Experimental Research on Titanium Recovery from Red Mud by Acid Leaching AITranslate
Abstract AITranslate
Titanium was recovered from red mud by acid leaching with sulfuric acid,hydrochloric acid or nitric acid as the leaching agent.The effects were investigated of kind and concentration of leaching agents,liquid to solid ratio,leaching temperature and reaction time on titanium recovery.The results show that sulfuric acid is more appropriate as the leaching agent.The leaching rate of titanium reaches 90% under the conditions of sulfuric acid concentration 40%,leaching temperature 100℃,liquid to solid ratio 6∶1and reaction time 60 min.Brookite and calcite disappear,perovskite,hematite and cancrinite decrease and anhydrite forms during acid leaching.Dissolution reaction of perovskite and brookite in sulfuric acid results in titanium recovery from red mud.
KeyWords AITranslate
1ZHU De-qing, CHUN Tie-jun, PAN Jian, HE Zhen (School of Minerals Processing and Bioengineering, Central South University, Changsha 410083, Hunan, China).Recovery of Iron From High-Iron Red Mud by Reduction Roasting With Adding Sodium Salt[J].钢铁研究学报:英文版,2012(8):1-5. 被引量:34
2王克勤,宋嘉伟,高燕,姜武.氧化铝赤泥盐酸浸出稀土元素研究[J].稀有金属,2012,36(4):676-680. 被引量:16
3魏昶,樊刚,李旻廷,邓志敢.含钒石煤氧压酸浸中影响钒浸出率的主要因素研究[J].稀有金属,2007,31(S1):98-101. 被引量:26
4南相莉,张廷安,刘燕,豆志河.我国赤泥综合利用分析[J].过程工程学报,2010,10(S1):264-270. 被引量:127
5孙道兴.赤泥脱碱处理和有价金属钛钪提取的研究[J].无机盐工业,2008,40(10):49-52. 被引量:39
6王重庆,王晖,符剑刚,陈勇.赤泥中稀有金属分布及回收工艺研究现状[J].稀有金属与硬质合金,2013,41(3):11-15. 被引量:10
7李小斌,肖伟,刘伟,刘桂华,彭志宏,周秋生,齐天贵.Recovery of alumina and ferric oxide from Bayer red mud rich in iron by reduction sintering[J].中国有色金属学会会刊:英文版,2009,19(5):1342-1347. 被引量:31
8姜平国,廖春发.盐酸浸出赤泥分离有价金属的工艺研究[J].中国矿业,2011,20(12):85-87. 被引量:15
9王琪,姜林.硫酸浸出赤泥中铁、铝、钛的工艺研究[J].矿冶工程,2011,31(4):90-94. 被引量:36
1李望,朱晓波.赤泥盐酸浸出钇试验研究[J].轻金属,2015(12):20-23.
2李望,朱晓波.酸浸提取赤泥中钪的研究[J].有色金属:冶炼部分,2016(5):36-38. 被引量:10
3李望,朱晓波.赤泥草酸脱碱实验研究[J].硅酸盐通报,2016,35(4):1283-1286. 被引量:10
4李望,朱晓波,管学茂.赤泥化学选矿制备富钛渣的研究[J].稀有金属与硬质合金,2016,44(4):25-27. 被引量:5
5龙琼,路坊海,周登凤,胡素丽,伍玉娇.磁场下硫酸浸出赤泥回收钛的研究[J].广东化工,2016,43(17):32-33. 被引量:4
6朱晓波,李望,李文中,汤森,白鹏远,管学茂.赤泥中钇浸出行为及动力学研究[J].硅酸盐通报,2016,35(10):3367-3372. 被引量:8
7罗宇智,徐璐,史光大.硫酸熟化浸出赤泥中钪的研究[J].有色金属:冶炼部分,2017(4):45-47. 被引量:12
8常军,邵延海,李硕,蒋丰祥,张校熔.赤泥中有价金属元素综合回收研究现状及进展[J].矿冶,2017,26(3):59-63. 被引量:18
9赵恒,李望,朱晓波,马名杰.赤泥提钛研究现状与展望[J].河南化工,2018,35(6):3-7. 被引量:3
10徐丽霜,隋丽丽,葛欣,翟玉春,邵爽.碱浸提钛渣提硅实验过程及其动力学研究[J].稀有金属与硬质合金,2019,47(4):20-23.
