Active Deformable and Flexible Triboelectric Nanogenerator Based on Super-Light Clay AITranslate

Guangxi University; Guangxi University; Beijing Institute of Nanoenergy and Nanosystems; University of Chinese Academy of Sciences; University of Chinese Academy of Sciences
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Triboelectric nanogenerators (TENGs) are demonstrated to possess great superiority in the field of low-frequency and high-entropy energy harvesting. Here, a kind of friction material, super-light clay (SLC), with outstanding stretchability and shape/size changeability is introduced to develop contact-separation triboelectric nanogenerators (SLC-TENGs), which exhibit outstanding flexible, shape-changeable, and adaptable properties but simple preparation processes. A high and stable electrical output can be achieved from the simple-structured SLC-TENG. The peak power density of the SLC-TENG output reaches up to 0.33 W/m2 under an effective contact with an area of 9 cm2 and an external load resistance of 50 MΩ. In addition, a balloon-structured TENG was also prepared with the filling of several SLC balls. The electrical signals can be generated even just by a slight shaking, revealing great application potential in the Internet of Things systems and self-powered sensors by energy harvesting from wind, ocean, human body movements, etc.

KeyWords AITranslate

active deformable and flexible superlight clay balloonstructure energy harvesting triboelectric nanogenerators
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.2c00985

Chinese Library Classification Number:

Citation Information:

Triboelectric nanogenerators (TENGs) are demonstrated to possess great superiority in the field of low-frequency and high-entropy energy harvesting. Here, a kind of friction material, super-light clay (SLC), with outstanding stretchability and shape/size changeability is introduced to develop contact-separation triboelectric nanogenerators (SLC-TENGs), which exhibit outstanding flexible, shape-changeable, and adaptable properties but simple preparation processes. A high and stable electrical output can be achieved from the simple-structured SLC-TENG. The peak power density of the SLC-TENG output reaches up to 0.33 W/m2 under an effective contact with an area of 9 cm2 and an external load resistance of 50 MΩ. In addition, a balloon-structured TENG was also prepared with the filling of several SLC balls. The electrical signals can be generated even just by a slight shaking, revealing great application potential in the Internet of Things systems and self-powered sensors by energy harvesting from wind, ocean, human body movements, etc.

quote

GB/T 7714-2015 [1] Kaixuan Wang, Yueming Zhang, Xiongxin Luo, et al. ACS Applied Electronic Materials, 2022(4). DOI:10.1021/acsaelm.2c00985.
MLA [1] Kaixuan Wang, et al., ACS Applied Electronic Materials, no. 4, 2022, https://doi.org/10.1021/acsaelm.2c00985.
APA [1] Kaixuan Wang, Yueming Zhang, Xiongxin Luo, Laipan Zhu, & Zhong Lin Wang. (2022). ACS Applied Electronic Materials(4). https://doi.org/10.1021/acsaelm.2c00985
IEEE [1] Kaixuan Wang, Yueming Zhang, Xiongxin Luo, Laipan Zhu, and Zhong Lin Wang, ACS Applied Electronic Materials, no. 4, 2022, doi: 10.1021/acsaelm.2c00985. keywords: {active deformable and flexible superlight clay balloonstructure energy harvesting triboelectric nanogenerators}