Quantitative Singlet Fission in Highly Stable Rubicene Skeleton: A Desirable Alternative to Acene Derivatives AITranslate

Taiyuan University of Technology; Taiyuan University of Technology; The Chinese University of Hong Kong; The Chinese University of Hong Kong; Taiyuan University of Technology; Taiyuan University of Technology; Capital Normal University; Institute of Chemistry
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Singlet fission (SF) processes hold great potential in boosting conversion efficiency of solar cells. However, practical applications were greatly hindered by the limited availability of suitable SF materials. Current studies mainly focus on acene derivatives, which are known to be subjected to knotty stability issues or low energy levels. Therefore, developing efficient and stable SF materials is a primary issue before the implementation of practical application. Herein, we present a new SF material based on a rubicene (Rc) skeleton as a desirable acene alternative. Spectroscopic and theoretical results highlight that Rc holds broad absorption, suitable triplet energy, efficient SF process, and excellent stability, which could be ascribed to the distinctive π-sextet resonance structures in the ground state and excited state featuring characteristic aromaticity. Our outcomes not only provide a robust SF system but also offer insights into modular aromaticity in polycyclic systems, which could be used to develop new optical function materials.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsmaterialslett.3c01016

Chinese Library Classification Number:

Citation Information:

Singlet fission (SF) processes hold great potential in boosting conversion efficiency of solar cells. However, practical applications were greatly hindered by the limited availability of suitable SF materials. Current studies mainly focus on acene derivatives, which are known to be subjected to knotty stability issues or low energy levels. Therefore, developing efficient and stable SF materials is a primary issue before the implementation of practical application. Herein, we present a new SF material based on a rubicene (Rc) skeleton as a desirable acene alternative. Spectroscopic and theoretical results highlight that Rc holds broad absorption, suitable triplet energy, efficient SF process, and excellent stability, which could be ascribed to the distinctive π-sextet resonance structures in the ground state and excited state featuring characteristic aromaticity. Our outcomes not only provide a robust SF system but also offer insights into modular aromaticity in polycyclic systems, which could be used to develop new optical function materials.

quote

GB/T 7714-2015 [1] Zuyuan Liu, Long Wang, Qianqian Deng, et al. ACS Materials Letters, 2023(5). DOI:10.1021/acsmaterialslett.3c01016.
MLA [1] Zuyuan Liu, et al., ACS Materials Letters, no. 5, 2023, https://doi.org/10.1021/acsmaterialslett.3c01016.
APA [1] Zuyuan Liu, Long Wang, Qianqian Deng, Jun Zhu, Jing Sun, Hua Wang, Hongbing Fu, & Jiannian Yao. (2023). ACS Materials Letters(5). https://doi.org/10.1021/acsmaterialslett.3c01016
IEEE [1] Zuyuan Liu, Long Wang, Qianqian Deng, Jun Zhu, Jing Sun, Hua Wang, Hongbing Fu, and Jiannian Yao, ACS Materials Letters, no. 5, 2023, doi: 10.1021/acsmaterialslett.3c01016.