Application and Prospect of Hydrogen Making by Natural Gas Reformation in Large-scale P/M Enterprises AITranslate
Abstract AITranslate
The paper describes the principles and process flowsheet of hydrolytic and electrolytic hydrogen making and hydrogen making by natural gas reformation. The results of comparison and technical analysis show that the latter is much more superior in respect of production and it is successfully applied in the P/ M enterprises. The process can take the place of hydrolytic and electrolytic hydrogen making in large P/M plants.
KeyWords AITranslate
1王廉舫.水电解制氢氧[M].长沙:湖南省工业气体专业委员会,1996..
2杨 R T[美].吸附法气体分离[M].王树森,等译.北京:化学工业出版社,1991.
1李艳,刘艳伟,杨滨.氢源廉价制备技术综述[J].郑州轻工业学院学报:自然科学版,2008,23(1):79-82. 被引量:2
2匡社颖.粉末冶金企业氢气系统设计的经济性及安全性分析[J].低温与特气,2010,28(3):17-22. 被引量:2
3匡社颖.吸附法氢气回收净化工艺在钨钼还原系统中的应用[J].稀有金属与硬质合金,2010,38(3):50-53. 被引量:1
4张云洁,李金英.天然气制氢工艺现状及发展[J].广州化工,2012,40(13):41-42. 被引量:10
5朱宇.天然气制氢工艺现状及发展[J].化学工程与装备,2016(7):213-214. 被引量:4
6周学虎.天然气制氢技术研究进展[J].中国石油和化工标准与质量,2015,35(23):42-44.
1杨晓阳,杨昌乐.制氢方法及氢气中微量杂质的测定[J].现代科学仪器,2011,28(6):151-153. 被引量:2
2王芳,刘光明,解东来.移动氢源用铝水反应制氢技术研究[J].电源技术,2012,36(2):198-200. 被引量:4
3林宇霖,陈同云,黄宪法,桂林,赵静霞.两段碳还原MoO_3反应产物的成分研究[J].稀有金属与硬质合金,2013,41(1):28-31. 被引量:2
4陈为强,丁彤,马智,谢洪燕.钡离子对镍基钙钛矿分解氨的影响[J].化工进展,2015,34(10):3676-3679. 被引量:2
5刘红梅,徐向亚,冯静,张明森,姜健准.Ni/Al_2O_3催化剂上甲烷自热重整制合成气反应[J].石油化工,2016,45(2):149-155. 被引量:5
6高振,侯建国,王秀林,宋鹏飞.焦炉尾气耦合生物沼气制取天然气的工艺集成研究[J].化学工程,2016,44(11):74-78. 被引量:1
7谢欣烁,杨卫娟,施伟,张圣胜,王智化,周俊虎.制氢技术的生命周期评价研究进展[J].化工进展,2018,37(6):2147-2158. 被引量:41
8薛琳,刘红梅,刘东兵,张明森.镍催化剂的结构特征及其催化甲烷二氧化碳重整反应[J].石油化工,2018,47(10):36-43. 被引量:2
9厉勇,张英,王元华.甲烷水蒸气重整技术研究现状及进展[J].炼油技术与工程,2019,49(7):1-7. 被引量:7
10顾炳波.提高甲醇合成气中有效气体利用率的探讨[J].化工管理,2014(23):18-18. 被引量:1
1匡社颖.天然气重整制氢工艺在大型粉末冶金企业的应用前景[J].工程设计与研究(长沙),2005(1):24-26.
2许玉琴,谢晓峰,王兆海,王要武,毛宗强,王树博.固定式质子交换膜燃料电池的天然气重整制氢[J].化工学报,2004,55(S1):26-33. 被引量:4
3王业勤,沈静,叶帆.小规模制氢方法的选择[J].工厂动力,2004(2):35-39. 被引量:1
4张二涛,解东来.天然气重整制氢新技术的研究进展[J].应用化工,2012,41(6):1067-1071. 被引量:6
5姚良琮,李玉富,赵丹.用变换气代替脱碳气作氢源的加氢脱硫研究[J].天然气化工—C1化学与化工,2012,37(3):30-33.
6匡社颖.粉末冶金企业氢气系统设计的经济性及安全性分析[J].低温与特气,2010,28(3):17-22. 被引量:2
7龚娟,苏庆泉,米万良,李志远,徐立昊.入口气体组成对天然气重整工作温度的影响[J].化工学报,2008,59(3):687-693. 被引量:3
8秦金国,张云华.水电解制氢工艺的节能分析[J].江西能源,2001,17(3):23-25. 被引量:2
9可降低天然气重整成本的铂浸渍催化剂[J].现代化工,2009(3):92-92.
10钱伯章.Gas2公司实施下一代GTL试验计划[J].石油炼制与化工,2013,44(10):37-37.
Basic Information:
DOI:
Chinese Library Classification Number:TQ116.25[化学工程—无机化工]
Citation Information:
The paper describes the principles and process flowsheet of hydrolytic and electrolytic hydrogen making and hydrogen making by natural gas reformation. The results of comparison and technical analysis show that the latter is much more superior in respect of production and it is successfully applied in the P/ M enterprises. The process can take the place of hydrolytic and electrolytic hydrogen making in large P/M plants.
quote
| GB/T 7714-2015 | [1] KUANG She-ying. Application and Prospect of Hydrogen Making by Natural Gas Reformation in Large-scale P/M Enterprises[J]. Rare Metals and Cemented Carbides, 2006(2): 58-60. |
| MLA | [1] KUANG She-ying. "Application and Prospect of Hydrogen Making by Natural Gas Reformation in Large-scale P/M Enterprises." Rare Metals and Cemented Carbides, no. 2, 2006, pp. 58-60. |
| APA | [1] KUANG She-ying. (2006). Application and Prospect of Hydrogen Making by Natural Gas Reformation in Large-scale P/M Enterprises. Rare Metals and Cemented Carbides(2), 58-60. |
| IEEE | [1] KUANG She-ying, "Application and Prospect of Hydrogen Making by Natural Gas Reformation in Large-scale P/M Enterprises," Rare Metals and Cemented Carbides, no. 2, pp. 58-60, 2006. keywords: {P/M;hydrogen making process;hydrogen making by natural gas reformation;hydrolytic and electrolytic hydrogen making;economic index .} |