Determination of Major and Minor Elements in Ilmenite by XRF AITranslate
Abstract AITranslate
The TiO2, TFe, Al2O3, SiO2, MnO in ilmenite have been measured by XRFA using pelletized powder samples. After separating the calibration curve into two sections or correcting the matrix effects,areasonable accuracy has been obtained. The analysis ranges are as follows: TiO2 7-50%, TFe 20-38%, Al2O3 0.70-30%, SiO2 0. 15-32%,MnO 0. 17-0.80% The results of XRFA agree with those of chemical analysis. The calculations of the equilibrium of metal volume meet the demands of beneficiation. Therefore, this method is an accurate, simple fast and economical one for ilmenite analysis.
KeyWords AITranslate
1杨乐山,陈玉生,杜新岳,朱文翅,严志远.硅酸盐岩石中主要元素的X荧光光谱分析——粉末压片经验系数法[J]光谱学与光谱分析,1985(06).
2袁汉章,吴长存,卜赛斌,张虎云,许佩珍,武清富.铜矿选矿流程中铜、铁、硫、硅、铝、钼和钛的X射线荧光光谱直接测定[J]分析化学,1981(02).
1邱林友,王重华.X射线荧光光谱──单标法测定铸铁中硅、锰、磷和硫[J].昆明理工大学学报:理工版,1996,21(1):107-110. 被引量:1
2黄玉龙,吴健玲,余敏.重晶石中BaSO_4、SrSO_4的分析方法[J].广西化工,1999,28(3):38-41. 被引量:2
3邱林友,邱然.硫酸铈滴定法连续测定钛铁矿中的二氧化钛和总铁[J].辽东学院学报:自然科学版,2011,18(1):10-12. 被引量:6
4散飞雪,凌文黎,胡艳华,谢淑云.峡东地区闪长岩风化剖面元素和Sr-Nd同位素特征及其地球化学意义[J].地球化学,2013,42(5):430-446. 被引量:5
5韩延兵,曹珊,马景治.X射线荧光光谱法快速测定钒钛磁铁矿中的Ti、Fe、P、V、Co[J].西北地质,2017,50(2):224-230. 被引量:6
6李松,李小莉,王毅民,邓赛文.X射线荧光光谱在钒钛磁铁矿分析中应用文献评介[J].冶金分析,2023,43(5):52-60.
1曾小平,宋武元,吴冰.熔融制样-X射线荧光光谱法测定重晶石中的主要组分[J].光谱实验室,2011,28(3):1311-1314. 被引量:7
2赵建为,杨红燕.2011年云南冶金分析年评[J].云南冶金,2012,41(2):84-90. 被引量:1
3汤志勇,邱海鸥,郑洪涛.岩石矿物分析[J].分析试验室,2012,31(12):108-124. 被引量:17
4高红武,张健,周清,余良谋,李理.钛铁矿中钛-铁连续测定试验方法影响因素分析[J].昆明冶金高等专科学校学报,2013,29(3):65-67.
5高红武,张健,余良谋.钛铁矿钛铁连续测定试验研究[J].云南冶金,2013,42(6):66-69. 被引量:1
6郝选科,关祥忠,张中亭,曹兴旺.高钛冷固球团矿中全铁和TiO_2联合测定方法的研究[J].宝鸡文理学院学报:自然科学版,2014,34(3):22-26.
