The presence of perfluorooctanoic acid, a perfluoralkyl substance, in water sources has raised health concerns due to its toxicity. Finding effective adsorbents is essential to ensure healthy sources of water for consumption. In this study, a heptazine-based polymer network (Py-HPOP) was synthesized using a one-pot nucleophilic substitution of 2,5,8-trichloro-s-heptazine (TCH) with 4,4′,4″,4‴-(pyrene-1,3,6,8-tetrayl) tetraaniline (Py-TA). For comparison, a triazine-based polymeric network (Py-TPOP) was also prepared using 2,4,6-trichloro-1,3,5-triazine under similar conditions. Both polymers were used to treat aqueous solutions containing 1 mg/L PFOA. Py-TPOP exhibited superior adsorption capacity (98.4% PFOA removal) relative to Py-HPOP (80.8% PFOA removal) despite Py-HPOP’s higher Brunauer–Emmett–Teller (BET) surface area SBET at 205 m2 g–1. The effect of electrostatic interactions was also observed as a critical factor for PFOA adsorption as demonstrated by the change in PFOA adsorption by both polymers under basic, neutral, and acidic conditions. This investigation illustrates a facile synthesis of amorphous covalent frameworks as strong, competitive adsorbents for PFOA removal from water.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.2c01580
Chinese Library Classification Number:
Citation Information:
The presence of perfluorooctanoic acid, a perfluoralkyl substance, in water sources has raised health concerns due to its toxicity. Finding effective adsorbents is essential to ensure healthy sources of water for consumption. In this study, a heptazine-based polymer network (Py-HPOP) was synthesized using a one-pot nucleophilic substitution of 2,5,8-trichloro-s-heptazine (TCH) with 4,4′,4″,4‴-(pyrene-1,3,6,8-tetrayl) tetraaniline (Py-TA). For comparison, a triazine-based polymeric network (Py-TPOP) was also prepared using 2,4,6-trichloro-1,3,5-triazine under similar conditions. Both polymers were used to treat aqueous solutions containing 1 mg/L PFOA. Py-TPOP exhibited superior adsorption capacity (98.4% PFOA removal) relative to Py-HPOP (80.8% PFOA removal) despite Py-HPOP’s higher Brunauer–Emmett–Teller (BET) surface area SBET at 205 m2 g–1. The effect of electrostatic interactions was also observed as a critical factor for PFOA adsorption as demonstrated by the change in PFOA adsorption by both polymers under basic, neutral, and acidic conditions. This investigation illustrates a facile synthesis of amorphous covalent frameworks as strong, competitive adsorbents for PFOA removal from water.
quote
| GB/T 7714-2015 | [1] Dana Abdullatif, Ahmadreza Khosropour, Anahita Khojastegi, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.2c01580. |
| MLA | [1] Dana Abdullatif, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.2c01580. |
| APA | [1] Dana Abdullatif, Ahmadreza Khosropour, Anahita Khojastegi, Imann Mosleh, Leila Khazdooz, Amin Zarei, & Alireza Abbaspourrad. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.2c01580 |
| IEEE | [1] Dana Abdullatif, Ahmadreza Khosropour, Anahita Khojastegi, Imann Mosleh, Leila Khazdooz, Amin Zarei, and Alireza Abbaspourrad, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.2c01580. keywords: {perfluoroalkyl substance;perfluorooctanoic acid;triazine;heptazine;porous organic polymer} |