The Present Application of Rare Earth Yttrium AITranslate

School of Materials Science and Engineering, Henan University of Science and Technology;School of Materials Science and Engineering, Henan University of Science and Technology;School of Materials Science and Engineering, Henan University of Science and Technology;School of Materials Science and Engineering, Henan University of Science and Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The applications of Y in related industry are introduced.And the comments are made for reference on the further extension of applications of rare earth Y in the field of infrastructure industry,environmental protection and high-tech industry.

KeyWords AITranslate

rare earth element yttrium characteristic application

1何梅,刘媛媛,时光辉,曹雅珊,李长起,汪承润.稀土钇离子溶液对蚕豆根尖细胞的遗传毒性[J].淮南师范学院学报,2006,8(3):37-38. 被引量:3

2徐广尧.稀土在传统产业中的应用[J].稀土,1999,20(3):65-70. 被引量:14

3郭伯生.稀土在生物领域中应用研究进展[J].稀土,1999,20(1):64-68. 被引量:117

4范才河,陈刚,严红革,陈振华.稀土在镁及镁合金中的作用[J].材料导报,2005,19(7):61-63. 被引量:62

5蔡明昌,王慧,税安泽,曾令可.稀土在汽车尾气净化催化剂中的应用现状[J].稀有金属快报,2006,25(3):13-17. 被引量:14

6王海滨,刘军,张迎,冯伟宏.稀土应用的概况和今后开发重点的建议[J].山东化工,1999,28(4):30-34. 被引量:2

7李兵.稀土元素发现史话[J].金属世界,2006(1):48-49. 被引量:2

8郭旭涛,李培杰,曾大本.Mg-Y合金的电子理论研究[J].中国稀土学报,2003,21(6):672-676. 被引量:11

9吴国华,李冠群,樊昱,丁文江,朱燕萍,李波,王群.Y对AZ91D镁合金组织及力学性能的影响[J].特种铸造及有色合金,2006,26(5):260-263. 被引量:25

10肖艳.谈稀有金属及其应用[J].金属世界,2006(2):45-47. 被引量:1

1于兵,黄海涛,张全军,闫奇操,康佳,刘玉宝.熔盐电解法制备Y-Ni合金的研究[J].稀土,2021(1):81-86.

2刘中兴,韩文帅,伍永福,胡永胜,鞠阳.60kA底部阴极稀土电解槽电场数值模拟[J].稀有金属与硬质合金,2015,43(1):26-28. 被引量:4

3鲁道荣,王靓靓.钇对Zn-Fe合金镀层耐蚀性的影响[J].中国稀土学报,2009,27(2):267-271. 被引量:3

4帕提曼.尼扎木丁,阿布力孜.伊米提,米日古丽.莫合买提,王吉德.钇掺杂对磷酸亚铁锂薄膜光波导传感元件气敏特性的影响[J].分析化学,2011,39(12):1871-1876. 被引量:6

5叶红勇,左广玲,李入林,谢英男.Y_2O_3/Ag_3VO_4复合可见光催化剂的制备及其光催化性能[J].中国稀土学报,2012,30(1):28-33. 被引量:7

6聂海棋,梁铎强.稀土金属钇的开发[J].四川冶金,2013,35(1):75-78. 被引量:5

7王彬.浅谈稀土元素的应用[J].内蒙古科技与经济,2013(12):116-116. 被引量:4

8曹小华,陶春元,谢宝华.Y_2P_2W_(18)O_(62)·nH_2O/MWCNTs催化剂的制备及其催化合成乙酸正丁酯[J].石油化工,2016,45(2):200-205. 被引量:2

9杨东艳,陈雨来,李静媛.稀土Y对MP35N合金组织和性能的影响[J].塑性工程学报,2016,23(5):131-138. 被引量:1

10陈沾,朱雷,汪恂.钇掺杂纳米氧化锌的光催化性能[J].环境工程学报,2016,10(11):6290-6294. 被引量:5

1于兵,黄海涛,张全军,闫奇操,康佳,刘玉宝.熔盐电解法制备Y-Ni合金的研究[J].稀土,2021(1):81-86.