7裴秋明,刘图强,苑鸿庆,曹华文,李社宏,胡昕凯.广西姑婆山离子吸附型稀土矿床微量元素地球化学特征[J].成都理工大学学报:自然科学版,2015,42(4):451-462. 被引量:16
8陆筱彬,冯秀梅,李颖,陈君,陈连芳.X射线荧光光谱在船用金属材料成分分析中的应用进展[J].船舶标准化工程师,2015,48(6):49-54. 被引量:1
9苑鸿庆,李社宏,缪秉魁,严松,粟阳扬.广东惠东地区离子吸附型稀土矿床地球化学特征[J].现代地质,2016,30(6):1267-1275. 被引量:6
10王集宁,蒙永辉,颜堂,姚英强,刘瑞峰,邹连庆,商婷婷,付娟.山东蓬莱史家沟西山火山碎屑岩风化壳元素地球化学特征[J].地球学报,2018,39(4):498-512. 被引量:5
1谭凯旋,刘顺生,GntherA.Wagner.新疆阿尔泰地区哈巴河花岗岩体及邻近金矿床中石英的释光特征及其意义[J].核技术,2001,24(12):969-973. 被引量:7
2鲍芳,刘伟新.中国石化无锡石油地质研究所实验地质技术之氩离子抛光分析技术[J].石油实验地质,2014(4). 被引量:1
3张静,杨黎.ICP发射光谱法测定天青石中的主量和次量元素[J].岩矿测试,1989,8(2):108-111. 被引量:3
4谢琼心.X射线荧光光谱分析法测定多金属矿中的铅锌铜[J].分析试验室,1997,16(5):74-76. 被引量:11
5程泽,董永胜,井卫华,赵兰芳.XRF法快速测定化探样品中铜铅锌镓钛锰[J].内蒙古科技与经济,2012(2):158-158.
6帕.,ЕИ.构造相分析范围内的构造岩分类[J].地质科技动态,1991(23):1-4.
7韩松,贾秀琴,董金泉.现代核分析技术在资源环境研究中的应用[J].地质力学学报,2003,9(1):85-90. 被引量:4
8程泽,谭玉娟,刘晓光,张芳蓉,张艳春,阿拉木斯.XRF法测定高异常化探样品中的铜、铅、锌、镍[J].分析仪器,2006(1):29-31. 被引量:3
9梁述廷.地质样品中稀土总量的X射线荧光分析法测定[J].矿物岩石,1997,17(1):117-120. 被引量:7
10谭凯旋r,刘顺生,谢焱石,Günther A. Wagne.黄铁矿的释光特征及其地质意义[J].核技术,2003,26(1):32-35. 被引量:4
Basic Information:
DOI:
Chinese Library Classification Number:P575[天文地球—矿物学]
Citation Information:
The TiO2, TFe, Al2O3, SiO2, MnO in ilmenite have been measured by XRFA using pelletized powder samples. After separating the calibration curve into two sections or correcting the matrix effects,areasonable accuracy has been obtained. The analysis ranges are as follows: TiO2 7-50%, TFe 20-38%, Al2O3 0.70-30%, SiO2 0. 15-32%,MnO 0. 17-0.80% The results of XRFA agree with those of chemical analysis. The calculations of the equilibrium of metal volume meet the demands of beneficiation. Therefore, this method is an accurate, simple fast and economical one for ilmenite analysis.
quote
| GB/T 7714-2015 | [1] WANG Zhong-hua, ZHANG Hai-yan, QIU Lin-you. Determination of Major and Minor Elements in Ilmenite by XRF[J]. Rare Metals and Cemented Carbides, 1995(4): 40-42. |
| MLA | [1] WANG Zhong-hua, et al., "Determination of Major and Minor Elements in Ilmenite by XRF." Rare Metals and Cemented Carbides, no. 4, 1995, pp. 40-42. |
| APA | [1] WANG Zhong-hua, ZHANG Hai-yan, & QIU Lin-you. (1995). Determination of Major and Minor Elements in Ilmenite by XRF. Rare Metals and Cemented Carbides(4), 40-42. |
| IEEE | [1] WANG Zhong-hua, ZHANG Hai-yan, and QIU Lin-you, "Determination of Major and Minor Elements in Ilmenite by XRF," Rare Metals and Cemented Carbides, no. 4, pp. 40-42, 1995. keywords: {ilmentie, XRF, pelletized powder samples} |