daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Vacancy-Mediated Anion Photosegregation Kinetics in Mixed Halide Hybrid Perovskites: Coupled Kinetic Monte Carlo and Optical Measurements AITranslate

University of Notre Dame; University of Notre Dame; University of Notre Dame; University of Notre Dame; University of Notre Dame; University of Notre Dame; Argonne National Laboratory; University of Notre Dame
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites
111111

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Solution-processed mixed halide perovskites are excellent materials for multijunction solar cells. Unfortunately, light-induced halide phase segregation has prevented their effective integration into working devices. In this study, we rationalize and quantify anion photosegregation in stoichiometric and halide-deficient MAPb(I1–xBrx)3 thin films through kinetic Monte Carlo simulations and complementary optical measurements. Our study reveals that segregation rates are dictated by halide vacancy hopping barriers and are modulated by vacancy concentrations. The simulations further suggest that near-ubiquitous emission energies, which converge on that for MAPb(I0.8Br0.2)3 (i.e., x ≈ 0.2) following photosegregation, arise from the existence of kinetically trapped Br– within nucleated I-rich domains. An established photosegregation excitation intensity threshold is independent of the number of vacancies and instead depends critically on parameters such as carrier diffusion length, lifetime, and bandgap tunability. The study thus sheds new light on important parameters that define halide photosegregation and presents opportunities for controlling the phenomenon.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.8b01369

Chinese Library Classification Number:

Citation Information:

Solution-processed mixed halide perovskites are excellent materials for multijunction solar cells. Unfortunately, light-induced halide phase segregation has prevented their effective integration into working devices. In this study, we rationalize and quantify anion photosegregation in stoichiometric and halide-deficient MAPb(I1–xBrx)3 thin films through kinetic Monte Carlo simulations and complementary optical measurements. Our study reveals that segregation rates are dictated by halide vacancy hopping barriers and are modulated by vacancy concentrations. The simulations further suggest that near-ubiquitous emission energies, which converge on that for MAPb(I0.8Br0.2)3 (i.e., x ≈ 0.2) following photosegregation, arise from the existence of kinetically trapped Br– within nucleated I-rich domains. An established photosegregation excitation intensity threshold is independent of the number of vacancies and instead depends critically on parameters such as carrier diffusion length, lifetime, and bandgap tunability. The study thus sheds new light on important parameters that define halide photosegregation and presents opportunities for controlling the phenomenon.

quote

GB/T 7714-2015 [1] Anthony Ruth, Michael C. Brennan, Sergiu Draguta, et al. ACS Energy Letters, 2018(3). DOI:10.1021/acsenergylett.8b01369.
MLA [1] Anthony Ruth, et al., ACS Energy Letters, no. 3, 2018, https://doi.org/10.1021/acsenergylett.8b01369.
APA [1] Anthony Ruth, Michael C. Brennan, Sergiu Draguta, Yurii V. Morozov, Maksym Zhukovskyi, Boldizsar Janko, Peter Zapol, & Masaru Kuno. (2018). ACS Energy Letters(3). https://doi.org/10.1021/acsenergylett.8b01369
IEEE [1] Anthony Ruth, Michael C. Brennan, Sergiu Draguta, Yurii V. Morozov, Maksym Zhukovskyi, Boldizsar Janko, Peter Zapol, and Masaru Kuno, ACS Energy Letters, no. 3, 2018, doi: 10.1021/acsenergylett.8b01369.