Microstructure and Properties of In-Situ Generated WC-Reinforced Ni60 Gradient Coating by Laser Cladding on H13 Steel AITranslate

School of Mechanical Engineering and Automation,Liaoning University of Technology;School of Mechanical Engineering and Automation,Liaoning University of Technology;School of Mechanical Engineering and Automation,Liaoning University of Technology;School of Mechanical Engineering and Automation,Liaoning University of Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The WC-reinforced Ni60 gradient coating was generated on the surface of H13 steel by laser cladding.The microstructure,phase composition,microhardness and friction&wear properties of the coating were analyzed by metallographic microscope,scanning electron microscope,X-ray diffractometer,microhardness tester and universal friction&wear tester.The results indicate that there are relatively few pores and cracks in WC-reinforced Ni60 gradient coating.The coating and the substrate form a good metallurgical bond.The phases of gradient coating surface are mainly iron-carbon compound(FexC),iron-nickel solid solution((Fe,Ni)23C6,Ni4B3)and ceramic-reinforced phases such as WC,W2C and Cr7C3.The hardness and wear resistance of the die steel surface are significantly improved by the gradient coating.The maximum microhardness of the coating surface is about 4 times of the substrate,and its wear amount is only about 18%of the substrate.The wear mechanism of the coating mainly includes adhesive wear,brittle spalling and abrasive wear,which can prolong the service life of the die and reduce the waste of resources.

KeyWords AITranslate

gradient coating laser cladding in-situ generation Ni60 WC microhardness wear mechanism

1GUAN Hong,LUO Aihui.Development and application of a new hot-work die steel for hot stamping[J].宝钢技术研究:英文版,2017,11(2):11-17. 被引量:5

2李绍宏,何文超,张旭,李东辉,肖茂果.H13型热作模具钢表面改性技术研究进展[J].钢铁,2021,56(3):13-22. 被引量:20

3时晓宇,温道胜,王守仁,王高琦,张明远.激光熔覆灰铸铁制动盘Fe-Ni-Cr梯度复合涂层微观组织及高温摩擦磨损性能研究[J].中国激光,2022,49(2):182-193. 被引量:7

4喻杰,夏如艇,吴建波,胡旭东.7CrSiMnMoV钢表面激光熔覆Ni/WC性能研究[J].热加工工艺,2015,44(20):98-100. 被引量:3

5崔雪,张松,张春华,吴臣亮,王强,董世运.高性能梯度功能材料激光增材制造研究现状及展望[J].材料工程,2020,48(9):13-23. 被引量:11

6马涛,赵忠民,刘良祥,高超,黄雪刚.功能梯度材料的研究进展及应用前景[J].化工科技,2012,20(1):71-75. 被引量:42

7Jie Xiong,Jian-cheng Fan,Jv Yuan.The Application and the Prospect of Remanufacturing Technologies in the Metallurgical Industry[J].工程管理前沿:英文版,2016,0(2):165-170. 被引量:4

8李晓峰,张泉,谢会起,冯英豪,杨晓辉.激光熔覆梯度高熵合金涂层组织与性能研究[J].中南大学学报:自然科学版,2021,52(11):3835-3842. 被引量:4

9张鸿羽,余敏,华俊伟,陈辉.Mo元素对Fe-Cr-Mo激光熔覆层组织及性能的影响[J].中国激光,2021,48(22):92-104. 被引量:3

1周梁栋,张亮,吴文恒,汪良,李翔,邹定锦.添加WC颗粒对钴基合金激光熔覆层组织形貌和显微硬度的影响研究[J].表面工程与再制造,2023,23(3):17-23.

2李金华,王应啸,姚芳萍.VC含量对原位生成WC增强Ni基涂层组织及性能的影响[J].制造技术与机床,2023(9):189-195.

1逄显娟,岳世伟,黄素玲,谢金梦,王帅,宋晨飞,岳赟,刘建,李栋.碳纤维/聚醚醚酮(CF/PEEK)复合材料摩擦磨损性能及抗摩擦静电特性研究[J].中国机械工程,2023,34(3):277-286. 被引量:2

2侯波.采煤机导向滑靴磨损检测装置设计与应用研究[J].矿业装备,2023(1):198-200.

