daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Autoclavable Polydopamine-Gelatin-Modified Polyethylene Terephthalate Microfibrous Carriers Regulate the Proliferation and Paracrine Signaling of Mesenchymal Stem Cells AITranslate

Sun Yat-sen University; Sun Yat-sen University; Sun Yat-sen University; Sun Yat-sen University; Sun Yat-sen University; Sun Yat-sen University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Mesenchymal stem cells (MSCs) have attracted considerable attention in cell therapies and tissue engineering for their multilineage differentiation potential and immunomodulatory properties. However, MSCs gradually lose their stemness and multipotentiality in prolonged two-dimensional (2D) culture in vitro. Herein, a three-dimensional (3D) polyethylene terephthalate (PET) microfiber sponge served as the substrate, and gelatin macromolecules were grafted onto PET through the adsorption of polydopamine to prepare a 3D cell carrier (PET-Gel) with an interpenetrating network structure. The cell carrier could be sterilized by autoclaving. The material characterization results showed that the 3D carrier had good coating stability, thermal stability, and mechanical properties; these properties did not decrease after autoclaving. In vitro cell experiments revealed that the 3D cell carrier promoted the adhesion and proliferation of human umbilical cord MSCs (HUCMSCs). In long-term culture (2 weeks), the cell proliferation rate was 2.4-fold higher than that on 2D plates because the interpenetrating network structure of the carrier led to a larger growing area than 2D plates and the cells infiltrated into the interior of the carrier. Simultaneously, HUCMSCs on PET-Gel expressed surface-specific antigens of the MSCs. The typical paracrine cytokine expression was characterized using qPCR and Western blotting. The paracrine function of cells on the 3D carrier was nearly equivalent to that on the 2D plates. These results showed that the PET-Gel carrier was suitable for the long-term culture of HUCMSCs in vitro.

KeyWords AITranslate

polyethylene terephthalate mesenchymal stem cells polydopamine gelatin paracrine
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c00232

Chinese Library Classification Number:

Citation Information:

Mesenchymal stem cells (MSCs) have attracted considerable attention in cell therapies and tissue engineering for their multilineage differentiation potential and immunomodulatory properties. However, MSCs gradually lose their stemness and multipotentiality in prolonged two-dimensional (2D) culture in vitro. Herein, a three-dimensional (3D) polyethylene terephthalate (PET) microfiber sponge served as the substrate, and gelatin macromolecules were grafted onto PET through the adsorption of polydopamine to prepare a 3D cell carrier (PET-Gel) with an interpenetrating network structure. The cell carrier could be sterilized by autoclaving. The material characterization results showed that the 3D carrier had good coating stability, thermal stability, and mechanical properties; these properties did not decrease after autoclaving. In vitro cell experiments revealed that the 3D cell carrier promoted the adhesion and proliferation of human umbilical cord MSCs (HUCMSCs). In long-term culture (2 weeks), the cell proliferation rate was 2.4-fold higher than that on 2D plates because the interpenetrating network structure of the carrier led to a larger growing area than 2D plates and the cells infiltrated into the interior of the carrier. Simultaneously, HUCMSCs on PET-Gel expressed surface-specific antigens of the MSCs. The typical paracrine cytokine expression was characterized using qPCR and Western blotting. The paracrine function of cells on the 3D carrier was nearly equivalent to that on the 2D plates. These results showed that the PET-Gel carrier was suitable for the long-term culture of HUCMSCs in vitro.

quote

GB/T 7714-2015 [1] Hao Ye, Yan Li, Jinze Li, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c00232.
MLA [1] Hao Ye, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c00232.
APA [1] Hao Ye, Yan Li, Jinze Li, Cong Cao, Yuxi Luo, & Yihong Gong. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c00232
IEEE [1] Hao Ye, Yan Li, Jinze Li, Cong Cao, Yuxi Luo, and Yihong Gong, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.2c00232. keywords: {polyethylene terephthalate;mesenchymal stem cells;polydopamine;gelatin;paracrine}