Soft Gel-Filled Composite Adhesive for Dry and Wet Adhesion AITranslate

Indian Institute of Technology Kanpur; Indian Institute of Technology Kanpur; Indian Institute of Technology Kanpur
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

We have presented a two-phase adhesive for both dry and wet adhesion applications and for using it over repeated bonding and debonding cycles. We have dispersed a hydrogel phase in the continuous matrix of an elastomer, both cross-linked in situ almost simultaneously. Adhesion tests showed that although the individual phases were elastic and displayed negligible adhesion hysteresis, for the two-phase adhesive, hysteresis increased with the content of the dispersed phase in the material, eventually attaining maxima at an intermediate loading. Hysteresis also increased with the rate of separation of the adherents. Experiments showed that such enhancement in hysteresis could not be explained by considering the bulk viscoelastic effect of the two-phase material, as the two-phase composites too are essentially elastic, similar to the individual phases. Instead, intrinsic, rate-dependent, interfacial interactions born out of topographical and chemical heterogeneity of the adhesive surface could account for it. The adhesive could be used for both dry and wet conditions; in fact, adhesion was stronger on a wet adherent. It could also be used over 50 times without any alteration in adhesion. The adhesion mechanism is expected to be useful for a host of diverse applications.

KeyWords AITranslate

Pressuresensitive adhesives ratedependency JKR test interfacial friction wet adhesion
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c00286

Chinese Library Classification Number:

Citation Information:

We have presented a two-phase adhesive for both dry and wet adhesion applications and for using it over repeated bonding and debonding cycles. We have dispersed a hydrogel phase in the continuous matrix of an elastomer, both cross-linked in situ almost simultaneously. Adhesion tests showed that although the individual phases were elastic and displayed negligible adhesion hysteresis, for the two-phase adhesive, hysteresis increased with the content of the dispersed phase in the material, eventually attaining maxima at an intermediate loading. Hysteresis also increased with the rate of separation of the adherents. Experiments showed that such enhancement in hysteresis could not be explained by considering the bulk viscoelastic effect of the two-phase material, as the two-phase composites too are essentially elastic, similar to the individual phases. Instead, intrinsic, rate-dependent, interfacial interactions born out of topographical and chemical heterogeneity of the adhesive surface could account for it. The adhesive could be used for both dry and wet conditions; in fact, adhesion was stronger on a wet adherent. It could also be used over 50 times without any alteration in adhesion. The adhesion mechanism is expected to be useful for a host of diverse applications.

quote

GB/T 7714-2015 [1] Kuldeep Kuhar, Muhamed Jesbeer, Animangsu Ghatak. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.1c00286.
MLA [1] Kuldeep Kuhar, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.1c00286.
APA [1] Kuldeep Kuhar, Muhamed Jesbeer, & Animangsu Ghatak. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.1c00286
IEEE [1] Kuldeep Kuhar, Muhamed Jesbeer, and Animangsu Ghatak, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.1c00286. keywords: {Pressuresensitive adhesives;ratedependency;JKR test;interfacial friction;wet adhesion}