In this study,composite solid-state electrolytes(CSEs)were fabricated by incorporating 20%,50%,and 80% of Li1.3Al0.3Ti1.7(PO4)3solid electrolyte powder into a poly(ethylene oxide)(PEO)-based solid polymer electrolyte(SPE)matrix via a solution casting method.The microstructural characteristics,ionic conductivity,Young’s modulus,and interfacial electrochemical stability with lithium metal anodes of the LATP/SPE composite electrolytes were systematically investigated.Experimental results demonstrated that the CSE containing 50%LATP exhibited optimal electrochemical performance,achieving stable cycling for 1600 h at a current density of 0.5 mA/cm2.This performance significantly surpassed that of composites with 0,20%,and 80%LATP additions.Furthermore,the interfacial failure mechanisms between lithium metal and CSEs with varying LATP contents were thoroughly elucidated.
KeyWords AITranslate
Basic Information:
DOI:
Chinese Library Classification Number:TM912[电气工程—电力电子与电力传动];TB332[一般工业技术—材料科学与工程]
Citation Information:
In this study,composite solid-state electrolytes(CSEs)were fabricated by incorporating 20%,50%,and 80% of Li1.3Al0.3Ti1.7(PO4)3solid electrolyte powder into a poly(ethylene oxide)(PEO)-based solid polymer electrolyte(SPE)matrix via a solution casting method.The microstructural characteristics,ionic conductivity,Young’s modulus,and interfacial electrochemical stability with lithium metal anodes of the LATP/SPE composite electrolytes were systematically investigated.Experimental results demonstrated that the CSE containing 50%LATP exhibited optimal electrochemical performance,achieving stable cycling for 1600 h at a current density of 0.5 mA/cm2.This performance significantly surpassed that of composites with 0,20%,and 80%LATP additions.Furthermore,the interfacial failure mechanisms between lithium metal and CSEs with varying LATP contents were thoroughly elucidated.
quote
| GB/T 7714-2015 | [1] SU Qiong, ZHONG Shengwen. Study on the interface stability between LATP/SPE composite solid electrolytes with different ratios and lithium metal[J]. Nonferrous Metals Science and Engineering, 2026(2): 245-257. |
| MLA | [1] SU Qiong, and ZHONG Shengwen. "Study on the interface stability between LATP/SPE composite solid electrolytes with different ratios and lithium metal." Nonferrous Metals Science and Engineering, no. 2, 2026, pp. 245-257. |
| APA | [1] SU Qiong, & ZHONG Shengwen. (2026). Study on the interface stability between LATP/SPE composite solid electrolytes with different ratios and lithium metal. Nonferrous Metals Science and Engineering(2), 245-257. |
| IEEE | [1] SU Qiong and ZHONG Shengwen, "Study on the interface stability between LATP/SPE composite solid electrolytes with different ratios and lithium metal," Nonferrous Metals Science and Engineering, no. 2, pp. 245-257, 2026. keywords: {polymer electrolyte;LATP solid electrolyte;organic-inorganic composite solid electrolyte;lithium metal;cyclic stability} |