies revealed that the copoly(ester-b-carbonate) self-assembled in a tetrahydrofuran/water solvent mixture (VTHF/VH2O = 1:5) to form a cubic nanostructure.

quote

GB/T 7714-2015 [1] Na Shi, Longlin Lu, Fengzhen Guo, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c01795.
MLA [1] Na Shi, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c01795.
APA [1] Na Shi, Longlin Lu, Fengzhen Guo, Zhenjiang Li, Lei Shen, Jin Huang, & Kai Guo. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c01795
IEEE [1] Na Shi, Longlin Lu, Fengzhen Guo, Zhenjiang Li, Lei Shen, Jin Huang, and Kai Guo, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c01795. keywords: {Onestep copolymerization;Amphiphilic copolymer;Zwitterionic ringopening polymerization;Selfassembly;Copolyester}