2谢建昌,李全安,李建弘,李克杰.稀土钇及其应用现状[J].稀有金属与硬质合金,2008,36(1):56-58. 被引量:18

3汪燕鸣,王飞,王跃.稀土元素农业应用的研究进展[J].化工时刊,2007,21(2):47-49. 被引量:24

4龚晓钟,汤皎宁,张晓萃.单一稀土镧在不同基底上的电沉积及其性能的研究[J].广州化学,2008,33(3):1-7. 被引量:1

5任晓晓,周青.稀土元素对植物矿质代谢的影响与机理[J].土壤通报,2009,40(2):451-455. 被引量:3

6陈晓刚,陈纯馨,陈忻,叶秀文.稀土-羧甲基壳聚糖复合物对印染废水脱色机理研究[J].环境科学与技术,2010,33(S2):263-267. 被引量:3

7王瑛,李文德.浅谈稀土元素的应用及生物学效应机制[J].西藏科技,2010(4):23-24. 被引量:2

8帕提曼.尼扎木丁,阿布力孜.伊米提,米日古丽.依明,帕提曼.亚森,艾拜都拉.热合曼,司马义.努尔拉.热处理对LiFe_(1-0.01x)Y_(0.005x)Ag_(0.005x)PO_4薄膜光波导传感元件气敏性的影响[J].中国稀土学报,2012,30(3):343-349. 被引量:1

9韩登峰,鲁道荣.Ce^(3+)对Zn-Ni合金镀层耐蚀性能的影响[J].表面技术,2012,41(4):19-22. 被引量:4

10艾拜拉·热合曼,阿斯娅·克里木,帕提曼·亚森,帕提曼·尼扎木丁,阿达来提·阿不都热合曼,阿布力孜·伊米提.MB-硬脂酸复合薄膜光波导传感器检测氯化氢气体[J].高等学校化学学报,2012,33(10):2173-2177. 被引量:5

1蔡晶.横梁移动式数控龙门机床的技术优势[J].金属加工:冷加工,2016,0(12):31-33.

2黄蓉.机械加工工艺对金属零件加工精度的影响研究[J].世界有色金属,2016,0(12):147-148. 被引量:5

3张文学.超高速磨削技术在机械制造领域中的应用研究[J].企业技术开发:下旬刊,2014,33(2):40-40. 被引量:3

4庞增涛,张强.五轴龙门机床转动轴的误差检测方法探究[J].科技风,2017(4):94-94.

5王晓琴.机电一体化技术在工程机械上的应用与发展[J].机械管理开发,2017,32(3):162-163. 被引量:12

6磨料磨具技术创新在机械加工中的意义[J].磨料磨具通讯,2010(6):23-24.

7郭树伟.高端锻件出自高端装备[J].金属加工:热加工,2012(1):24-24.

8中铝山东企业铸造技术填补国家空白[J].铸造技术,2011,32(7):922-922.

9李晓,井溢农.包钢φ180机组市场竞争力分析与对策[J].包钢科技,2000,26(1):59-61.

10平越芳.CAD技术在模具设计中的应用[J].中国集体经济,2010,0(3S):179-179. 被引量:1

Basic Information:

DOI:

Chinese Library Classification Number:TG146.452[金属学及工艺—金属材料]

Citation Information:

The applications of Y in related industry are introduced.And the comments are made for reference on the further extension of applications of rare earth Y in the field of infrastructure industry,environmental protection and high-tech industry.

quote

GB/T 7714-2015 [1] XIE Jian-chang, LI Quan-an, LI Jian-hong, et al. The Present Application of Rare Earth Yttrium[J]. Rare Metals and Cemented Carbides, 2008(1): 56-58.
MLA [1] XIE Jian-chang, et al., "The Present Application of Rare Earth Yttrium." Rare Metals and Cemented Carbides, no. 1, 2008, pp. 56-58.
APA [1] XIE Jian-chang, LI Quan-an, LI Jian-hong, & LI Ke-jie. (2008). The Present Application of Rare Earth Yttrium. Rare Metals and Cemented Carbides(1), 56-58.
IEEE [1] XIE Jian-chang, LI Quan-an, LI Jian-hong, and LI Ke-jie, "The Present Application of Rare Earth Yttrium," Rare Metals and Cemented Carbides, no. 1, pp. 56-58, 2008. keywords: {rare earth element;yttrium;characteristic;application}