Determination of Chlorine in Ta/Nb Composite AITranslate
Abstract AITranslate
Analysis is made of the determination of chlorine in tantalum-niobium composite. Chlorine in tan- talum-niobium composite is determined through heating and distillati'on with high-temperature tubular fur- nace and silver chloride turbidimetry. The results showed that 89.10%-92.5% recovery (with standard specimen) was achieved at relative deviation 6.75% by the said method.
KeyWords AITranslate
1陈晓青,胡雪松,付涛.氯化石蜡中氯含量测定方法的改进[J].分析化学,1996,24(7):867-867. 被引量:4
2高甲友,咸爱红.流动注射—吸光光度法测定自来水中余氯[J].理化检验:化学分册,1997,33(5):220-220. 被引量:4
3陈汝珍 张俊峰 于红燕 等.离子色谱法测定钽铌氧化物中的氯离子.钽铌工业进展,2004,(3):26-27.
1夏明星,郑欣,李中奎,王东辉,王峰.电容器用钽铌粉的研究进展[J].材料导报:纳米与新材料专辑,2009,23(2):109-111. 被引量:8
2韦文业.氯离子选择性电极直接测定锌铟电解液中氯离子含量[J].冶金分析,2011,31(8):65-68. 被引量:14
3巫来富.氯化银浊度法测定铜电解液中氯离子[J].嘉应学院学报,2012,30(8):52-55. 被引量:2
4鲁青庆,向德磊.自动电位滴定法测定铅锌混合矿中的氯[J].中国无机分析化学,2013,3(B10):22-25. 被引量:1
1王东新,李军义,孙本双,任晓,何季麟.钽粉制备新工艺研究进展[J].湖南有色金属,2011,27(3):34-37. 被引量:19
2王珊,魏姜勉,高向阳.浓度直读法快速测定酱菜中的氯离子[J].食品科学,2012,33(12):264-267. 被引量:1
3王亚健,张利波,彭金辉,孙成余,巨少华,张旭.火焰原子吸收光谱法间接测定氧化锌烟尘中氯[J].冶金分析,2013,33(7):41-44. 被引量:3
4袁齐.氢氧化钠熔融-氯化银比浊法测定铅锌矿中氯[J].冶金分析,2014,34(1):79-81. 被引量:10
5杨国启,何季麟,郑爱国,罗文,周小军,李军义.电容器级高比容钽粉制备工艺研究进展[J].湖南有色金属,2014,30(1):48-52. 被引量:17
6张积锴,张旭,沈庆峰,胡安生,孙敬会,张云彭.自动电位滴定法间接测定除氯铜渣中氯[J].冶金分析,2014,34(12):78-82. 被引量:6
7王婷香.硝酸银电位滴定法测定高纯二氧化锗中氯[J].冶金分析,2015,35(5):74-76. 被引量:4
8闻向东,谭谦,邵梅,张穗忠.超声溶解-电位滴定法测定硅钢涂层用纳米二氧化钛中氯[J].冶金分析,2015,35(6):78-82. 被引量:1
9孙钟雷,许艺,李宇.多电极复合法快速测定榨菜食盐含量[J].食品科学,2015,36(24):164-167. 被引量:3
10钱庆长,史静,周颖,余晶晶,徐庆红.硝酸银自动电位滴定法测定铜电解液中氯离子时稳定剂的影响[J].冶金分析,2016,36(3):35-38. 被引量:5
1张家相,邓雯锦,喻娟,王陆琼,何吉兰.红外碳硫仪测定煤中全硫技术研究[J].冶金标准化与质量,2011(1):33-35.
2奚奇辉,孙军,裘翼舟,张萌萌.气相色谱法测定氯化胆碱中1,4-二氧杂环己烷[J].饲料与畜牧:新饲料,2010(10):37-38.
3谢晓峰,贾桂玲,张剑平,方建慧,施利毅.纳米SiO_2/TiO_(2-x)N_x复合粒子的制备与表征[J].太阳能学报,2006,27(1):14-18. 被引量:1
4魏红兵,王虹,李异.管式电阻炉加热红外吸收法测定红土镍矿中硫[J].冶金分析,2008,28(11):65-67. 被引量:9
5窦光宇.磷:奇异的元素[J].百科知识,2007(10S):17-18.
6王茹,刘敏.热分解一气体容量法测定岩石矿物中CO_2的最佳分析方案的选择[J].当代化工,2016,45(1):203-204.
7李辉,韩奎华,刘洪涛,路春美.铁基添加剂调质石灰石用于O_2/CO_2燃煤脱硫的实验研究[J].锅炉技术,2013,44(1):76-80. 被引量:2
8李新义,司崇殿,陈万东.高纯无水氯化镁的制备及制镁工艺[J].化学工业与工程,2011,28(5):37-40. 被引量:2
9周志彬,黄开勋,陈泽宪,徐辉碧.聚[1,3-双(对羧基苯氧基)丙烷-癸二酸]的改进合成[J].华中理工大学学报,2000,28(9):101-103.
10陶骏骏,陈帅,姚奉奇,王海晖.植物焦炭氧化中的平行反应及其动力学解析[J].化学学报,2016,74(1):81-88. 被引量:2
Basic Information:
DOI:
Chinese Library Classification Number:O614.51[理学—无机化学]
Citation Information:
Analysis is made of the determination of chlorine in tantalum-niobium composite. Chlorine in tan- talum-niobium composite is determined through heating and distillati'on with high-temperature tubular fur- nace and silver chloride turbidimetry. The results showed that 89.10%-92.5% recovery (with standard specimen) was achieved at relative deviation 6.75% by the said method.
quote
| GB/T 7714-2015 | [1] YU Hong-yan, JIANG Ning-fen. Determination of Chlorine in Ta/Nb Composite[J]. Rare Metals and Cemented Carbides, 2007(4): 39-41. |
| MLA | [1] YU Hong-yan, and JIANG Ning-fen. "Determination of Chlorine in Ta/Nb Composite." Rare Metals and Cemented Carbides, no. 4, 2007, pp. 39-41. |
| APA | [1] YU Hong-yan, & JIANG Ning-fen. (2007). Determination of Chlorine in Ta/Nb Composite. Rare Metals and Cemented Carbides(4), 39-41. |
| IEEE | [1] YU Hong-yan and JIANG Ning-fen, "Determination of Chlorine in Ta/Nb Composite," Rare Metals and Cemented Carbides, no. 4, pp. 39-41, 2007. keywords: {tantalum-niobium composite;chlorine content;high-temperature tubular furnace, silver nitrate;turbidimetry} |