3舒雷,张正文,刘丽君,毛胜兰.粉末床激光熔化成形H13钢工艺优化及力学性能研究[J].机械科学与技术,2022,41(12):1914-1920.

4徐乙人,祝天一,李永健,王长亮,马婷,胡广阳,王玉明.钴基合金刷丝与碳化铬涂层高线速度磨损行为研究[J].摩擦学学报,2022,42(6):1216-1225. 被引量:1

5张宇鹏,王永东,常萌阳,王金宇.MoS_(2)添加量对MoS_(2)/Ni60A固体自润滑涂层显微组织和性能的影响[J].机械工程材料,2022,46(12):24-29.

6徐国旺.表面处理对活塞环摩擦磨损性能影响的试验研究[J].今日自动化,2022(11):42-45.

7王成,王伟,丁士杰,宫鹏辉,高原.激光熔覆铁基耐磨涂层的制备及摩擦学性能研究[J].中国激光,2022,49(22):131-141. 被引量:1

8陈铅城.锅炉汽包裂纹缺陷产生原因分析[J].化学工程与装备,2022(11):226-228.

9欧阳伟豪,周健,高鹏,迟宏宵,谢官利,王文军.铌含量对H13钢枝晶偏析及碳化物组成和形貌的影响[J].机械工程材料,2022,46(12):43-49.

10高维刚,杜鹏,俞中围,凌青飞.低压输送泵异声故障分析[J].设备管理与维修,2023(3):52-54.

Basic Information:

DOI:

Chinese Library Classification Number:TG174.4[金属学及工艺—金属表面处理]

Citation Information:

The WC-reinforced Ni60 gradient coating was generated on the surface of H13 steel by laser cladding.The microstructure,phase composition,microhardness and friction&wear properties of the coating were analyzed by metallographic microscope,scanning electron microscope,X-ray diffractometer,microhardness tester and universal friction&wear tester.The results indicate that there are relatively few pores and cracks in WC-reinforced Ni60 gradient coating.The coating and the substrate form a good metallurgical bond.The phases of gradient coating surface are mainly iron-carbon compound(FexC),iron-nickel solid solution((Fe,Ni)23C6,Ni4B3)and ceramic-reinforced phases such as WC,W2C and Cr7C3.The hardness and wear resistance of the die steel surface are significantly improved by the gradient coating.The maximum microhardness of the coating surface is about 4 times of the substrate,and its wear amount is only about 18%of the substrate.The wear mechanism of the coating mainly includes adhesive wear,brittle spalling and abrasive wear,which can prolong the service life of the die and reduce the waste of resources.

quote

GB/T 7714-2015 [1] XUE Sheng-li, LI Jin-hua, YAO Fang-ping, et al. Microstructure and Properties of In-Situ Generated WC-Reinforced Ni60 Gradient Coating by Laser Cladding on H13 Steel[J]. Rare Metals and Cemented Carbides, 2022(6): 41-45.
MLA [1] XUE Sheng-li, et al., "Microstructure and Properties of In-Situ Generated WC-Reinforced Ni60 Gradient Coating by Laser Cladding on H13 Steel." Rare Metals and Cemented Carbides, no. 6, 2022, pp. 41-45.
APA [1] XUE Sheng-li, LI Jin-hua, YAO Fang-ping, & LI Xiang-xin. (2022). Microstructure and Properties of In-Situ Generated WC-Reinforced Ni60 Gradient Coating by Laser Cladding on H13 Steel. Rare Metals and Cemented Carbides(6), 41-45.
IEEE [1] XUE Sheng-li, LI Jin-hua, YAO Fang-ping, and LI Xiang-xin, "Microstructure and Properties of In-Situ Generated WC-Reinforced Ni60 Gradient Coating by Laser Cladding on H13 Steel," Rare Metals and Cemented Carbides, no. 6, pp. 41-45, 2022. keywords: {gradient coating;laser cladding;in-situ generation;Ni60;WC;microhardness;wear mechanism}