1龙昌鑫,方琴,杨小洁,郭玉兰,李宇.赤泥基本性能及赤泥混凝土力学性能研究[J].中国水运:下半月,2021,21(10):126-127. 被引量:2
2路晓涛,张志斌,郑洁,邵帅.国内赤泥脱碱工艺的研究进展[J].铝镁通讯,2016,0(4):1-5. 被引量:1
3常军,邵延海,李硕,蒋丰祥,张校熔.赤泥中有价金属元素综合回收研究现状及进展[J].矿冶,2017,26(3):59-63. 被引量:18
4闵小波,柴立元,柯勇,史美清,费讲驰,梁彦杰.我国有色冶炼固体废物处理相关技术及政策建议[J].环境保护,2017,45(20):24-30. 被引量:8
5李望,朱晓波,汤森,李文中.选择性萃取分离酸溶液中钪的试验与热力学研究[J].中国稀土学报,2017,35(6):755-760. 被引量:6
6赵恒,李望,朱晓波,马名杰.赤泥提钛研究现状与展望[J].河南化工,2018,35(6):3-7. 被引量:3
7杨玉珠,周强.2017年云南选矿年评[J].云南冶金,2018,47(3):16-34.
8王璐,郝彦忠,郝增发.赤泥中有价金属提取与综合利用进展[J].中国有色金属学报,2018,28(8):1697-1710. 被引量:32
9李爱民,何瑞明,刘敬,李诚,赵玉莲.低铁拜耳法赤泥熔融态深度还原除铁试验研究[J].矿业研究与开发,2018,38(10):101-105. 被引量:4
10刘万超,段光福,闫琨,张朝普,和新忠.赤泥微粉填料制备高分子复合材料技术研究[J].轻金属,2018(10):5-10. 被引量:3
1李望,朱晓波.赤泥盐酸浸出钇试验研究[J].轻金属,2015(12):20-23.
2李望,朱晓波,管学茂.赤泥化学选矿制备富钛渣的研究[J].稀有金属与硬质合金,2016,44(4):25-27. 被引量:5
3辽宁省钢铁行业脱硫工程年可减排20万t[J].钢结构,2010(5):86-86.
4李穗中.废干电池热解过程的物相变化研究——《废干电池无害化与资源化技术研究》第一报[J].广州环境科学,2004,19(4):22-25.
5高尔乐,何滨,江桂斌,陈登云.酸浸提-HPLC-ICP-MS系统测定土壤与底泥样品中的甲基汞、乙基汞[J].环境化学,2008,27(5):698-700. 被引量:32
6范美容,黄懿.高氯酸浸提-氟离子电极法测定氟化物[J].企业技术开发,2000,18(2):6-7. 被引量:3
7平安,魏忠义,李培军,李晓军,金京华.有机酸与表面活性剂联合作用对土壤重金属的浸提效果研究[J].生态环境学报,2011,20(6):1152-1157. 被引量:22
8辽宁启动钢铁行业烧结机脱硫减排工程[J].钢结构,2010(7):88-89.
9罗冰,张清东.柠檬酸浸出土壤中铜、锌的优化设计[J].环境工程学报,2013,7(9):3629-3634. 被引量:12
10谢文鹏,王贵明.柳钢中板废水处理利用技术[J].冶金环境保护,2000(4):31-33.
Basic Information:
DOI:
Chinese Library Classification Number:X758[环境科学与工程—环境工程]
Citation Information:
Titanium was recovered from red mud by acid leaching with sulfuric acid,hydrochloric acid or nitric acid as the leaching agent.The effects were investigated of kind and concentration of leaching agents,liquid to solid ratio,leaching temperature and reaction time on titanium recovery.The results show that sulfuric acid is more appropriate as the leaching agent.The leaching rate of titanium reaches 90% under the conditions of sulfuric acid concentration 40%,leaching temperature 100℃,liquid to solid ratio 6∶1and reaction time 60 min.Brookite and calcite disappear,perovskite,hematite and cancrinite decrease and anhydrite forms during acid leaching.Dissolution reaction of perovskite and brookite in sulfuric acid results in titanium recovery from red mud.
quote
| GB/T 7714-2015 | [1] ZHU Xiao-bo, GUAN Xue-mao, LI Wang. Experimental Research on Titanium Recovery from Red Mud by Acid Leaching[J]. Rare Metals and Cemented Carbides, 2015(2): 11-13. |
| MLA | [1] ZHU Xiao-bo, et al., "Experimental Research on Titanium Recovery from Red Mud by Acid Leaching." Rare Metals and Cemented Carbides, no. 2, 2015, pp. 11-13. |
| APA | [1] ZHU Xiao-bo, GUAN Xue-mao, & LI Wang. (2015). Experimental Research on Titanium Recovery from Red Mud by Acid Leaching. Rare Metals and Cemented Carbides(2), 11-13. |
| IEEE | [1] ZHU Xiao-bo, GUAN Xue-mao, and LI Wang, "Experimental Research on Titanium Recovery from Red Mud by Acid Leaching," Rare Metals and Cemented Carbides, no. 2, pp. 11-13, 2015. keywords: {red mud;titanium recovery;acid leaching;sulfuric acid;hydrochloric acid;nitric acid} |